journal article·2025-11Open access

Fuel cell membrane durability impacts of incidental non-metallic particle deposition – Part 1: Effect of particle type

MohammadAmin Bahrami, Nitish Kumar, Yixuan Chen, Olivia C. Lowe, Francesco P. Orfino, Monica Dutta, Michael Lauritzen, Erin Setzler, Alexander L. Agapov, Erik Kjeang

Abstract

This two-part article series examines the impacts of incidental non-metallic particle deposition on fuel cell membrane durability. Part 1 investigates the effect of particle type, while Part 2 focuses on mitigation approaches. In this part (Part 1), selected foreign particles are intentionally introduced at the membrane and catalyst layer interface of a fuel cell, which is then subjected to chemo-mechanical stress testing with 4D tracking of local degradation using in-situ X-ray computed tomography. The results show that 35 μm polytetrafluoroethylene particles, 100 μm polyethylene terephthalate fibers, and 60 μm polymethyl methacrylate (PMMA) microspheres are unlikely to affect the durability in long-term operation due to minuscule effect on the catalyst coated membrane. However, 300 μm PMMA microspheres, 60 μm silica microspheres, and 1000 μm graphite flakes have the potential to compromise durability by damaging the membrane during fabrication or creating room for increased membrane deformation, which can lead to greater stress fluctuations during operation. The results indicate that stiffness, shape, and size determine whether a given particle is harmful to cell durability. • Durability impacts depend on particle size, shape, hardness, and interaction mode. • PTFE, PET, and 60 μm PMMA particles had minor impact on membrane durability. • 300 μm PMMA and 60 μm silica particles caused membrane damage during fabrication. • Graphite flakes created adjacent cavities, leading to inevitable membrane failure.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Fuel Cells and Related Materials · Electrocatalysts for Energy Conversion · Advancements in Solid Oxide Fuel Cells

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. New roads and challenges for fuel cells in heavy-duty transportation10.1038/s41560-021-00775-z ↗
2. Polymer electrolyte membrane degradation mechanisms in fuel cells - findings over the past 30 years and comparison with electrolyzers10.1149/1.2214554 ↗
3. The effect of membrane casting irregularities on initial fuel cell performance10.1002/fuce.201900149 ↗
4. Local degradation at membrane defects in polymer electrolyte fuel cells10.1149/1.023306jes ↗
5. Factors determining the gas crossover through pinholes in polymer electrolyte fuel cell membranes10.1016/j.electacta.2012.07.013 ↗
6. Impact of electrode thick spot irregularities on polymer electrolyte membrane fuel cell initial performance10.1016/j.jpowsour.2020.228344 ↗
7. Effect of catalyst layer defects on local membrane degradation in polymer electrolyte fuel cells10.1016/j.jpowsour.2016.05.016 ↗
8. Impact of membrane scratches on fuel cell durability10.1016/j.ijhydene.2025.05.379 ↗
9. Prasad · 2019
10. Improved decal transfer method to reduce membrane damage from foreign particles in membrane electrode assembly10.1149/1945-7111/ad0dc3 ↗
11. Quality implications of foreign metallic particles in the membrane electrode assembly of a fuel cell10.1149/1945-7111/ad650c ↗
12. Airborne particle deposition in cleanrooms: relationship between deposition rate and airborne concentration
13. Particulate fallout predictions for clean
14. Fuel cell perfluorinated sulfonic acid membrane degradation correlating accelerated stress testing and lifetime10.1021/cr200424d ↗
15. In situ metal ion contamination and the effects on proton exchange membrane fuel cell performance10.1016/j.jpowsour.2011.01.086 ↗
16. In-situ modeling of chemical membrane degradation and mitigation in ceria-supported fuel cells10.1149/2.1201712jes ↗
17. Macroscopic in-situ modeling of chemical membrane degradation in polymer electrolyte fuel cells10.1149/2.0031409jes ↗
18. Accelerated stress test procedures for PEM fuel cells under actual load constraints: state-Of-Art and proposals10.1016/j.ijhydene.2015.07.026 ↗
19. DOE fuel cell program: durability technical targets and testing protocols10.1149/1.2781004 ↗
20. 3D failure analysis of pure mechanical and pure chemical degradation in fuel cell membranes10.1149/2.0451713jes ↗
21. Four-dimensional in situ imaging of chemical membrane degradation in fuel cells10.1016/j.electacta.2021.138194 ↗
22. Membrane degradation during combined chemical and mechanical accelerated stress testing of polymer electrolyte fuel cells10.1016/j.jpowsour.2014.01.106 ↗
23. Radical (HO • , H • and HOO •) formation and ionomer degradation in polymer electrolyte fuel cells10.1149/1.3581040 ↗
24. Decay in mechanical properties of catalyst coated membranes subjected to combined chemical and mechanical membrane degradation10.1002/fuce.201400040 ↗
25. Mechanical degradation of fuel cell membranes under fatigue fracture tests10.1016/j.jpowsour.2014.10.135 ↗
26. Tracking the evolution of mechanical degradation in fuel cell membranes using 4D in situ visualization10.1016/j.jpowsour.2018.11.049 ↗
27. Mitigation of mechanical membrane degradation in fuel cells – part 1: gas diffusion layers with low surface roughness
28. Effect of hygral swelling and shrinkage on mechanical durability of fuel cell membranes10.1016/j.jpowsour.2019.04.081 ↗
29. 4D imaging of chemo-mechanical membrane degradation in polymer electrolyte fuel cells - part 2: unraveling the coupled degradation mechanisms within the active area
30. 4D imaging of chemo-mechanical membrane degradation in polymer electrolyte fuel cells - part 1: understanding and evading edge failures
31. Residual fatigue life modeling of fuel cell membranes10.1016/j.jpowsour.2020.228714 ↗
32. Simulation of ionomer membrane fatigue under mechanical and hygrothermal loading conditions10.1016/j.jpowsour.2014.12.133 ↗
33. In-situ simulation of membrane fatigue in polymer electrolyte fuel cells10.1016/j.ijhydene.2017.01.173 ↗
34. Mitigation of mechanical membrane degradation in fuel cells – part 2: bonded membrane electrode assembly
35. 3D printed flow field and fixture for visualization of water distribution in fuel cells by X-ray computed tomography10.1149/2.0461613jes ↗
36. Four-dimensional joint visualization of electrode degradation and liquid water distribution inside operating polymer electrolyte fuel cells10.1038/s41598-018-38464-9 ↗
37. 4D in situ visualization of mechanical degradation evolution in reinforced fuel cell membranes10.1016/j.ijhydene.2020.02.013 ↗
38. Effect of accelerated stress testing conditions on combined chemical and mechanical membrane durability in fuel cells10.1149/1945-7111/ad0e43 ↗
39. Interactions between reinforced membrane durability and gas diffusion layer and flow field plate designs in fuel cells10.1016/j.jpowsour.2025.237726 ↗
40. Degradation and deformation patterns in reinforced fuel cell membranes subjected to chemo-mechanical stress testing degradation and deformation patterns in reinforced fuel cell membranes subjected to chemo-mechanical stress testing10.1149/1945-7111/add29a ↗
41. Membrane degradation at catalyst layer edges in PEMFC MEAs10.1149/1.2789791 ↗
42. Impacts of cathode catalyst layer defects on performance and durability in PEM fuel cells10.1016/j.jpowsour.2023.233565 ↗
43. Review of hydrogen crossover through the polymer electrolyte membrane10.1016/j.ijhydene.2021.04.050 ↗
44. Fuel cell membrane durability impacts of incidental non-metallic particle deposition–Part 2: Failure prevention strategies10.1016/j.jpowsour.2025.237912 ↗