Compatibility of LiCoO2 and LiMn2O4 cathode materials for Li0.55La0.35TiO3 electrolyte to fabricate all-solid-state lithium battery
Source abstract
Abstract
Abstract In order to improve performance of all-solid-state lithium ion battery with honeycomb structure, a compatibility of two commonly used cathode materials, LiCoO 2 and LiMn 2 O 4 , to Li 0.55 La 0.35 TiO 3 (LLT) solid electrolyte was studied. LiCoO 2 /honeycomb LLT and LiMn 2 O 4 /honeycomb LLT half cells were fabricated by the impregnation of mixture of the cathode material with its precursor sol into honeycomb holes followed by the calcination. Impurity phases were observed at interface between LiCoO 2 and honeycomb LLT, while no impurity phase was confirmed in the case of LiMn 2 O 4 . In half cell test, the LiMn 2 O 4 /honeycomb LLT cell showed about 6 times larger discharge capacity than the LiCoO 2 /honeycomb LLT cell, because of high internal resistance of the LiCoO 2 /honeycomb LLT cell caused by the impurity phases. It can be said that the formation of low resistance interface at active material/electrolyte is one of the most important key to improve performance of the all-solid-state battery. Using LiMn 2 O 4 instead of LiCoO 2 , better interface between cathode material and LLT was obtained.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Murugan · Appl. Phys. A · 2008 · 91 · 61510.1007/s00339-008-4494-2 ↗
2. Knauth · Solid State Ionics · 2009 · 180 · 91110.1016/j.ssi.2009.03.022 ↗
3. Stephan · Polymer · 2006 · 47 · 595210.1016/j.polymer.2006.05.069 ↗
4. Niitani · J. Power Sources · 2005 · 146 · 38610.1016/j.jpowsour.2005.03.102 ↗
5. Bates · Solid State Ionics · 2000 · 135 · 3310.1016/S0167-2738(00)00327-1 ↗
6. Baba · J. Power Sources · 2001 · 97–98 · 79810.1016/S0378-7753(01)00733-9 ↗
7. Hart · Electrochem. Commun. · 2003 · 5 · 12010.1016/S1388-2481(02)00556-8 ↗
8. Golodnitsky · Solid State Ionics · 2006 · 177 · 281110.1016/j.ssi.2006.02.048 ↗
9. Min · J. Power Sources · 2008 · 178 · 79510.1016/j.jpowsour.2007.10.003 ↗
10. Kotobuki · J. Electrochem. Soc. · 2010 · 157 · A49310.1149/1.3308459 ↗
11. Liao · J. Alloys Compd. · 2007 · 432 · L2210.1016/j.jallcom.2006.06.024 ↗
12. Hara · J. Power Sources · 2009 · 189 · 48510.1016/j.jpowsour.2008.12.048 ↗
13. Rho · J. Electrochem. Soc. · 2003 · 150 · A10710.1149/1.1526514 ↗
14. Dokko · J. Power Sources · 2009 · 189 · 78310.1016/j.jpowsour.2008.07.081 ↗
15. Katiyara · J. Power Sources · 2009 · 194 · 52610.1016/j.jpowsour.2009.05.017 ↗