journal article·2007-01

Electrochemical studies of low-temperature processed nano-crystalline LiMn2O4 thin film cathode at 55°C

S.B. Tang, M.O. Lai, L. Lu

Journal of Power Sources· Volume 164· Issue 1
Publisher page

Abstract

Abstract LiMn2O4 thin films with nano-crystals less than 100 nm were successfully grown on polished stainless steel substrates at 400 °C and 200 m Torr of oxygen by pulsed laser deposition. A maximum discharge capacity of 62.4 μAh cm−2 μm−1 cycled between 3.0 and 4.5 V with a current density of 20 μAh cm−2 was achieved. The effect of several overdischarge cycles was negligible, and both the effect of Jahn–Teller distortion at low potentials on capacity loss and structure instability at high potentials were effectively inhibited in this nano-crystalline film, resulting in an excellent cycling stability with a very low fading rate of capacity up to 500 cycles at 55 °C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Battery Materials · Semiconductor materials and devices · Advanced Memory and Neural Computing

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Broussely · Electrochim. Acta · 1999 · 45 · 310.1016/S0013-4686(99)00189-9 ↗
2. Thackeray · Mater. Res. Bull. · 1983 · 18 · 46110.1016/0025-5408(83)90138-1 ↗
3. Wen · J. Electrochem. Soc. · 1996 · 143 · 13610.1149/1.1836902 ↗
4. Kanoh · J. Electrochem. Soc. · 1996 · 143 · 261010.1149/1.1837056 ↗
5. Manev · J. Power Sources · 1995 · 57 · 9910.1016/0378-7753(95)02227-9 ↗
6. Xia · J. Electrochem. Soc. · 1997 · 144 · 259310.1149/1.1837870 ↗
7. Guohua · J. Electrochem. Soc. · 1996 · 143 · 17810.1149/1.1836405 ↗
8. Antonini · J. Electrochem. Soc. · 1998 · 145 · 272610.1149/1.1838705 ↗
9. Moon · J. Power Sources · 2003 · 119 · 71710.1016/S0378-7753(03)00209-X ↗
10. Hosoya · Solid State Ionics · 1998 · 111 · 15310.1016/S0167-2738(98)00156-8 ↗
11. Zheng · Solid State Ionics · 2002 · 148 · 31710.1016/S0167-2738(02)00068-1 ↗
12. Shu · Solid State Ionics · 2003 · 160 · 22710.1016/S0167-2738(03)00190-5 ↗
13. Moon · J. Power Sources · 2003 · 119 · 71310.1016/S0378-7753(03)00218-0 ↗
14. Lee · J. Power Sources · 2004 · 130 · 24110.1016/j.jpowsour.2003.11.059 ↗
15. Van Zomeren · J. Aerosol Sci. · 1994 · 25 · 122910.1016/0021-8502(94)90211-9 ↗
16. Mohamedi · J. Power Sources · 2001 · 93 · 9310.1016/S0378-7753(00)00551-6 ↗
17. Mohamedi · J. Electrochem. Soc. · 2002 · 149 · A1910.1149/1.1424285 ↗
18. Shui · Electrochim. Acta · 2004 · 49 · 220910.1016/j.electacta.2004.01.002 ↗
19. Thackeray · J. Electrochem. Soc. · 1997 · 144 · L10010.1149/1.1837624 ↗
20. Brousse · J. Power Sources · 1997 · 68 · 41210.1016/S0378-7753(97)02521-4 ↗
21. Chiu · J. Electrochem. Soc. · 2005 · 152 · A205810.1149/1.2034524 ↗
22. Striebel · J. Electrochem. Soc. · 1996 · 143 · 182110.1149/1.1836910 ↗
23. Morcrette · Solid State Ionics · 2001 · 138 · 21310.1016/S0167-2738(00)00796-7 ↗
24. Yamada · Electrochem. Commun. · 2003 · 5 · 50210.1016/S1388-2481(03)00113-9 ↗
25. Julien · Mater. Sci. Eng. B · 2000 · 72 · 3610.1016/S0921-5107(99)00598-X ↗
26. Mohamedi · Electrochim. Acta · 2002 · 47 · 348310.1016/S0013-4686(02)00285-2 ↗
27. Rougier · J. Electrochem. Soc. · 1998 · 145 · 297510.1149/1.1838750 ↗
28. Ho · J. Electrochem. Soc. · 1980 · 127 · 34310.1149/1.2129668 ↗
29. Striehel · J. Electrochem. Soc. · 1999 · 146 · 433910.1149/1.1392640 ↗
30. Song · J. Electrochem. Soc. · 2003 · 150 · A12110.1149/1.1527937 ↗
31. Ammundsen · J. Phys. Chem. B · 1999 · 103 · 517510.1021/jp984398l ↗