Analysis of the kinetics of borohydride oxidation in Cu anode for direct borohydride fuel cell
Source abstract
Abstract
Abstract A multi-step mechanism is discussed for the oxidation of BH 4 − on Cu anode in NaOH solution. Polarization experiments are conducted in 2 M sodium hydroxide solutions with 0.5, 1.0, and 2.0 M NaBH 4 at 25, 50, and 75 °C, respectively. The rate-determining step is the electrochemical oxidation of B H 4 , ad − that reacted with O H ad − at low overpotentials and changes to the competitive adsorption of BH 4 − or OH − at higher overpotentials. The theoretical predictions are satisfactorily in accordance with the polarization data. However, these predictions deviate from the data at the highest temperature or concentration of BH 4 − because of the bubbling of the side product, H 2 .
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen Storage and Materials · Electrocatalysts for Energy Conversion · Ammonia Synthesis and Nitrogen Reduction
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Amendola · J. Power Sources · 2000 · 85 · 18610.1016/S0378-7753(99)00301-8 ↗
2. Krishnan · J. Power Sources · 2005 · 143 · 1710.1016/j.jpowsour.2004.12.007 ↗
3. Finkelstein · J. Power Sources · 2011 · 196 · 622310.1016/j.jpowsour.2011.03.034 ↗
4. Atwana · Int. J. Hydrogen Energy · 2007 · 32 · 311610.1016/j.ijhydene.2005.12.022 ↗
5. Gyenge · Electrochim. Acta · 2004 · 49 · 96510.1016/j.electacta.2003.10.008 ↗
6. Liu · Electrochim. Acta · 2004 · 49 · 309710.1016/j.electacta.2004.02.023 ↗
7. Celik · Int. J. Hydrogen Energy · 2010 · 35 · 867810.1016/j.ijhydene.2010.04.150 ↗
8. Liu · J. Electrochem. Soc. · 2003 · 150 · A39810.1149/1.1553785 ↗
9. Lee · J. Electrochem. Soc. · 2002 · 149 · A60310.1149/1.1467365 ↗
10. Elder · Trans. Faraday Soc. · 1962 · 58 · 185210.1039/tf9625801852 ↗
11. Indig · J. Electrochem. Soc. · 1962 · 109 · 110410.1149/1.2425247 ↗
12. Izumi · J. Electrochem. Soc. · 1985 · 132 · 232310.1149/1.2113572 ↗
13. Mirkin · J. Electrochem. Soc. · 1992 · 139 · 221210.1149/1.2221204 ↗
14. Martins · Electrochim. Acta · 2007 · 52 · 644310.1016/j.electacta.2007.04.066 ↗
15. Chatenet · Electrochim. Acta · 2006 · 51 · 545910.1016/j.electacta.2006.02.015 ↗
16. Morris · Chem. Rev. · 1985 · 85 · 5110.1021/cr00065a003 ↗
17. Iotova · Electrochim. Acta · 2009 · 54 · 723610.1016/j.electacta.2009.07.032 ↗
18. Meerakker · J. Appl. Electrochem. · 1981 · 11
19. Escano · J. Phys. Chem. C · 2011 · 115 · 1988310.1021/jp207768e ↗
20. Wang · Catal. Today · 2011 · 170 · 9910.1016/j.cattod.2010.12.023 ↗
21. Dong · J. Phys. Chem. B · 2005 · 109 · 1089610.1021/jp050322v ↗
22. Santos · Electrochim. Acta · 2010 · 55 · 677510.1016/j.electacta.2010.05.091 ↗
23. Santos · J. Electrochem. Soc. · 2010 · 157 · B1310.1149/1.3247540 ↗
24. Concha · Electrochim. Acta · 2009 · 54 · 611910.1016/j.electacta.2009.05.027 ↗
25. Geng · J. Power Sources · 2008 · 185 · 62710.1016/j.jpowsour.2008.09.010 ↗
26. Concha · Electrochem. Commun. · 2009 · 11 · 22310.1016/j.elecom.2008.11.018 ↗
27. Concha · J. Phys. Chem. C · 2011 · 115 · 1243910.1021/jp2002589 ↗
28. Lam · J. Phys. Chem. C · 2011 · 115 · 272710.1021/jp108771h ↗
29. Li · J. Alloys Compd. · 2003 · 356–357 · 46910.1016/S0925-8388(02)01241-0 ↗
30. Verma · J. Power Sources · 2007 · 168 · 20010.1016/j.jpowsour.2007.02.069 ↗
31. Sanli · Int. J. Hydrogen Energy · 2011 · 36 · 854210.1016/j.ijhydene.2011.03.141 ↗
32. Rostamikia · J. Power Sources · 2011 · 196 · 922810.1016/j.jpowsour.2011.07.042 ↗
33. Shivhare · J. Power Sources · 2007 · 173 · 24010.1016/j.jpowsour.2007.05.004 ↗
34. Shivhare · J. Electroanal. Chem. · 2006 · 595 · 14510.1016/j.jelechem.2006.07.017 ↗
35. Li · J. Power Sources · 2006 · 163 · 55510.1016/j.jpowsour.2006.09.037 ↗
36. Sun · J. Power Sources · 2010 · 195 · 110.1016/j.jpowsour.2009.07.028 ↗