Modeling of kinetic behavior of the lead dioxide electrode in a lead–acid battery by means of electrochemical impedance spectroscopy
Source abstract
Abstract
Abstract In this paper a mathematical model for the electrochemical impedance of a positive electrode in the lead–acid battery was developed. The mechanisms of the electrode processes involved in the batteries were obtained from the literature. Having selected the rate-controlling step as well as the fast reversible (equilibrated) and irreversible steps, we embarked on the formulation of I – V behavior using Butler–Volmer and Fick's law for charge and mass transfer process, respectively. The equivalent circuit consists of resistors, capacitors and mass transfer elements. Each electrical element expresses physico-chemical parameters such as diffusion coefficient, concentration, rate constant, etc. So, impedance plots can be used to determine the effects of each parameter on the performance of the cells. The simulation model also shows that the state-of-charge (SOC) plays an important role in the Nyquist plot of the positive electrode. Model results are compared with experimental results for cell potential and different SOC.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Battery Technologies Research · Advanced battery technologies research · Ionic liquids properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Nakagama · J. Power Sources · 2002 · 107 · 19210.1016/S0378-7753(01)01005-9 ↗
2. Misra · J. Power Sources · 2001 · 95 · 16210.1016/S0378-7753(00)00616-9 ↗
3. Parker · J. Power Sources · 2001 · 100 · 1810.1016/S0378-7753(01)00880-1 ↗
4. Crew · J. Power Sources · 2001 · 95 · 24110.1016/S0378-7753(00)00646-7 ↗
5. Salkind · J. Power Sources · 1999 · 80 · 29310.1016/S0378-7753(99)00079-8 ↗
6. Salkind · J. Power Sources · 2001 · 96 · 15110.1016/S0378-7753(01)00561-4 ↗
7. Huet · J. Power Sources · 1998 · 70 · 5910.1016/S0378-7753(97)02665-7 ↗
8. Buller · J. Power Sources · 2003 · 113 · 42210.1016/S0378-7753(02)00558-X ↗
9. Stoynov · J. Power Sources · 1990 · 30 · 27510.1016/0378-7753(93)80085-4 ↗
10. Tenno · J. Power Sources · 2002 · 111 · 6510.1016/S0378-7753(02)00276-8 ↗
11. Tenno · J. Power Sources · 2001 · 103 · 4210.1016/S0378-7753(01)00830-8 ↗
12. Mauracher · J. Power Sources · 1997 · 67 · 6910.1016/S0378-7753(97)02498-1 ↗
13. Nguyen · Electrochim. Acta · 1993 · 38 · 93510.1016/0013-4686(93)87012-3 ↗
14. Gu · J. Power Sources · 2002 · 108 · 17410.1016/S0378-7753(02)00043-5 ↗
15. Andersson · J. Appl. Electrochem. · 2001 · 31 · 110.1023/A:1004105622558 ↗
16. Gu · J. Electrochem. Soc. · 1987 · 134 · 295310.1149/1.2100322 ↗
17. Nelatury · J. Power Sources · 2004 · 132 · 30910.1016/j.jpowsour.2003.12.013 ↗
18. Hampson · J. Appl. Electrochem. · 1980 · 10 · 310.1007/BF00937331 ↗
19. Willihnganz · Electr. Eng. · 1959 · 78 · 92210.1109/EE.1959.6445924 ↗
20. S. De Bardelaben, Determining the End of Battery Life, INTELLEC 86, IEEE Publication, 1986, pp. 365–386.10.1109/INTLEC.1986.4794452 ↗
21. Pavlov · J. Electrochem. Soc.: Electrochem. Sci. Technol. · 1980 · 127 · 85510.1149/1.2129770 ↗