Hot corrosion of yttria-stabilized zirconia by liquid antimony and antimony oxide

Jiyang Ma, Nanqi Duan, Yue Han, Peiyao Li, Bin Zhu, Dong Yan, Bo Chi, Jian Pu, Jian Li

Publisher page

Abstract

Abstract Direct carbon solid oxide fuel cells (DC-SOFCs) with a liquid Sb anode have many advantages over other types of SOFCs; however, their electrolyte faces corrosion by liquid Sb and Sb 2 O 3 . To evaluate the tolerance of the electrolyte to the liquid Sb and Sb 2 O 3 , 8 mol.% Y 2 O 3 –ZrO 2 electrolyte (YSZ) discs are prepared and evaluated at 750 °C for up to 100 h in both chemical and electrochemical modes, simulating DC-SOFC operating conditions. In the chemical mode, the corrosion by liquid Sb causes Y dissolution from YSZ into the liquid Sb, while the YSZ experiences a phase transformation from cubic to tetragonal structure and grain boundary crack on the surface. Liquid Sb 2 O 3 is more corrosive than liquid Sb, penetrating additionally the grain boundaries into a depth around 15 μm. In the electrochemical mode, liquid Sb is separated from YSZ by a layer (~150 μm) of liquid Sb 2 O 3 formed during cell operation. The liquid Sb 2 O 3 layer so formed corrodes YSZ in the same way as in the chemical mode, but the corrosion is intensified with the presence of a current, resulting in a top porous layer (~15 μm) on YSZ surface with a grain boundary penetration layer (~100 μm) underneath.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Catalysis and Oxidation Reactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. Choudhury · Renew. Sustain. Energy Rev. · 2013 · 20 · 43010.1016/j.rser.2012.11.031 ↗
2. Stambouli · Renew. Sustain. Energy Rev. · 2002 · 6 · 43310.1016/S1364-0321(02)00014-X ↗
3. Mahato · Prog. Mater. Sci. · 2015 · 72 · 14110.1016/j.pmatsci.2015.01.001 ↗
4. Larminie · 2003
5. Tsiakaras · J. Power Sources · 2001 · 102 · 21010.1016/S0378-7753(01)00803-5 ↗
6. Gür · Prog. Energy Combust. Sci. · 2016 · 54 · 110.1016/j.pecs.2015.10.004 ↗
7. Murray · Nature · 1999 · 400 · 64910.1038/23220 ↗
8. Aravind · Prog. Energy Combust. Sci. · 2012 · 38 · 73710.1016/j.pecs.2012.03.006 ↗
9. Panopoulos · J. Power Sources · 2006 · 159 · 57010.1016/j.jpowsour.2005.12.024 ↗
10. Park · Nature · 1999 · 404 · 26510.1038/35005040 ↗
11. Li · Int. J. Hydrogen Energy · 2014 · 39 · 1597510.1016/j.ijhydene.2014.01.132 ↗
12. Gorte · Adv. Mater. · 2010 · 12 · 146510.1002/1521-4095(200010)12:19<1465::AID-ADMA1465>3.0.CO;2-9 ↗
13. Jiang · Chem. Soc. Rev. · 2017 · 46 · 288910.1039/C6CS00784H ↗
14. Javadekar · J. Electrochem. Soc. · 2012 · 159 · A38610.1149/2.050204jes ↗
15. Jayakumar · Energy Environ. Sci. · 2011 · 4 · 413310.1039/c1ee01863a ↗
16. Duan · Energy · 2016 · 95 · 27410.1016/j.energy.2015.10.033 ↗
17. Duan · Appl. Energy · 2016 · 165 · 98310.1016/j.apenergy.2015.11.050 ↗
18. Zhou · J. Electrochem. Soc. · 2015 · 162 · F56710.1149/2.0871506jes ↗
19. Oh · ECS Trans. · 2015 · 68 · 269510.1149/06801.2695ecst ↗
20. Cao · Energy · 2017 · 125 · 52610.1016/j.energy.2017.02.106 ↗
21. Ma · J. Power Sources · 2018 · 401 · 39710.1016/j.jpowsour.2018.08.083 ↗
22. Cao · Ceram. Int. · 2017 · 43 · 1657510.1016/j.ceramint.2017.09.045 ↗
23. Los Alamos National Laboratory Report LAUR
24. EXPGUI, a graphical user interface for GSAS10.1107/S0021889801002242 ↗
25. Fracture resistance of 8 mol% yttria stabilized zirconia10.1007/BF02710085 ↗
26. Mechanical properties of high-temperature-degraded yttria-stabilized zirconia10.1016/j.actamat.2014.01.017 ↗
27. Effect of temperature on solid particle impact erosion wear mechanism of 5mol% Yttria Stabilized Zirconia ceramics10.1016/j.ceramint.2015.01.128 ↗
28. Yttria concentration dependence of tensile strength in yttria-stabilized zirconia10.1016/S0925-8388(03)00640-6 ↗
29. Effect of sintering temperature on the microstructure and mechanical properties of ZrO2-3mol%Y2O3 sol–gel films10.1016/j.ceramint.2010.07.033 ↗
30. Hot corrosion behavior of rare earth zirconates and yttria partially stabilized zirconia thermal barrier coatings10.1016/j.surfcoat.2010.04.044 ↗
31. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
32. Recovery of tetragonal phase from previously transformed Y-TZP10.1590/1980-5373-MR-2015-0426 ↗
33. Electrochemical characterization of liquid metal anode solid oxide fuel cell10.1149/1.3697433 ↗
34. Polarization characteristics of liquid antimony anode with smooth single-crystal solid oxide electrolyte10.1016/j.jpowsour.2013.06.125 ↗
35. A FIB-STEM study of strontium segregation and interface formation of directly assembled La0.6Sr0.4Co0.2Fe0.8O3-δCathode on Y2O3-ZrO2Electrolyte of solid oxide fuel cells10.1149/2.0151807jes ↗
36. A review of state of the art on stripping phenomenon in asphalt concrete10.1016/j.conbuildmat.2012.08.033 ↗
37. The electrical conductivity of molten oxides10.1139/v53-133 ↗