Although fuel cell operation at intermediate temperatures ( e.g. , 100–120 °C) could potentially reduce cost in heavy-duty transportation, the associated durability challenges need systematic investigation. This work employs ex-situ dynamic mechanical analysis and pressure differential accelerated mechanical stress test together with in-situ fuel cell stability and durability tests to evaluate a sulfo-phenylated poly(phenylene)-based composite membrane for intermediate temperature operation. Compared to wet/dry cycling at 80 °C, the membrane shows ∼50 % lower stress of dehydration and 10x slower crack propagation at 110 °C, albeit the risks of creep failure are higher. Fuel cell testing at fixed current density (1.5 A cm −2 ) demonstrates stable performance at 110 °C and 34 % RH for 100 h, with no indication of irreversible degradation over longer durations. However, single-frequency electrochemical impedance spectroscopy shows that RH cycling at such temperatures increases the rate and depth of membrane drying. In-situ RH cycling durability tests combined with electrochemical diagnostics and 4D X-ray computed tomography visualization reveals membrane-electrode incompatibility and localized thinning near the edges as failure modes. Hence, fully hydrocarbon-based designs with proper stress concentration management are believed to enhance the durability of next generation fuel cell membranes at intermediate temperatures. • Operation at 110 °C, low RH reduces membrane dehydration stress and crack growth. • MEAs ran ∼100 h at 110 °C, 34 % RH, 1.5 A cm −2 with no sign of membrane degradation. • RH cycling AST at 110 °C is proposed, guided by stress–strain and hydration data. • Interface incompatibility in CCMs causes membrane failure during 110 °C RH cycling. • RH cycling at 110 °C induces localized creep and membrane thinning near the edges.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Fuel Cells and Related Materials · Advancements in Solid Oxide Fuel Cells · Nanopore and Nanochannel Transport Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (78)

Show source-provided references
1. Jiao · Nature. · 2021 · 595 · 36110.1038/s41586-021-03482-7 ↗
2. Aminudin · Int. J. Hydrogen Energy. · 2023 · 48 · 437110.1016/j.ijhydene.2022.10.156 ↗
3. Ahluwalia · J. Electrochem. Soc. · 2024 · 171
4. Anselma · Appl. Energy. · 2022 · 32110.1016/j.apenergy.2022.119354 ↗
5. Suzuki · ECS Trans. · 2019 · 92 · 310.1149/09208.0003ecst ↗
6. Cullen · Nat. Energy. · 2021 · 6 · 46210.1038/s41560-021-00775-z ↗
7. Lochner · Chemelectrochem. · 2020 · 7 · 354510.1002/celc.202000588 ↗
8. Haider · Chem. Soc. Rev. · 2021 · 50 · 113810.1039/D0CS00296H ↗
9. Tse · J. Phys. Chem. A · 2015 · 119 · 124610.1021/acs.jpca.5b00572 ↗
10. Gittleman · Joule · 2021 · 5 · 166010.1016/j.joule.2021.05.016 ↗
11. Meyer · Electrochem. Energy Rev. · 2023 · 610.1007/s41918-023-00180-y ↗
12. Strandberg · Fuel Cells · 2025 · 25
13. Peighambardoust · Int. J. Hydrogen Energy. · 2010 · 35 · 934910.1016/j.ijhydene.2010.05.017 ↗
14. Giacinti Baschetti · Int. J. Hydrogen Energy. · 2013 · 38 · 1197310.1016/j.ijhydene.2013.06.104 ↗
15. Mukundan · J. Electrochem. Soc. · 2018 · 165 · F308510.1149/2.0101806jes ↗
16. Stariha · J. Electrochem. Soc. · 2018 · 165 · F49210.1149/2.0881807jes ↗
17. Jeon · Int. J. Hydrogen Energy. · 2015 · 40 · 305710.1016/j.ijhydene.2015.01.010 ↗
18. Butori · J. Power Sources. · 2023 · 56310.1016/j.jpowsour.2023.232803 ↗
19. Li · RSC Adv. · 2014 · 4 · 394410.1039/C3RA43735C ↗
20. Zhao · Mater. · 2021 · 15
21. Xiao · J. Membr. Sci. · 2013 · 442 · 6510.1016/j.memsci.2013.04.014 ↗
22. Stassi · J. Power Sources · 2011 · 196 · 892510.1016/j.jpowsour.2010.12.084 ↗
23. Yin · J. Membr. Sci. · 2024 · 70710.1016/j.memsci.2024.122997 ↗
24. Mirfarsi · Processes. · 2020 · 8 · 106910.3390/pr8091069 ↗
25. Ibrahim · Int. J. Hydrogen Energy · 2020 · 45 · 552610.1016/j.ijhydene.2019.05.210 ↗
26. Wehkamp · RSC Adv. · 2016 · 6 · 2426110.1039/C5RA27462A ↗
27. Kakinuma · J. Electrochem. Soc. · 2022 · 16910.1149/1945-7111/ac624b ↗
28. Karimi · Int. J. Energy Res. · 2022 · 46 · 1985510.1002/er.8411 ↗
29. Butori · Int. J. Hydrogen Energy. · 2024 · 95 · 115810.1016/j.ijhydene.2024.06.286 ↗
30. Mirfarsi · Int. J. Hydrogen Energy. · 2024 · 50 · 150710.1016/j.ijhydene.2023.07.236 ↗
31. Han · Int. J. Hydrogen Energy · 2024 · 58 · 27910.1016/j.ijhydene.2024.01.131 ↗
32. Shi · Int. J. Fatig. · 2022 · 15410.1016/j.ijfatigue.2021.106554 ↗
33. Shi · Appl. Energy · 2025 · 393
34. Gaines · Am. J. Ind. Med. · 2023 · 66 · 35310.1002/ajim.23362 ↗
35. Yandrasits · J. Electrochem. Soc. · 2022 · 16910.1149/1945-7111/ac5d96 ↗
36. Mirfarsi · Int. J. Hydrogen Energy · 2022 · 47 · 1346010.1016/j.ijhydene.2022.02.077 ↗
37. Park · Chem. Soc. Rev. · 2024
38. Noh · J. Power Sources · 2023 · 58010.1016/j.jpowsour.2023.233422 ↗
39. Adamski · Angew. Chem. · 2017 · 129 · 918610.1002/ange.201703916 ↗
40. Adamski · Mater. Adv. · 2021 · 2 · 496610.1039/D1MA00511A ↗
41. Nguyen · Sustain. Energy Fuels. · 2021 · 5 · 368710.1039/D1SE00556A ↗
42. Long · iScience · 2021 · 24
43. Choi · ACS Energy Lett. · 2025 · 10 · 239210.1021/acsenergylett.5c00487 ↗
44. Park · 2025
45. Tanaka · J. Power Sources Adv. · 2021 · 1010.1016/j.powera.2021.100063 ↗
46. Miyake · ACS Mater. Au · 2021 · 1 · 8110.1021/acsmaterialsau.1c00002 ↗
47. Sadeghi Alavijeh · J. Power Sources · 2019 · 427 · 20710.1016/j.jpowsour.2019.04.081 ↗
48. Goulet · J. Power Sources. · 2013 · 234 · 3810.1016/j.jpowsour.2013.01.128 ↗
49. Sadeghi Alavijeh · J. Power Sources. · 2015 · 285 · 1610.1016/j.jpowsour.2015.03.082 ↗
50. Mirfarsi · J. Power Sources. · 2025 · 63010.1016/j.jpowsour.2024.236137 ↗
51. Sadeghi Alavijeh · J. Power Sources Adv. · 2020 · 210.1016/j.powera.2020.100010 ↗
52. Sebdani · Polym. Test. · 2024
53. Garland · ECS Trans. · 2007 · 11 · 92310.1149/1.2781004 ↗
54. Chen · J. Electrochem. Soc. · 2023 · 170
55. Chen · J. Power Sources. · 2022 · 520
56. Chen · J. Power Sources. · 2022 · 520
57. Shin · ACS Omega. · 2019 · 4 · 1915310.1021/acsomega.9b02436 ↗
58. Zhang · J. Electrochem. Soc. · 2014 · 161
59. Cai · Energy Convers. Manag. · 2024 · 30710.1016/j.enconman.2024.118348 ↗
60. Messing · J. Power Sources · 2020 · 45110.1016/j.jpowsour.2020.227750 ↗
61. Khattra · J. Power Sources. · 2020 · 47710.1016/j.jpowsour.2020.228714 ↗
62. Kusoglu · J. Power Sources. · 2006 · 161 · 98710.1016/j.jpowsour.2006.05.020 ↗
63. Long · ACS Appl. Mater. Interfaces. · 2021 · 13 · 1536610.1021/acsami.1c04270 ↗
64. Wu · J. Membr. Sci. · 2020 · 610
65. Bangay · Phys. Chem. Chem. Phys. · 2025
66. Liu · J. Mater. Chem. A · 2022 · 10 · 766010.1039/D1TA10480B ↗
67. Egemole · Electrochim. Acta · 2024 · 50810.1016/j.electacta.2024.145259 ↗
68. Ding · J. Power Sources · 2016 · 316 · 11410.1016/j.jpowsour.2016.03.031 ↗
69. Wang · J. Power Sources · 2024 · 597
70. Singh · J. Power Sources. · 2019 · 412 · 22410.1016/j.jpowsour.2018.11.049 ↗
71. Ramani · Int. J. Hydrogen Energy. · 2020 · 45 · 1008910.1016/j.ijhydene.2020.02.013 ↗
72. Huang · J. Polym. Sci. B Polym. Phys. · 2006 · 44 · 234610.1002/polb.20863 ↗
73. Bograchev · Int. J. Hydrogen Energy. · 2008 · 33 · 570310.1016/j.ijhydene.2008.06.066 ↗
74. Pahon · J. Power Sources. · 2022 · 54610.1016/j.jpowsour.2022.231895 ↗
75. Chen · J. Power Sources · 2020 · 476
76. Ishikawa · J. Power Sources · 2016 · 325 · 3510.1016/j.jpowsour.2016.06.012 ↗
77. Shimizu · J. Electrochem. Soc. · 2019 · 166
78. Alavijeh · J. Electrochem. Soc. · 2015 · 16210.1149/2.0471514jes ↗