journal article·2006-10

Electrochemical performance of Nd0.6Sr0.4Co0.5Fe0.5O3−δ–Ag composite cathodes in intermediate temperature solid oxide fuel cells

K.T. Lee, A. Manthiram

Journal of Power Sources· Volume 160· Issue 2
Publisher page

Abstract

Abstract The electrochemical performances of Nd 0.6 Sr 0.4 Co 0.5 Fe 0.5 O 3− δ –Ag composite cathodes have been investigated in intermediate temperature solid oxide fuel cells. The Nd 0.6 Sr 0.4 Co 0.5 Fe 0.5 O 3− δ –Ag cathodes prepared by ball milling followed by firing at 920 °C show the maximum performance (power density: 0.15 W cm −2 at 800 °C) at 3 wt.% Ag. On the other hand, the Nd 0.6 Sr 0.4 Co 0.5 Fe 0.5 O 3− δ –Ag composite cathodes with 0.1 mg cm −2 (∼0.5 wt.%) Ag that were prepared by an impregnation of Ag into Nd 0.6 Sr 0.4 Co 0.5 Fe 0.5 O 3− δ followed by firing at 700 °C (but the electrolyte–Nd 0.6 Sr 0.4 Co 0.5 Fe 0.5 O 3− δ assembly was prepared first by firing at 1100 °C) exhibit much better performance (power density: 0.27 W cm −2 at 800 °C) than the composite cathodes prepared by ball milling, despite a much smaller amount of Ag due to a better dispersion and an enhanced adhesion. AC impedance analysis indicates that the Ag catalysts dispersed in the porous Nd 0.6 Sr 0.4 Co 0.5 Fe 0.5 O 3− δ cathode reduce the ohmic and the polarization resistances due to an increased electronic conductivity and enhanced electrocatalytic activity.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Minh · J. Am. Ceram. Soc. · 1993 · 76 · 56310.1111/j.1151-2916.1993.tb03645.x ↗
2. Colomer · Solid State Ionics · 2002 · 147 · 4110.1016/S0167-2738(02)00002-4 ↗
3. Zheng · J. Electrochem. Soc. · 1999 · 146 · 281010.1149/1.1392012 ↗
4. De Souza · Solid State Ionics · 1998 · 106 · 17510.1016/S0167-2738(97)00499-2 ↗
5. Petrov · Solid State Ionics · 1995 · 80 · 18910.1016/0167-2738(95)00114-L ↗
6. Kawada · J. Electrochem. Soc. · 2002 · 149 · E25210.1149/1.1479728 ↗
7. Tai · Solid State Ionics · 1995 · 76 · 25910.1016/0167-2738(94)00244-M ↗
8. Yamamoto · Solid State Ionics · 1987 · 22 · 24110.1016/0167-2738(87)90039-7 ↗
9. Kostogloudis · Solid State Ionics · 1998 · 106 · 20710.1016/S0167-2738(97)00506-7 ↗
10. Lee · J. Electrochem. Soc. · 2005 · 152 · A19710.1149/1.1828243 ↗
11. Xia · Solid State Ionics · 2002 · 149 · 1110.1016/S0167-2738(02)00131-5 ↗
12. Takeda · Solid State Ionics · 1996 · 86–88 · 118710.1016/0167-2738(96)00285-8 ↗
13. Stevenson · J. Electrochem. Soc. · 1996 · 143 · 272210.1149/1.1837098 ↗
14. Lee · Solid State Ionics · 2005 · 176 · 152110.1016/j.ssi.2005.05.002 ↗
15. Lee · J. Electrochem. Soc. · 2006 · 153 · A79410.1149/1.2172572 ↗
16. Uchida · Solid State Ionics · 2000 · 135 · 34710.1016/S0167-2738(00)00465-3 ↗
17. Sasaki · Solid State Ionics · 2001 · 144 · 22310.1016/S0167-2738(01)00973-0 ↗
18. Sasaki · Solid State Ionics · 2002 · 148 · 55110.1016/S0167-2738(02)00116-9 ↗
19. Uchida · J. Electrochem. Soc. · 2002 · 149 · A1310.1149/1.1423641 ↗
20. Baker · J. Electrochem. Soc. · 1997 · 144 · 242710.1149/1.1837831 ↗
21. Zhang · J. Alloys Compd. · 2005 · 395 · 32210.1016/j.jallcom.2004.11.056 ↗
22. Xia · Appl. Phys. Lett. · 2003 · 82 · 90110.1063/1.1542933 ↗
23. Uhlenbruck · J. Solid State Electrochem. · 2004 · 8 · 92310.1007/s10008-004-0510-4 ↗
24. Wang · Solid State Ionics · 2002 · 146 · 20310.1016/S0167-2738(01)01015-3 ↗
25. Azaroff · 1968
26. Chick · Mater. Lett. · 1990 · 10 · 610.1016/0167-577X(90)90003-5 ↗
27. K.T. Lee, A. Manthiram, J. Power Sources, in press.
28. Craciun · J. Electrochem. Soc. · 1999 · 146 · 401910.1149/1.1392586 ↗