journal article·2020-02Open access

Durability of nanostructured LaPrNiO4+δ electrode for solid oxide cells: Electrochemical, microstructural, and structural investigation

Nur Istiqomah Khamidy, Jérôme Laurencin, Dario Ferreira Sanchez, Federico Monaco, Frederic Charlot, Elisabeth Djurado

Abstract

Abstract This work reports a durability study in galvanostatic mode at 700 °C for 900–960 h related to structural and microstructural evolution of LaPrNiO4+δ (LPNO) oxygen electrode. The performances of the electrode, deposited by electrostatic spray deposition (ESD) and screen printing (SP), are not changed when operated under electrolysis current whereas a degradation is observed in fuel cell mode. Small quantities of secondary phases (La,Pr)3Ni2O7-δ in the fine ESD microstructure and Pr6O11 on both ESD and SP layers are detected in the pristine electrode by synchrotron μ-X-ray diffraction and fluorescence. The destabilization of LPNO electrode, which slightly occurs in the ESD layer after thermal aging in air, is strongly accelerated under anodic and cathodic currents. Indeed, the formation of a new phase (La,Pr)4Ni3O10-δ on both ESD and SP layers occurs with the extension of (La,Pr)3Ni2O7-δ in the SP layer, and a significant increase in the amount Pr6O11 at high current density. Nevertheless, the electrode microstructure, determined by FIB-SEM tomography, remains stable under current whereas severe delamination is observed after aging in fuel cell mode. Based on these characterizations, the mechanisms of electrode aging have been discussed to explain the different behavior in fuel cell and electrolysis modes.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Magnetic and transport properties of perovskites and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Review of progress in high temperature solid oxide fuel cells
2. Progress in material selection for solid oxide fuel cell technology: a review10.1016/j.pmatsci.2015.01.001 ↗
3. Lowering the temperature of solid oxide fuel cells10.1126/science.1204090 ↗
4. Intermediate temperature solid oxide fuel cells10.1039/b612060c ↗
5. Layered perovskites as promising cathodes for intermediate temperature solid oxide fuel cells10.1039/b704320a ↗
6. Anisotropic oxygen diffusion in tetragonal La2NiO4+δ: molecular dynamics calculations10.1039/B917118E ↗
7. Oxygen diffusion and transport properties in non-stoichiometric Ln2-xNiO4+δ oxides10.1016/j.ssi.2005.06.033 ↗
8. The semiconductor-to-metal transition in question in La2-xNiO4+δ (δ > 0 or δ < 0)10.1006/jssc.1994.1146 ↗
9. Oxygen diffusion and surface exchange in La2-xSrxNiO4+δ10.1016/S0167-2738(00)00388-X ↗
10. Advances in layered oxide cathodes for intermediate temperature solid oxide fuel cells10.1039/b922430k ↗
11. La2-xPrxNiO4+δ as suitable cathodes for metal supported SOFCs10.1016/j.ssi.2015.05.005 ↗
12. Thermal stability of Ln2NiO4+δ (Ln: La, Pr, Nd) and their chemical compatibility with YSZ and CGO solid electrolytes10.1016/j.ijhydene.2011.08.105 ↗
13. Influence of La/Pr ratio on the ageing properties of La2-XPrxNiO4+δ as cathodes in IT-SOFCs10.1149/06801.0825ecst ↗
14. Design of La2−xPrxNiO4+δ SOFC cathodes: a compromise between electrochemical performance and thermodynamic stability10.1039/C6TA08011A ↗
15. Improving the electrochemical performance of LaPrNiO4+δ as an oxygen electrode for intermediate temperature solid oxide cells by varying the architectural design10.1016/j.jelechem.2019.113373 ↗
16. Rational design of hierarchically nanostructured electrodes for solid oxide fuel cells10.1016/j.jpowsour.2016.09.156 ↗
17. Reaction mechanism and impact of microstructure on performances for the LSCF-CGO composite electrode in solid oxide cells10.1002/fuce.201800185 ↗
18. Ni/YSZ electrodes structures optimized for increased electrolysisperformance and durability10.1016/j.ssi.2016.06.003 ↗
19. Degradation of Ni-YSZ electrodes in solid oxide cells: impact of polarization and initial microstructure on the Ni evolution10.1149/2.1261915jes ↗
20. Electrode properties of the ruddlesden-popper series, Lan +1NinO3n+1 (n=1, 2, and 3), as intermediate-temperature solid oxide fuel cells10.1111/j.1551-2916.2010.03743.x ↗
21. High performance La3Ni2O7 cathode prepared by a facile sol-gel method for intermediate temperature solid oxide fuel cells10.1016/j.elecom.2012.06.004 ↗
22. XANES study on Ruddlesden-Popper phase, Lan+1NinO3n+1 (n = 1, 2 and ∞)10.1107/S0909049500015983 ↗
23. Electrostatic spray deposition of thin layers of cathode materials for lithium battery10.1016/0167-2738(96)00305-0 ↗
24. An innovative architectural design to enhance the electrochemical performance of La2NiO4+?? cathodes for solid oxide fuel cell applications10.1016/j.jpowsour.2016.03.067 ↗
25. Stochastic geometrical modeling of solid oxide cells electrodes validated on 3D reconstructions10.1016/j.commatsci.2017.11.015 ↗
26. Role of microstructure on electrode operating mechanisms for mixed ionic electronic conductors: from synchrotron-based 3D reconstruction to electrochemical modeling10.1016/j.ssi.2016.07.001 ↗
27. Focused ion beam induced deposition of platinum10.1116/1.585167 ↗
28. Recent advances in magnetic structure determination by neutron powder diffraction10.1016/0921-4526(93)90108-I ↗
29. The fast azimuthal integration Python library: pyFAI10.1107/S1600576715004306 ↗
30. Micro X-ray diffraction and fluorescence tomography for the study of multilayered automotive paints10.1002/sia.3125 ↗
31. XRDUA : crystalline phase distribution maps by two-dimensional scanning and tomographic (micro) X-ray powder diffraction10.1107/S1600576714008218 ↗
32. Distortions in electrochemical impedance spectroscopy measurements using 3-electrode methods in SOFC. I-effect of cell geometry10.1002/fuce.200700019 ↗
33. Degradation of solid oxide electrolysis cells: phenomena, mechanisms, and emerging mitigation strategies – a review
34. Mixed ionic-electronic conductivity in phases in the praseodymium oxide system10.1007/s100080000187 ↗
35. Fabrication, characterization, and electrical conductivity properties of Pr6O11 nanoparticles10.1016/S1002-0721(12)60345-7 ↗
36. Comparison of morphology and electrical conductivity of various thin films containing nano-crystalline praseodymium oxide particles10.1016/j.sna.2006.11.019 ↗
37. Highly efficient architectured Pr6O11 oxygen electrode for solid oxide fuel cell10.1016/j.jpowsour.2019.02.077 ↗
38. La4Ni3O10−δ as an efficient solid oxide fuel cell cathode: electrochemical properties versus microstructure10.1039/C5TA07862H ↗
39. Degradation mechanism of La0.6Sr0.4Co0.2Fe0.8O3-δ/Gd0.1Ce0.9O2-δ composite electrode operated under solid oxide electrolysis and fuel cell conditions10.1016/j.electacta.2017.05.011 ↗
40. 23,000 h steam electrolysis with an electrolyte supported solid oxide cell10.1016/j.ijhydene.2017.01.072 ↗
41. Degradation phenomena in a solid oxide electrolysis cell after 9000 h of operation10.1016/j.jpowsour.2012.09.061 ↗
42. Vibhu · 2016
43. On the Praseodymium+Oxygen system