An insulating material in a structured host enables sustainable formation of a granular Li metal for highly durable Li metal battery

Yongho Shin, Wontae Lee, Kyungho Ahn, Chulhaeng Lee, Byoungwoo Kang

Publisher page

Abstract

© 2022 Elsevier B.V.For using Li metal anode, controlling Li metal morphology for long-term cycles is an essential requirement, but the porous Li metal easily form due to a dendritic Li growth. Here, we report on a novel strategy to reversibly form a granular Li metal by confining Li deposition sites and controlling the Li metal morphology via a structured functional host that is composed of small portion of a Li-alloying region and large portion of an insulating region. The insulating region confines the nucleation sites to the Li-alloying region because the nucleation cannot occur in the insulating region, and strongly affects the growth/morphology of the Li metal because the insulating particles mitigate the Li+ concentration around the Li-alloying particles. The persistent effects of the confinement and control of the Li metal morphology enable to sustainably form the granular Li metal. The Cu electrode with the functional host structure achieve Coulombic efficiency of >98% over 500 cycles, and can reversibly deposit Li metal with LiCoO2 cathode even in typical standard carbonate electrolytes. The findings reveal novel capabilities of insulating materials for sustainable use of Li and provide a new avenue for designing practical use of Li metal for durable Li metal batteries. ; 1 ; 1 ; N ; scie ; scopus
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. A short review of failure mechanisms of lithium metal and lithiated graphite anodes in liquid electrolyte solutions10.1016/S0167-2738(02)00080-2 ↗
2. Lithium metal anodes for rechargeable batteries10.1039/C3EE40795K ↗
3. A review of lithium deposition in lithium-ion and lithium metal secondary batteries10.1016/j.jpowsour.2013.12.099 ↗
4. Structural modulation of lithium metal-electrolyte interface with three-dimensional metallic interlayer for high-performance lithium metal batteries
5. Failure mechanism for fast-charged lithium metal batteries with liquid electrolytes
6. Morphological transitions on lithium metal anodes10.1149/1.3158548 ↗
7. Quantifying inactive lithium in lithium metal batteries10.1038/s41586-019-1481-z ↗
8. Controlled lithium dendrite growth by a synergistic effect of multilayered graphene coating and an electrolyte additive10.1021/cm503447u ↗
9. Ultrathin two-dimensional atomic crystals as stable interfacial layer for improvement of lithium metal anode10.1021/nl503125u ↗
10. Interconnected hollow carbon nanospheres for stable lithium metal anodes10.1038/nnano.2014.152 ↗
11. A lithium superionic conductor10.1038/nmat3066 ↗
12. Plating a dendrite-free lithium anode with a polymer/ceramic/polymer sandwich electrolyte10.1021/jacs.6b05341 ↗
13. Flexible ion-conducting composite membranes for lithium batteries10.1002/aenm.201500265 ↗
14. Constructing a high-strength solid electrolyte layer by in vivo alloying with aluminum for an ultrahigh-rate lithium metal anode
15. Chlorinated dual-protective layers as interfacial stabilizer for dendrite-free lithium metal anode10.1016/j.ensm.2021.06.023 ↗
16. The synergetic effect of lithium polysulfide and lithium nitrate to prevent lithium dendrite growth
17. Stable lithium electrodeposition in salt-reinforced electrolytes10.1016/j.jpowsour.2015.01.030 ↗
18. Effect of vinylene carbonate as additive to electrolyte for lithium metal anode10.1016/j.electacta.2003.09.010 ↗
19. Advanced liquid electrolytes for rechargeable Li metal batteries10.1002/adfm.201910777 ↗
20. An inorganic-rich solid electrolyte interphase for advanced lithium-metal batteries in carbonate electrolytes10.1002/anie.202012005 ↗
21. Dendrite-Free lithium deposition with self-aligned nanorod structure10.1021/nl5039117 ↗
22. Dendrite-Free lithium deposition via self-healing electrostatic shield mechanism10.1021/ja312241y ↗
23. Synergistic effect of 3D current collectors and ALD surface modification for high coulombic efficiency lithium metal anodes
24. Composite lithium metal anode by melt infusion of lithium into a 3D conducting scaffold with lithiophilic coating10.1073/pnas.1518188113 ↗
25. Dendrite-Free lithium deposition induced by uniformly distributed lithium ions for efficient lithium metal batteries10.1002/adma.201506124 ↗
26. Polymer nanofiber-guided uniform lithium deposition for battery electrodes10.1021/nl5046318 ↗
27. Dendritic growth mechanisms in lithium/polymer cells10.1016/S0378-7753(98)00242-0 ↗
28. Electrochemical aspects of the generation of ramified metallic electrodeposits10.1103/PhysRevA.42.7355 ↗
29. Correlating microstructural lithium metal growth with electrolyte salt depletion in lithium batteries using Li-7 MRI10.1021/jacs.5b09385 ↗
30. Shaping Li deposits from wild dendrites to regular crystals via the ferroelectric effect10.1021/acs.nanolett.0c03206 ↗
31. Ferroelectric polarization accelerates lithium-ion diffusion for dendrite-free and highly-practical lithium-metal batteries10.1016/j.nanoen.2020.105481 ↗
32. Mixed ion and electron-conducting scaffolds for high-rate lithium metal anodes10.1002/aenm.201900193 ↗
33. Stable lithium electrodeposition at ultra-high current densities enabled by 3D PMF/Li composite anode10.1002/aenm.201703360 ↗