Improvement of nucleation and electrical properties of Bi3.15Nd0.85Ti2.99Mn0.01O12 thin films with an upper Bi4Ti3O12 buffer layer
Source abstract
Abstract
A highly (117)-preferred Bi3.15Nd0.85Ti2.99Mn0.01O12 (BNTM) thin film with an upper Bi4Ti3O12 (BTO) buffer layer was fabricated on Pt(111)/Ti/SiO2/Si(100) substrates by a sol–gel method. The effects of the added upper Bi4Ti3O12 (BTO) layer on the structural and electrical properties of BNTM were investigated. X-ray diffraction, SEM and AFM images indicated that BTO/BNTM thin films exhibited a significantly higher (117) orientation and larger grain growth compared with the BNTM thin films (without the upper BTO layer). It was found that the BTO/BNTM thin films further showed the relatively larger remanent polarization (2P r = 94.3 μC/cm2) and dielectric constant (e r = 467.8). The enhancement of piezoelectric properties was also obtained in BTO/BNTM thin films. Moreover, the BTO/BNTM thin films displayed the better fatigue properties, degraded by only 7.4 % after 109 pulse cycles as compared to 30.2 % for BNTM thin films. A highly (117)-preferred Bi3.15Nd0.85Ti2.99Mn0.01O12 (BNTM) thin film with an upper Bi4Ti3O12 (BTO) buffer layer was fabricated on Pt(111)/Ti/SiO2/Si(100) substrates by a sol–gel method. The effects of the added upper Bi4Ti3O12 (BTO) layer on the structural and electrical properties of BNTM were investigated. X-ray diffraction, SEM and AFM images indicated that BTO/BNTM thin films exhibited a significantly higher (117) orientation and larger grain growth compared with the BNTM thin films (without the upper BTO layer). It was found that BTO/BNTM thin films further showed the relatively larger remanent polarization (2P r = 94.3 μC/cm2) and dielectric constant (e r = 467.8). The enhancement of piezoelectric properties was also obtained in BTO/BNTM thin films. Moreover, the BTO/BNTM thin films displayed the better fatigue properties, degraded by only 7.4 % after 109 pulse cycles as compared to 30.2 % for BNTM thin films.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Acoustic Wave Resonator Technologies · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Xie D, Luo YF, Han XG, Ren TL, Liu LT (2009) J Appl Phys 106:4117
2. Song HJ, Ding T, Zhong XL, Wang JB, Li B, Zhang Y, Zhou YC (2014) RSC Adv 4:60497–6050110.1039/C4RA11952E ↗
3. Yuan SG, Wang JB, Zhong XL, Wang F, Li B, Zhou YC (2013) J Mater Chem C 1:418–42110.1039/C2TC00097K ↗
4. Lu ZY, Yang CH, Hu GD, Wang JC, Wang X (2010) J Alloys Compd 508:106–10910.1016/j.jallcom.2010.05.096 ↗
5. Cheng CP, Tang MH, Tang ZH, Zhou YC (2013) J Sol–Gel Sci Technol 68:346–45010.1007/s10971-013-3176-5 ↗
6. Tang ZH, Xiong Y, Tang MH, Xiao YG, Zhang W, Yuan ML, Ouyang J, Zhou YC (2014) J Mater Chem C 2:1427–143510.1039/c3tc32105c ↗
7. Rae AD, Thompson JG, Withers RL, Willis AC (1990) Acta Cryst B 46:474–48710.1107/S0108768190003251 ↗
8. Chon U, Jang HM, Kim MG, Chang CH (2002) Phys Rev Lett 89:08760110.1103/PhysRevLett.89.087601 ↗
9. Garga A, Barber ZH, Dawber M, Scott JF, Snedden A, Lightfoot P (2003) Appl Phys Lett 83:2414–241610.1063/1.1613052 ↗
10. Lu CJ, Qiao Y, Qi YJ, Chen XQ, Zhu JS (2005) Appl Phys Lett 87:22290110.1063/1.2135386 ↗
11. Hu GD (2006) J Appl Phys 100:6109
12. Hou F, Shen MR, Cao WW (2005) Thin Solid Films 471:35–3910.1016/j.tsf.2004.03.030 ↗
13. Yu J, Yang B, Li J, Liu XM, Zheng CD, Wu YY, Zhang DM (2008) J Phys D Appl Phys 41:03530410.1088/0022-3727/41/3/035304 ↗
14. Zhong XL, Wang JB, Liao M, Tan CB, Shu HB, Zhou YC (2008) Thin Solid Films 516:8240–824310.1016/j.tsf.2008.03.004 ↗
15. Zhong XL, Li B, Wang JB, Liao M, Liao H, Zhou YC (2008) Mater Lett 62:2891–289310.1016/j.matlet.2008.01.065 ↗
16. Bao DH, Chiu TW, Wakiya N, Shinozaki K, Mizutani N (2003) J Appl Phys 93:497–50310.1063/1.1524708 ↗
17. Wang Q, Shen MR (2005) Thin Solid Films 473:74–7910.1016/j.tsf.2004.07.012 ↗
18. Li JJ, Li P, Zhang GJ, Yu J, Li J, Yang WM (2011) J Mater Sci: Mater Electron 22:299–303
19. Lee HN, Hesse D, Zakharov N, Gosele U (2002) Science 296:2006–200910.1126/science.1069958 ↗
20. Pei L, Hu N, Deng G, Bie YG, Chen YW, Li MY (2015) J Electron Mater 44:2340–234710.1007/s11664-015-3800-y ↗
21. Wu YY, Zhang DM, Yu J, Wang YB (2009) J Appl Phys 105:06161310.1063/1.3055362 ↗
22. Simões AZ, Pianno RFC, Ries A, Varela JA, Longo E (2006) J Appl Phys 100:08410610.1063/1.2356096 ↗
23. He L, Ling ZY (2011) J Appl Phys 110:09370810.1063/1.3657772 ↗
24. Lampert MA, Mark P (1970) Current injection in solids. Academic, New York
25. Shin JC, Hwang CS, Kim HJ, Park SO (1999) Appl Phys Lett 75:3411–341310.1063/1.125310 ↗
26. Yang F, Zhang FW, Hu GD, Zong ZH, Tang MH (2015) Appl Phys Lett 106:17290310.1063/1.4919566 ↗
27. Zhang W, Gao YQ, Kang LM, Yuan ML, Yang Q, Cheng HB, Pan W, Ouyang J (2015) Acta Mater 85:207–21510.1016/j.actamat.2014.10.063 ↗
28. Zhong N, Xiang PH, Zhang YY, Wu X, Tang XD, Yang PX, Chun CG, Chu JH (2015) J Appl Phys 118:10410210.1063/1.4930041 ↗