Design of hard surfaces with metal (Hf/V) nitride multinanolayers
Source abstract
Abstract
Physical properties as mechanical and tribological evolution on 4140 steel surfaces coated with hafnium nitride/vanadium nitride [HfN/VN] n multinanolayered systems deposited in various bilayer periods via magnetron sputtering has been exhaustively studied in this work. The coatings have been characterized in terms of structural, chemical, morphological, mechanical, and tribological properties by X-ray diffraction, X-ray photoelectron spectroscopy, atomic force microscopy, scanning and transmission electron microscopies, nanoindentation, pin-on-disc and scratch tests. Moreover, the failure mode mechanisms were observed via scanning electron microscopy. The preferential growth in the face-centered cubic (111) crystal structure for [HfN/VN] n multilayered coatings have been shown by X-ray diffraction results. The best enhancement of the mechanical behavior has been obtained when the bilayer period was 15 nm (n = 80), yielding the highest hardness (37 GPa) and elastic modulus was (351 GPa). The values of the hardness and elastic modulus were 1.48 and 1.32 times higher than the coating with n = 1, respectively, as well as the lowest friction coefficient (∼ 0.15) and the highest critical load (72 N). These results indicated significant enhancements in mechanical, tribological, and adhesion properties, compared to HfN/VN multilayered systems with bilayer period of 1200 nm (n = 1). The hardness and toughness enhancement in the multilayered coatings could be attributed to the different mechanisms that produce the layer formation with nanometric thickness due to the number of interfaces acting as obstacles for crack deflection and dissipation of crack energy. Due to the emergent characteristics of the synthesized multinanolayered material, the developed adaptive coating could be considered as higher ordered tool machining systems, capable of sustaining extreme operating conditions for industrial applications.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Ghosh, S.K., Limaye, P.K., Swain, B.P., Soni, N.L., Agrawal, R.G., Dusane, R.O., and Grover, A.K., Tribological behavior and residual stress of electrodeposited Ni/Cu multilayer films on stainless steel substrate, Surf. Coat. Tech., 2007, vol. 201, pp. 4609–4618.10.1016/j.surfcoat.2006.09.314 ↗
2. Barshilia, H.C., Jain, A., and Rajam, K.S., Structure, hardness and thermal stability of nanolayered TiN/CrN multilayer coatings, Vacuum, 2003, vol. 72, pp. 241–248.10.1016/j.vacuum.2003.08.003 ↗
3. Morant, C., Cáceres, D., Sanz, J.M., and Elizalde, E., Nano-mechanical properties of BCN/CN/BN multilayer films, Diamond Relat. Mater., 2007, vol. 16, pp. 1441–1444.10.1016/j.diamond.2006.09.024 ↗
4. Kim, S., Analysis of interfacial strengthening from composite hardness of TiN/VN and TiN/NbN multilayer hard coatings, Surf. Coat. Tech., 2004, vol. 187, pp. 47–53.10.1016/j.surfcoat.2004.01.011 ↗
5. Wu, F.-B., Tien, S.-K., and Duh, J.-G., Manufacture, microstructure and mechanical properties of CrWN and CrN/WN nanolayered coatings, Ibid., 2005, vol. 200, pp. 1514–1518.
6. Chan, Y.-C., Chen, H.-W., Chao, P.-S., Duh, J.-G., and Lee, J.-W., Microstructure control in TiAlN/SiNx multilayers with appropriate thickness ratios for improvement of hardness and anticorrosion characteristics, Vacuum, 2013, vol. 87, pp. 195–199.10.1016/j.vacuum.2012.02.052 ↗
7. Yu, L., Dong, S., Xu, J., and Kojima, I., Microstructure and hardening mechanisms in a-Si3N4/nc-TiN nanostructured multilayers, Thin Solid Films, 2008, vol. 516, pp. 1864–1870.10.1016/j.tsf.2007.09.022 ↗
8. Nordin, M., Larsson, M., and Hogmark, S., Mechanical and tribological properties of multilayered PVD TiN/CrN, TiN/MoN, TiN/NbN and TiN/TaN coatings on cemented carbide, Surf. Coat. Tech., 1998, vol. 106, pp. 234–241.10.1016/S0257-8972(98)00544-1 ↗
9. Tsai, Y.-Z. and Duh, J.-G., Tribological behavior of CrN/WN multilayer coatings grown by ion-beam assisted deposition, Ibid., 2006, vol. 201, pp. 4266–4272.10.1016/j.surfcoat.2006.08.078 ↗
10. Escobar, C., Villarreal, M., Caicedo, J.C., Aperador, W., and Prieto, P., Novel performance in physical and corrosion resistance HfN/VN coating system, Ibid., 2013, vol. 221, pp. 182–190.10.1016/j.surfcoat.2013.02.002 ↗
11. Arranz, A., Synthesis of hafnium nitride films by 0.5–5 keV nitrogen implantation of metallic Hf: an X-ray photoelectron spectroscopy and factor analysis study, Surf. Sci., 2004, vol. 563, pp. 1–12.10.1016/j.susc.2004.06.162 ↗
12. Glaser, A., Surnev, S., Ramsey, M.G., Lazar, P., Redinger, J., Podloucky, R., and Netzer, F. P., The growth of epitaxial VN (111) nanolayer surfaces, Ibid., 2007, vol. 601, pp. 4817–4823.
13. Caicedo, J.C., Amaya, C., Yate, L., Gómez, M.E., Zambrano, G., Alvarado-Rivera, J., Muñoz-Saldaña, J., and Prieto, P., TiCN/TiNbCN multilayer coatings with enhanced mechanical properties, Appl. Surf. Sci., 2010, vol. 256, pp. 5898–5904.10.1016/j.apsusc.2010.03.071 ↗
14. Stueber, M., Holleck, H., Leiste, H., Seemann, K., Ulrich, S., and Ziebert, C., Concepts for the design of advanced nanoscale PVD multilayer protective thin films, J. Alloy. Compd., 2009, vol. 483, pp. 321–333.10.1016/j.jallcom.2008.08.133 ↗
15. Oliver, W.C. and Pharr, G.M., An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments, J. Mater. Research, 1992, vol. 7, pp. 1564–1583.10.1557/JMR.1992.1564 ↗
16. Korsunsky, A.M., McGurk, M.R., Bull, S.J., and Page, T.F., On the hardness of coated systems, Surf. Coat. Tech., 1998, vol. 99, pp. 171–183.10.1016/S0257-8972(97)00522-7 ↗
17. Jehn, H.A., Improvement of the corrosion resistance of PVD hard coating-substrate systems, Ibid., 2000, vol. 125, pp. 212–217.10.1016/S0257-8972(99)00551-4 ↗
18. Ipaz, L., Caicedo, J.C., Esteve, J., Espinoza-Beltran, F.J., and Zambrano, G., Improvement of mechanical and tribological properties in steel surfaces by using titanium-aluminum/titanium-aluminum nitride multilayered system, Appl. Surf. Sci., 2012, vol. 258, pp. 3805–3814.10.1016/j.apsusc.2011.12.033 ↗
19. Holleck, H., Lahres, M., and Woll, P., Multilayer coatings-influence of fabrication parameters on constitution and properties, Surf. Coat. Tech., 1990, vol. 41, pp. 179–190.10.1016/0257-8972(90)90166-A ↗
20. Yashar, P.C. and Sproul, W.D., Nanometer scale multilayered hard coatings, Vacuum, 1999, vol. 55, pp. 179–190.10.1016/S0042-207X(99)00148-7 ↗
21. Park, J.-K. and Baik, Y.-J., The crystalline structure, hardness and thermal stability of AlN/CrN superlattice coating prepared by D.C. magnetron sputtering, Surf. Coat. Tech., 2005, vol. 200, pp. 1519–1523.10.1016/j.surfcoat.2005.08.099 ↗
22. Wang, X.C., Mi, W.B., Jiang, E.Y., and Bai, H.L., Structure and mechanical properties of titanium nitride/carbon nitride multilayers, Appl. Surf. Sci., 2009, vol. 255, pp. 4005–4010.10.1016/j.apsusc.2008.10.066 ↗
23. Kim, G.S., Lee, S.Y., and Hahn, J.H., Synthesis of CrN/AlN superlattice coatings using closed-field unbalanced magnetron sputtering process, Surf. Coat. Tech., 2002, vol. 171, pp. 91–95.10.1016/S0257-8972(03)00244-5 ↗
24. Lewis, D.B., Wadsworth, I., Mu, W., Kuzeljr, R., and Valvoda, V., Structure and stress of TiAlN/CrN superlattice coatings as a function of CrN layer thickness, Ibid., 1999, vols. 116–119, pp. 284–291.10.1016/S0257-8972(99)00132-2 ↗
25. Archard, J.F., Contact and Rubbing of Flat Surfaces, J. Appl. Phys., 1953, vol. 24, no. 8, pp. 981–987.10.1063/1.1721448 ↗
26. Leyland, A. and Matthews, A., On the significance of the H/E ratio in wear control: a nanocomposite coating approach to optimized tribological behavior, Wear, 2000, vol. 246, pp. 1–11.10.1016/S0043-1648(00)00488-9 ↗
27. Podgornik, B., Hogmark, S., Sandberg O., and Leskovsek, V., Wear resistance and anti-sticking properties of duplex treated forming tool steel, Ibid., 2003, vol. 254, pp. 1113–1121.10.1016/S0043-1648(03)00322-3 ↗
28. Holmberg, K., Ronkainen, H., and Matthews, A., Tribology of thin coatings, Ceram. Int., 2000, vol. 26, pp. 787–795.10.1016/S0272-8842(00)00015-8 ↗