Activation of cement hydration with carbon dioxide
Source abstract
Abstract
Additions of carbon dioxide to hydrating concrete have been observed to result in performance benefits. In this study, oil-well cement (selected for its very low initial carbonate content) was hydrated in the presence and absence of pure CO2 gas. The evolution of the products and reactants was assessed through isothermal calorimetry, Quantitative X-ray Diffraction (QXRD), Loss on Ignition, and Total Inorganic Carbon. A one minute exposure to carbon dioxide gas during mixing improved the heat of hydration though 24 h by 8%. The amount of C-S-H formed increased by 20%, and the estimated degree of hydration increased by 23%. The carbon dioxide promoted the formation of calcium carbonate that was observed in the sample immediately after treatment with carbon dioxide. The carbonate was initially amorphous calcium carbonate not detectable with QXRD, but it changed over 24 h to crystalline calcite (CaCO3) detectable by QXRD.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Concrete and Cement Materials Research · Building materials and conservation · Microbial Applications in Construction Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
CarbonCure Technologies, 60 Trider Crescent, Dartmouth, Canada
Department of Earth, Ocean and Atmospheric Sciences, University of British Columbia, Vancouver, Canada
Funding
Natural Sciences and Engineering Research Council of Canada
References (37)
Show source-provided references
1. 10.5194/essd-8-605-201610.5194/essd-8-605-2016 ↗
2. 10.1016/j.conbuildmat.2016.05.08010.1016/j.conbuildmat.2016.05.080 ↗
3. 10.1016/j.conbuildmat.2016.10.01710.1016/j.conbuildmat.2016.10.017 ↗
4. 10.1016/j.jcou.2017.07.00310.1016/j.jcou.2017.07.003 ↗
5. 10.1016/j.jhazmat.2004.04.01910.1016/j.jhazmat.2004.04.019 ↗
6. 10.1139/L09-14010.1139/L09-140 ↗
7. 10.1061/(ASCE)MT.1943-5533.000046210.1061/(ASCE)MT.1943-5533.0000462 ↗
8. 10.1016/j.cemconcomp.2016.10.00710.1016/j.cemconcomp.2016.10.007 ↗
9. 10.1111/jace.1979.62.issue-3-410.1111/jace.1979.62.issue-3-4 ↗
10. 10.1016/j.jclepro.2017.08.19410.1016/j.jclepro.2017.08.194 ↗
11. Shi C · Concr Int · 2009 · 31 · 39
12. 10.1016/j.conbuildmat.2011.06.02010.1016/j.conbuildmat.2011.06.020 ↗
13. El-Hassan H · ACI Mater J · 2013 · 110 · 441
14. 10.1080/21650373.2013.79737310.1080/21650373.2013.797373 ↗
15. 10.1080/19648189.2015.104207010.1080/19648189.2015.1042070 ↗
16. 10.1016/S1359-8368(03)00052-010.1016/S1359-8368(03)00052-0 ↗
17. 10.3141/2141-0210.3141/2141-02 ↗
18. 10.1016/j.ijfatigue.2006.10.00410.1016/j.ijfatigue.2006.10.004 ↗
19. 10.3141/2141-1110.3141/2141-11 ↗
20. 10.1680/adcr.9.0001610.1680/adcr.9.00016 ↗
21. 10.1016/j.egypro.2012.01.15810.1016/j.egypro.2012.01.158 ↗
22. 10.1617/s11527-012-9940-010.1617/s11527-012-9940-0 ↗
23. 10.1016/S0008-8846(99)00128-310.1016/S0008-8846(99)00128-3 ↗
24. 10.1002/(ISSN)1521-374910.1002/(ISSN)1521-3749 ↗
25. 10.1016/S0008-8846(01)00558-010.1016/S0008-8846(01)00558-0 ↗
26. 10.1016/j.tca.2007.07.02210.1016/j.tca.2007.07.022 ↗
27. 10.1016/S0040-6031(98)00348-710.1016/S0040-6031(98)00348-7 ↗
28. 10.6028/NIST.IR.575610.6028/NIST.IR.5756 ↗
29. 10.1111/j.1151-2916.1997.tb02785.x10.1111/j.1151-2916.1997.tb02785.x ↗
30. 10.1016/j.apgeochem.2009.09.01810.1016/j.apgeochem.2009.09.018 ↗
31. 10.1021/ja106959p10.1021/ja106959p ↗
32. Molina L. On predicting the influence of curing conditions on the degree of hydration. Cement och Betong Institututet; 1992; p. 96. (Report No.: 1992:5).
33. Steinour HH · J Am Concr Inst · 1959 · 55 · 905
34. 10.1016/j.cemconres.2011.10.00510.1016/j.cemconres.2011.10.005 ↗
35. 10.3151/jact.7.35510.3151/jact.7.355 ↗
36. 10.1039/C0NR00589D10.1039/C0NR00589D ↗
37. 10.1155/2013/71017510.1155/2013/710175 ↗