Steel reinforcement corrosion in strain hardening cementitious composites (SHCC): the role of multiple microcracks and surface impregnation
Source abstract
Abstract
Fiber reinforcement in SHCCs causes the formation of many fine cracks under imposed strain. In this way, ductility is increased, but water and chloride may still quickly penetrate deep into microcracks by capillary action. As a consequence, corrosion of steel rebars can be initiated at early stage. In this contribution, multiple cracked steel reinforced SHCC specimens with and without hydrophobic surface impregnation were prepared. The corrosion of the rebars in multi-cracked SHCCs was monitored and it can be concluded that multiple cracked SHCCs with fine small cracks exhibit a higher corrosion resistance to steer reinforcement than fractured ordinary mortar. The corrosion of steel reinforcement initiates from the bottom interface between the rebar and matrix. Steel reinforcement corrosion can be reduced remarkably through hydrophobic surface impregnation, even in the cracked state. In this way, the working life of steel strengthened SHCC elements exposed to erosive environments could be substantially prolonged.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Innovative concrete reinforcement materials · Concrete Corrosion and Durability · Structural Behavior of Reinforced Concrete
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Civil Engineering, Qingdao University of Technology, Qingdao, PR China
Center for Durability & Sustainability Studies of Shandong Province, Qingdao University of Technology, Qingdao, PR China
References (52)
Show source-provided references
1. 10.1080/21650373.2021.189999810.1080/21650373.2021.1899998 ↗
2. 10.1080/21650373.2016.116923110.1080/21650373.2016.1169231 ↗
3. 10.1080/21650373.2021.187527310.1080/21650373.2021.1875273 ↗
4. 10.1016/j.cemconres.2018.03.00310.1016/j.cemconres.2018.03.003 ↗
5. 10.1080/21650373.2017.139423610.1080/21650373.2017.1394236 ↗
6. 10.1016/j.conbuildmat.2021.12310010.1016/j.conbuildmat.2021.123100 ↗
7. 10.1016/j.conbuildmat.2019.11784510.1016/j.conbuildmat.2019.117845 ↗
8. 10.1016/j.cemconres.2017.05.01810.1016/j.cemconres.2017.05.018 ↗
9. 10.1016/j.cemconres.2007.04.00910.1016/j.cemconres.2007.04.009 ↗
10. 10.3151/jact.1.21510.3151/jact.1.215 ↗
11. 10.1016/j.mtcomm.2020.10142110.1016/j.mtcomm.2020.101421 ↗
12. 10.1617/s11527-009-9544-510.1617/s11527-009-9544-5 ↗
13. Li V. · 2010 · 181
14. 10.1007/s40069-017-0205-810.1007/s40069-017-0205-8 ↗
15. 10.3390/s2005139410.3390/s20051394 ↗
16. 10.1016/j.compositesb.2020.10828910.1016/j.compositesb.2020.108289 ↗
17. 10.1016/j.conbuildmat.2020.11965510.1016/j.conbuildmat.2020.119655 ↗
18. 10.1002/suco.20190020010.1002/suco.201900200 ↗
19. Li Z. · 2003
20. 10.1016/j.conbuildmat.2020.12100810.1016/j.conbuildmat.2020.121008 ↗
21. Sahmaran M · Aci Mater J · 2007 · 104 · 604
22. 10.1016/S0008-8846(97)00031-810.1016/S0008-8846(97)00031-8 ↗
23. 10.3151/jact.9.15910.3151/jact.9.159 ↗
24. 10.1016/j.conbuildmat.2019.07.05210.1016/j.conbuildmat.2019.07.052 ↗
25. 10.1016/j.cemconcomp.2017.03.00610.1016/j.cemconcomp.2017.03.006 ↗
26. 10.1016/j.cemconcomp.2016.03.00210.1016/j.cemconcomp.2016.03.002 ↗
27. 10.1016/j.conbuildmat.2018.05.16310.1016/j.conbuildmat.2018.05.163 ↗
28. 10.1016/j.nima.2010.04.11910.1016/j.nima.2010.04.119 ↗
29. 10.1016/j.cemconcomp.2016.12.00610.1016/j.cemconcomp.2016.12.006 ↗
30. 10.1016/j.conbuildmat.2014.11.06210.1016/j.conbuildmat.2014.11.062 ↗
31. 10.1016/j.conbuildmat.2016.03.20610.1016/j.conbuildmat.2016.03.206 ↗
32. 10.3151/jact.12.34010.3151/jact.12.340 ↗
33. 10.1016/j.conbuildmat.2019.03.24710.1016/j.conbuildmat.2019.03.247 ↗
34. 10.3151/jact.2.20710.3151/jact.2.207 ↗
35. 10.1016/j.cemconcomp.2009.11.00110.1016/j.cemconcomp.2009.11.001 ↗
36. 10.1515/rbm-2005-592610.1515/rbm-2005-5926 ↗
37. 10.1016/j.conbuildmat.2017.12.05710.1016/j.conbuildmat.2017.12.057 ↗
38. ASTM C876-15 · 2015
39. ASTM G59-97 · 2014
40. 10.3151/jact.5.28510.3151/jact.5.285 ↗
41. 10.3151/jact.4.36910.3151/jact.4.369 ↗
42. 10.1016/j.jclepro.2020.12068210.1016/j.jclepro.2020.120682 ↗
43. 10.1016/j.conbuildmat.2014.09.02610.1016/j.conbuildmat.2014.09.026 ↗
44. 10.1617/s11527-010-9688-310.1617/s11527-010-9688-3 ↗
45. Ahlström J. Corrosion of steel in concrete at various moisture and chloride levels Report TVBM 133, Lund University2015.
46. 10.1016/j.compositesb.2012.09.08510.1016/j.compositesb.2012.09.085 ↗
47. 10.1680/macr.2008.61.8.57110.1680/macr.2008.61.8.571 ↗
48. 10.1016/j.cemconcomp.2021.10429210.1016/j.cemconcomp.2021.104292 ↗
49. 10.1016/S0958-9465(02)00089-610.1016/S0958-9465(02)00089-6 ↗
50. Attanayaka U · 2002
51. Zhang P. · 2010
52. Lunk P · 1998