journal article·2024-09-01

Fracture Toughness Measurement for B4C Composites with Hierarchical Microstructures: Comparison of Micro-indentation and Four-Point Bending Methods

Jingyao Dai, Jogender Singh, Namiko Yamamoto

Journal of Testing and Evaluation· Volume 52· Issue 5
Publisher page

Abstract

ABSTRACT Because of the advantage of simple preparation of small-sized samples, micro-indentation has been widely adapted to evaluate the fracture toughness of materials including brittle ceramic composites. However, fracture toughness results measured by micro-indentation often differ from those measured by standardized methods such as four-point bending. Such differences can be attributed to loading condition differences (contact load for micro-indentation), fracture mechanism differences, and the associated usage of empirically obtained formulas for fracture toughness evaluation. These differences are expected to amplify when testing hierarchically microstructured ceramic composites, as multiple and complex fracture mechanisms can be triggered at different size scales and loads. Here, we compared the fracture toughness measured using micro-indentation (fracture under compression) and four-point bending (surface crack in flexure method) about three types of hierarchically microstructured boron carbide composites: one reinforced with sub-micron and micron-sized graphite platelets, one reinforced with titanium diboride particulates, and one reinforced with both. The fracture toughness value differences were correlated with fracture and deformation mechanisms observed after the micro-indentation and four-point bending tests. This study provides insights into the origin of the toughness value differences, and also insights into fair interpretation of micro-indentation data when the four-point bending test option is not available for brittle hierarchical composites.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Aerospace Engineering, The Pennsylvania State University 1 , 229 Hammond Bldg., University Park, PA 16802 ,

Applied Research Laboratory, The Pennsylvania State University 2 , 4000D Applied Science Bldg., University Park, PA 16802 ,

Department of Aerospace Engineering, The Pennsylvania State University 3 , 229 Hammond Bldg., University Park, PA 16802 ,

Funding

Office of Naval Research

References (54)

Show source-provided references
1. Designing Highly Toughened Hybrid Composites through Nature-Inspired Hierarchical Complexity10.1016/j.actamat.2009.03.003 ↗
2. Resilient 3D Hierarchical Architected Metamaterials10.1073/pnas.1509120112 ↗
3. Strong, Tough and Stiff Bioinspired Ceramics from Brittle Constituents10.1038/nmat3915 ↗
4. Tough, Bio-inspired Hybrid Materials10.1126/science.1164865 ↗
5. Fabrication of Ceramic Components with Hierarchical Porosity10.1007/s10853-010-4708-9 ↗
6. Standard Test Methods for Determination of Fracture Toughness of Advanced Ceramics at Ambient Temperature , ASTM C1421-18 (West Conshohocken, PA: ASTM International, approved January 1, 2018). https://doi.org/10.1520/C1421-1810.1520/C1421-18 ↗
7. A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: I, Direct Crack Measurements10.1111/j.1151-2916.1981.tb10320.x ↗
8. A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: II, Strength Method10.1111/j.1151-2916.1981.tb10321.x ↗
9. On the Vickers Indentation Fracture Toughness Test10.1111/j.1551-2916.2006.01482.x ↗
10. Fabrication and Characterization of FAST Sintered Micro/Nano Boron Carbide Composites with Enhanced Fracture Toughness10.1016/j.jeurceramsoc.2020.05.074 ↗
11. Damage Development in an Armor Ceramic under Quasi-static Indentation10.1111/j.1551-2916.2011.04472.x ↗
12. Nonbrittle Nanopore Deformation of Anodic Aluminum Oxide Membranes10.1111/jace.15367 ↗
13. Inelastic Deformation under Indentation and Scratch Loads in a Zrb2-SiC Composite10.1016/j.jeurceramsoc.2009.04.014 ↗
14. Fracture Toughness of Ceramics by the Vickers Indentation Crack Length Method: A Critical Review
15. Hierarchical Toughening of Laminated Nanocomposites with Three-Dimensional Graphene/Carbon Nanotube/SiC Nanowire10.1016/j.mtnano.2022.100180 ↗
16. Hierarchical Composites of B4C–TiB2 Eutectic Particles Reinforced with Ti10.1016/j.ceramint.2020.07.312 ↗
17. Elastic Properties of Boron Carbide10.1007/BF00720044 ↗
18. Boron Carbide—A Comprehensive Review10.1016/0955-2219(90)90048-K ↗
19. Bauccio · 1994
20. Matkovich · 197710.1007/978-3-642-66620-9 ↗
21. Hardness and Fracture Toughness of Pressureless-Sintered Boron Carbide (B4C)10.1111/j.1151-2916.2002.tb00260.x ↗
22. Synthesis and Consolidation of Boron Carbide: A Review10.1179/095066009X12506721665211 ↗
23. Microcracking in B4C-TiB2 Composites10.1111/j.1151-2916.1995.tb08671.x ↗
24. High Strength-High Toughness B4C-Tib2 Composites10.1023/A:1006766910536 ↗
25. High Strength B4C-TiB2 Composites Fabricated by Reaction Hot-Pressing10.1016/S0955-2219(02)00274-1 ↗
26. Microstructure and Mechanical Properties of Pulsed Electric Current Sintered B4C-TiB2 Composites10.1016/j.msea.2010.10.022 ↗
27. In Situ Synthesis and Densification of Submicrometer-Grained B4C-TiB2 Composites by Pulsed Electric Current Sintering10.1016/j.jeurceramsoc.2010.10.028 ↗
28. Investigation on Addition of ZrO2-3 Mol% Y2O3 Powder on Sintering Behavior and Mechanical Properties of B4C10.1007/s10853-006-0355-6 ↗
29. Microstructure, Mechanical and Thermal Properties of B4C/CNT Composites with Al Additive10.1016/j.jnucmat.2013.02.061 ↗
30. Effect of Particle Size, Heating Rate and CNT Addition on Densification, Microstructure and Mechanical Properties of B4C Ceramics10.1016/j.ceramint.2015.03.167 ↗
31. Electrically Conductive Graphene Nanoplatelet/Boron Carbide Composites with High Hardness and Toughness10.1016/j.scriptamat.2015.12.008 ↗
32. Enhancing Toughness in Boron Carbide with Reduced Graphene Oxide10.1111/jace.13943 ↗
33. Macro-scale Testing and Micromechanics Modeling of Fracture Behaviors for Boron Carbide Composites with Hierarchical Microstructures10.2514/6.2021-0405 ↗
34. Fracture Toughness Determinations by Indentation10.1111/j.1151-2916.1976.tb10991.x ↗
35. Reply to ‘Comment on “Elastic/Plastic Indentation Damage in Ceramics: The Median/Radial Crack System,”’10.1111/j.1151-2916.1981.tb15909.x ↗
36. Evaluation of KIc of Brittle Solids by the Indentation Method with Low Crack-to-Indent Ratios10.1007/BF00724706 ↗
37. Material Properties of Titanium Diboride10.6028/jres.105.057 ↗
38. Elastic Properties of Isotropic Graphite10.1080/14786436808223035 ↗
39. J. Dai, “Toughening of Boron Carbide Composites with Hierarchical Microstructuring” (PhD diss., Pennsylvania State University,2021).10.12783/asc36/35877 ↗
40. Experimental Observations of Amorphization in Stoichiometric and Boron-Rich Boron Carbide10.1016/j.actamat.2019.09.052 ↗
41. Amorphization-Induced Volume Change and Residual Stresses in Boron Carbide10.1111/jace.15417 ↗
42. Directionally Solidified Boride and Carbide Eutectic Ceramics10.1111/jace.14287 ↗
43. Micromechanics-Based Simulation of B4C-TiB2 Composite Fracture under Tensile Load10.1016/j.jeurceramsoc.2022.07.010 ↗
44. Residual Stress Effects in Sharp Contact Cracking10.1007/BF00551043 ↗
45. Crack Propagation during Vickers Indentation of Zirconia Ceramics10.1016/j.ceramint.2020.05.225 ↗
46. Contact-Damage-Resistant Ceramic/Single-Wall Carbon Nanotubes and Ceramic/Graphite Composites10.1038/nmat1161 ↗
47. Pressureless Sintering and Properties of Boron Carbide-Titanium Diboride Composites by In Situ Reaction10.4028/www.scientific.net/KEM.525-526.321 ↗
48. Effects of B4C Particle Size on the Microstructures and Mechanical Properties of Hot-Pressed B4C–TiB2 Composites10.1016/j.ceramint.2018.08.200 ↗
49. Microstructure and Mechanical Properties of B4C–TiB2 Ceramic Composites Prepared via a Two-Step Method10.1016/j.jeurceramsoc.2021.07.013 ↗
50. Spark Plasma Sintering of B4C and B4C-TiB2 Composites: Deformation and Failure Mechanisms under Quasistatic and Dynamic Loading10.1016/j.jeurceramsoc.2021.01.044 ↗
51. Microstructure and Mechanical Properties of B4C-TiB2 Composite Ceramic Fabricated by Reactive Spark Plasma Sintering10.1016/j.ijrmhm.2020.105307 ↗
52. Effects of Processing on Mechanical Properties of B4C-Graphene Composites Fabricated by Hot Pressing10.1016/j.msea.2021.140872 ↗
53. Boron Carbide/Graphene Platelet Ceramics with Improved Fracture Toughness and Electrical Conductivity10.1016/j.jeurceramsoc.2017.04.061 ↗
54. In-Situ Graphene Platelets Formation and Its Suppression during Reactive Spark Plasma Sintering of Boron Carbide/Titanium Diboride Composites10.1016/j.jeurceramsoc.2021.06.053 ↗