journal article·2021-11-01

Studies on the Spatial Location Method of Corrosion Defect in Bridge Cable Considering Self-Magnetic Flux Leakage Effect

Runchuan Xia, Hong Zhang, Jianting Zhou, Leng Liao, Haibo Di, Zeyu Zhang

Journal of Testing and Evaluation· Volume 49· Issue 6
Publisher page

Abstract

ABSTRACT To detect the hidden defects of ferromagnetic components, it is crucial to first locate the position of defects. In this paper, the three-dimensional magnetic dipole model of a solid columnar structure with a sector cube defect was built to theoretically explain the self-magnetic flux leakage effect of the bridge-stayed cable. The uniform or linear distribution of charge density on specific defect planes was considered in the model. Then, an experimental study on the defective steel strand cable specimens under different corrosion degrees was carried out. The results show that the corrosion accelerates the variation of magnetic signal Bz near the corrosion region, and the phenomenon is consistent with the theoretical model. Moreover, the relationship between the normalized signal Bznor and the corrosion factor αφ reveals the influence of the corrosion defect on the magnetic signal intensity in different detection positions, demonstrating the three-order polynomial growth trend. Combined with the axial and the circumferential scanning, the spatial location method of the corrosion defect was proposed for the detection of the bridge-stayed cable.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Non-Destructive Testing Techniques · Welding Techniques and Residual Stresses · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Chongqing Jiaotong University, State Key Laboratory of Mountain Bridge and Tunnel Engineering 1 , 66 Xuefu Ave., Nan’an 400074, Chongqing ,

Chongqing Jiaotong University, School of Civil Engineering 2 , 66 Xuefu Ave., Nan’an 400074, Chongqing ,

Chongqing Jiaotong University, School of Civil Engineering 3 , 66 Xuefu Ave., Nan’an 400074, Chongqing ,

Chongqing Jiaotong University, School of Materials Science and Engineering 4 , 66 Xuefu Ave., Nan’an 400074, Chongqing ,

Sichuan Yakang Expressway Co., Ltd., Scientific Research Project Department 5 , Longxi Village, Yadong Rd., Ya’an 625000, Sichuan ,

Guizhou Expressway Group Co., Ltd., Scientific Research Project Department 6 , Huaxi District, Development Ave., Guiyang 550025, Guizhou ,

Funding

National Science Fund for Distinguished Young Scholars · Chongqing Engineering Laboratory for Transportation Engineering Application Robot Open Fund · Post-graduate Education Innovation Fund Project in Chongqing Jiaotong University · Science and Technology Research Program of Chongqing Municipal Education Commission of China · National Key Research and Development Program of China · National Natural Science Foundation of China

References (43)

Show source-provided references
1. Mechanical Behavior of Chinese Woven Timber Arch Bridges10.1016/j.engstruct.2019.05.068 ↗
2. Research Progress on Corrosion Prevention Technology of Main Cables for Suspension Bridge
3. Non-Destructive Monitoring of Corrosion Extent in Steel Rope Wires via Barkhausen Noise Emission10.1016/j.jmmm.2019.04.017 ↗
4. Identification and Characterisation of Steel Corrosion Using Passive High Frequency RFID Sensors10.1016/j.measurement.2016.06.041 ↗
5. Probabilistic Approach for Cable Residual Strength Assessment10.1016/S0141-0296(02)00173-6 ↗
6. Potential Correlation between Corrosion-Induced Configuration Alteration and the Seismic Performance of Long-Span Cable-Stayed Bridges with Floating Systems10.1061/(ASCE)BE.1943-5592.0001153 ↗
7. 3-D FEM Simulation and Analysis on the Best Range of Lift-off Values in MFL Testing10.1520/JTE20130133 ↗
8. Analysis of MFL Model for Sucker Rod Defects and Its MFL Signal Processing10.1520/JTE20170687 ↗
9. Three-Dimensional Localization of Defects in Stay Cables Using Magnetic Flux Leakage Methods10.1023/B:JONE.0000010736.74285.b6 ↗
10. Application of Dipole Magnetic Charge Method to MFL Signal Analytical Model
11. Experimental and Theoretical Analysis of Metal Magnetic Memory Signals in the Stress Concentration Area of 45# Steel under Tensile Testing10.3233/JAE-141777 ↗
12. Detection and Characterization of Hidden Corrosion in Aircraft Lap Joints by Optical NDT Method10.1520/JTE20170389 ↗
13. A Study of Metal Properties Using the Method of Magnetic Memory10.1007/BF02469065 ↗
14. The Quantitative Interpretation by Measurement Using the Magnetic Memory Method (MMM)-based on Density Functional Theory10.1016/j.ndteint.2013.01.002 ↗
15. Quantitative Study on Corrosion of Steel Strands Based on Self-Magnetic Flux Leakage10.3390/s18051396 ↗
16. Experimental Study on Corrosion of Unstressed Steel Strand Based on Metal Magnetic Memory10.1007/s12205-019-0715-9 ↗
17. Research of Pipeline Weld Detection Based on Magnetic Memory Technology10.4028/www.scientific.net/AMR.940.222 ↗
18. Metal Magnetic Memory Testing of Welded Joints of Ferritic and Austenitic Steels10.1016/j.ndteint.2011.01.008 ↗
19. Residual Magnetic Field Variation Induced by Applied Magnetic Field and Cyclic Tensile Stress10.1016/j.ndteint.2014.01.003 ↗
20. Characterization of Stress Concentration Degree Based on 2-Dementional Magnetic Memory Signals10.4028/www.scientific.net/AMM.268-270.396 ↗
21. Stress Concentration Degree Affects Spontaneous Magnetic Signals of Ferromagnetic Steel under Dynamic Tension Load10.1016/j.ndteint.2009.08.002 ↗
22. Metal Magnetic Memory Technique Used to Predict the Fatigue Crack Propagation Behavior of 0.45 %C Steel10.1016/j.jmmm.2015.12.035 ↗
23. Characterizing the Magnetic Memory Signals on the Surface of Plasma Transferred Arc Cladding Coating under Fatigue Loads10.1016/j.jmmm.2017.07.067 ↗
24. MMM Fatigue Damage Evaluation and Life Prediction Modeling for Ferromagnetic Materials10.4028/www.scientific.net/KEM.324-325.619 ↗
25. Experiment Research on the Applicability of Magnetic Dipole Model of Magnetic Object10.3969/j.issn.1005-0930.2010.05.016 ↗
26. Theoretical Research on the Characteristics of the Self-Magnetic Leakage Field Induced by Ferromagnetic Pipelines10.1784/insi.2016.58.11.601 ↗
27. A Magnetomechanical Model for the Magnetic Memory Method10.1016/j.ijmecsci.2017.03.001 ↗
28. Strong Coupling of Magnetic and Mechanical Finite Element Analysis10.1016/s0304-8853(00)00999-9 ↗
29. Theoretical Studies of Metal Magnetic Memory Technique on Magnetic Flux Leakage Signals10.1016/j.ndteint.2009.12.006 ↗
30. Quantitative Study of Metal Magnetic Memory Signal versus Local Stress Concentration10.1016/j.ndteint.2010.05.007 ↗
31. Dipole Modeling of Stress-Dependent Magnetic Flux Leakage10.1016/j.ndteint.2018.01.004 ↗
32. Dipole Modelling of Metal Magnetic Memory for V-Notched Plates10.1784/insi.2012.55.9.498 ↗
33. Quantitative Representation of Magnetic Memory Signal
34. Research on the Stress-Magnetism Effect of Ferromagnetic Materials Based on Three-Dimensional Magnetic Flux Leakage Testing10.1016/j.ndteint.2013.11.002 ↗
35. Experimental Research on Metal Magnetic Memory Method10.1007/s11340-011-9490-3 ↗
36. Metal Magnetic Memory Signal Response to Plastic Deformation of Low Carbon Steel10.1016/j.ndteint.2013.01.005 ↗
37. Research on the Method of Predicting Corrosion Width of Cables Based on the Spontaneous Magnetic Flux Leakage10.3390/ma12132154 ↗
38. Quantitative Study of Magnetic Memory Signal Characteristic Affected by External Magnetic Field10.1016/j.measurement.2018.09.025 ↗
39. Effect of Sample Initial Magnetic Field on the Metal Magnetic Memory NDT Result10.1016/j.jmmm.2018.04.006 ↗
40. Studies on Laws of Stress-Magnetization Based on Magnetic Memory Testing Technique10.1016/j.jmmm.2017.09.050 ↗
41. Numerical Studies to Signal Characteristics with the Metal Magnetic Memory-Effect in Plastically Deformed Samples10.1016/j.ndteint.2011.12.004 ↗
42. Three-Dimensional Finite Element Analysis of Residual Magnetic Field for Ferromagnets under Early Damage10.1016/j.jmmm.2013.10.047 ↗
43. A Steel Wire Stress Measuring Sensor Based on the Static Magnetization by Permanent Magnets10.3390/s16101650 ↗