journal article·2013-08Open access

Solution‐Controlled Dissolution of Supplementary Cementitious Material Glasses at pH 13: The Effect of Solution Composition on Glass Dissolution Rates

Ruben Snellings

Abstract

Supplementary cementitious materials ( SCM s) are widely used to partially replace portland clinker in blended cements. Reducing clinker contents further without compromising the development of early strength necessitates a better assessment and enhancement of the reactivity of the available SCM s. To this purpose, the reactivity of synthesized calcium aluminosilicate glasses covering a compositional range from blast‐furnace slags (BFS) over fly ashes to silica fume was analyzed by dissolution experiments. Initial glass dissolution rates were measured at 20°C and pH 13, and with varying initial concentrations of aqueous Al , Ca , and Si . At pH 13, glass dissolution rates were observed to scale linearly with the glass Ca /( Al + Si ) molar ratio. Ca ‐rich blast‐furnace type glass dissolution was shown to be up to one order of magnitude faster than tectosilicate fly ash and silica fume type glass dissolution, supporting different pathways to dissolution. In solutions that are strongly undersaturated with respect to hydrous glass and hydration products, glass dissolution rates are independent of changes in solution undersaturation and aqueous Si activity. In contrast, dissolution rates decrease with aqueous Ca concentration for all glasses and with aqueous Al concentration for tectosilicate‐type glasses. The insights gained are instrumental in finding ways to enhance SCM reactivity.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Laboratory of Construction Materials Institute of Materials Ecole Polytechnique Fédérale de Lausanne Ecublens 1015 Switzerland

Funding

European Community

References (53)

Show source-provided references
1. 10.1016/j.cemconres.2004.01.02110.1016/j.cemconres.2004.01.021 ↗
2. 10.1016/j.cemconres.2007.09.02510.1016/j.cemconres.2007.09.025 ↗
3. 10.1016/j.cemconres.2011.03.01910.1016/j.cemconres.2011.03.019 ↗
4. World Business Council for Sustainable Development Cement Technology Roadmap 2009 Carbon Emissions Reductions up to 2050 http://www.wbcsdcement.org/pdf/technology/WBCSD-IEA_Cement%20Roadmap.pdf 2009(accessed on 12 Febraury 2013).
5. 10.2138/rmg.2012.74.610.2138/rmg.2012.74.6 ↗
6. Lime Combination and new Formations in the Trass–Lime Reactions
7. U.CostaandF.Massazza “Factors Affecting the Reaction With Lime of Pozzolans”; ppIII–6:1–17 in Proceedings of the 6th International Congress on the Chemistry of Cement Moscow 1974.
8. K.TakemotoandH.Uchikawa “Hydratation des Ciments Pouzzolaniques”; pp.IV–2:1–29 in Proceedings of the 7th International Congress on the Chemistry of Cement Paris 1980.
9. 10.1016/0008-8846(94)90162-710.1016/0008-8846(94)90162-7 ↗
10. 10.1016/S0008-8846(03)00252-710.1016/S0008-8846(03)00252-7 ↗
11. 10.1016/j.cemconres.2008.11.00510.1016/j.cemconres.2008.11.005 ↗
12. 10.1016/j.cemconres.2008.11.00810.1016/j.cemconres.2008.11.008 ↗
13. Corrosion of Granulated Glassy Blast Furnace Slags in Aqueous Solutions
14. 10.1111/j.1551-2916.2008.02787.x10.1111/j.1551-2916.2008.02787.x ↗
15. Calcium Aluminosilicate Glasses as Supplementary Cementitious Materials
16. Lang E. · 2002 · 310
17. R.Snellings G.Mertens andJ.Elsen “Evaluation of the Pozzolanic Activity of Natural Zeolite Tuffs”; in Proceedings of the 13th International Congress on the Chemistry of Cement Madrid 2011.
18. 10.1016/S0016-7037(01)00710-410.1016/S0016-7037(01)00710-4 ↗
19. 10.1016/j.gca.2009.05.02810.1016/j.gca.2009.05.028 ↗
20. 10.2138/rmg.2009.70.610.2138/rmg.2009.70.6 ↗
21. 10.1016/j.gca.2005.09.01710.1016/j.gca.2005.09.017 ↗
22. 10.1111/jace.1209810.1111/jace.12098 ↗
23. 10.1016/j.cemconres.2010.09.01110.1016/j.cemconres.2010.09.011 ↗
24. GEM‐Selektor Geochemical Modeling Package: Revised Algorithm and GEMS3K Numerical Kernel for Coupled Simulation Codes
25. 10.1016/j.cemconres.2007.08.01710.1016/j.cemconres.2007.08.017 ↗
26. Three‐Dimensional Network Structure of Quenched Melts (Glass) in the System SiO2–NaAlO2, SiO2–CaAl2O4 and SiO2–MgAl2O4
27. 10.1016/0022-3093(90)90263-L10.1016/0022-3093(90)90263-L ↗
28. 10.1016/j.chemgeo.2006.01.01910.1016/j.chemgeo.2006.01.019 ↗
29. 10.1016/0008-8846(83)90002-910.1016/0008-8846(83)90002-9 ↗
30. 10.1016/j.jeurceramsoc.2005.07.05310.1016/j.jeurceramsoc.2005.07.053 ↗
31. 10.1007/978-0-387-73563-4_610.1007/978-0-387-73563-4_6 ↗
32. 10.1016/0016-7037(94)90218-610.1016/0016-7037(94)90218-6 ↗
33. 10.1016/S0009-2541(97)00079-X10.1016/S0009-2541(97)00079-X ↗
34. 10.1016/S0009-2541(99)00055-810.1016/S0009-2541(99)00055-8 ↗
35. Mechanism, Rates and Consequences of Basaltic Glass Dissolution: II. An Experimental Study of the Dissolution Rates of Basaltic Glass as a Function of pH and Temperature10.1016/S0016-7037(03)00176-5 ↗
36. 10.1016/j.gca.2005.10.01610.1016/j.gca.2005.10.016 ↗
37. 10.1016/j.gca.2004.05.02710.1016/j.gca.2004.05.027 ↗
38. 10.1016/0022-3093(84)90151-010.1016/0022-3093(84)90151-0 ↗
39. 10.1016/S0883-2927(02)00245-710.1016/S0883-2927(02)00245-7 ↗
40. 10.1111/j.1551-2916.2007.02101.x10.1111/j.1551-2916.2007.02101.x ↗
41. 10.2475/ajs.282.3.23710.2475/ajs.282.3.237 ↗
42. A General Rate Equation for Nuclear Waste Glass Corrosion
43. 10.1016/0016-7037(94)90280-110.1016/0016-7037(94)90280-1 ↗
44. 10.1016/S0016-7037(98)00036-210.1016/S0016-7037(98)00036-2 ↗
45. 10.1016/0016-7037(94)90281-X10.1016/0016-7037(94)90281-X ↗
46. 10.1016/S0016-7037(01)00664-010.1016/S0016-7037(01)00664-0 ↗
47. 10.1016/0016-7037(94)90190-210.1016/0016-7037(94)90190-2 ↗
48. 10.1111/jace.1209810.1111/jace.12098 ↗
49. 10.1016/j.jnucmat.2012.12.03210.1016/j.jnucmat.2012.12.032 ↗
50. 10.1016/j.gca.2011.05.00510.1016/j.gca.2011.05.005 ↗
51. 10.1016/j.cemconres.2010.12.00110.1016/j.cemconres.2010.12.001 ↗
52. 10.1016/j.cemconres.2010.07.00410.1016/j.cemconres.2010.07.004 ↗
53. 10.1016/j.cemconres.2011.11.01010.1016/j.cemconres.2011.11.010 ↗