Thermal Expansion of Al 2 O 3 , BeO, MgO, B 4 C, SiC, and TiC Above 1000°C.
Source abstract
Abstract
Thermal‐expansion data on Al 2 O 3 , BeO, MgO, B 4 C, SiC, and TiC were obtained to the temperatures where permanent deformation begins, due to sintering or other causes. The thermal expansion for these materials was found to be approximately linear over the measured temperature range. But as a linear extrapolation to room temperature was not possible, the coefficient of thermal expansion is not a constant over this temperature range. The results are compared with the latest published data for each material. The average coefficients of linear thermal expansion are given as follows: image All BeO specimens which were heated to above 2050°C. had a very large expansion. Visual examination of the cooled specimens revealed that they had bent and cracked, the physical dimensions had enlarged, and the color had changed to a bright milky white. A brief discussion of the probable reasons for these changes is given. In the attempt to extend the expansion measurements, the melting point of BeO was obtained. A specimen of hot‐pressed BeO melted at 2450°± 30°C., whereas a slip‐cast BeO specimen melted at 2470°± 20° C.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. N. S.RasorandJ. D.McClelland “Thermal Properties of Materials: I Properties of Graphite Molybdenum. and Tantalum to Their Destruction Temperature ”WADC‐TR‐56‐400 Part I Wright Air Development Center Wright‐Patterson.Air Force Base Ohio 1956 August.
2. D. J.Klein “Measurement of Crystallographic Thermal Expansion of Alpha Alumina and Beryllia to Elevated Temperatures Emphasizing Anistropic Effect ”NAA‐SR‐2542 U. S. Atomic Energy Commission Technical Information Service Oak Ridge Tenn. August 1 1958.
3. 10.1111/j.1151-2916.1956.tb15619.x10.1111/j.1151-2916.1956.tb15619.x ↗
4. Directional Dilatation of Crystal Lattices at Elevated Temperatures
5. Thermal Expansion of Some Refractory Oxides
6. Etherington H. · 1948
7. Long R. E. · 1955
8. 10.6028/jres.035.02810.6028/jres.035.028 ↗
9. Crawford J. N. · 1949
10. Campbell I. E. · 1956 · 63
11. 10.1111/j.1151-2916.1950.tb12782.x10.1111/j.1151-2916.1950.tb12782.x ↗
12. Chang Roger · 195810.2172/4335018 ↗
13. A Thermal Expansion Apparatus with a Silicon Carbide Dilatometer for Temperatures to 1500°C.,” Am
14. F. A.MauerandL. H.Bolz “Thermal Expansion of Cermet Components by High‐Temperature X‐Ray Diffraction ” WADC‐TR‐ 55–473 Wright Air Development Center. Wright‐Patterson Air Force Base Ohio December 1955.