Densification of ZrB 2 –TaSi 2 and HfB 2 –TaSi 2 Ultra‐High‐Temperature Ceramic Composites
Source abstract
Abstract
The microstructure of fully dense hot‐pressed ultra‐high‐temperature ceramics (UHTCs), namely ZrB 2 and HfB 2 containing 15 vol% of TaSi 2 , was characterized by X‐ray diffraction, scanning electron microscopy (SEM), and transmission electron microscopy (TEM). ZrB 2 and HfB 2 grains displayed a core–shell structure: the core was constituted by the original MB 2 grain and the shell by a (M, Ta)B 2 solid solution, which grew epitaxially on the core. The compositional misfit between core–shell was accommodated by low‐angle grain boundaries and dislocations pile‐up, especially pronounced in the ZrB 2 ‐based composite, where a higher amount of Ta entered the boride lattice. Ta 5 Si 3 , Ta 4.8 Si 3 C 0.3 , and Ta 5 SiB 2 , with Zr or Hf impurities, were detected at the triple points and wetting of the grain boundaries by a Ta–Si–B–C–O amorphous phase was observed. Based on the new microstructural features detected by TEM, thermodynamic calculations and the available phase diagrams, a densification mechanism for ZrB 2 and HfB 2 with addition of TaSi 2 is proposed. The microstructures of the UHTC composites presented here are compared with composites sintered with the addition of MoSi 2 in the same amount.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Oxidation‐Based Materials Selection for 2000°C+Hypersonic Aerosurfaces
2. The Hypersonic Environment
3. Affordable Hypersonic Missiles for Long‐Range Precision Strike
4. Cutler R. A. · 1991 · 787
5. 10.1111/j.1551-2916.2004.01170.x10.1111/j.1551-2916.2004.01170.x ↗
6. 10.1002/adem.20040001610.1002/adem.200400016 ↗
7. 10.1557/jmr.2006.018010.1557/jmr.2006.0180 ↗
8. 10.1016/j.scriptamat.2007.02.04010.1016/j.scriptamat.2007.02.040 ↗
9. An Investigation of the Effect of Additions of Metal Silicides on Titanium and Zirconium Borides from the Point of View of Their Sintering Behavior and Their Resistance to Oxidation at High Temperatures
10. Talmy L. G. · 2001 · 144
11. 10.1557/jmr.2006.032110.1557/jmr.2006.0321 ↗
12. Oxidation of ZrB2 and HfB2‐Based Ultra‐High Temperature Ceramics
13. S. R.LevineandE. J.Opila “Tantalum Addition to Zirconium Diboride for Improved Oxidation Resistance ” NASA/TM—2003‐212483.
14. 10.1016/j.jallcom.2006.01.10710.1016/j.jallcom.2006.01.107 ↗
15. 10.1111/j.1551-2916.2008.02593.x10.1111/j.1551-2916.2008.02593.x ↗
16. 10.1016/0955-2219(95)00174-310.1016/0955-2219(95)00174-3 ↗
17. 10.1111/j.1551-2916.2009.03049.x10.1111/j.1551-2916.2009.03049.x ↗
18. Transmission Electron Microscopy on Zr‐ and Hf‐Borides Doped with MoSi2
19. 10.1111/j.1551-2916.2009.03040.x10.1111/j.1551-2916.2009.03040.x ↗
20. 10.1557/JMR.2002.040810.1557/JMR.2002.0408 ↗
21. German R. M. · 1996 · 432pp
22. 10.1111/j.1551-2916.2008.02420.x10.1111/j.1551-2916.2008.02420.x ↗
23. 10.1070/RC1996v065n05ABEH00021710.1070/RC1996v065n05ABEH000217 ↗
24. O–Si (Oxygen–Silicon)10.1007/s11669-007-9062-5 ↗
25. 10.1007/BF0266768810.1007/BF02667688 ↗
26. Liquidation in the System ZrO2–SiO2
27. Phase Equilibrius in the Hafnium Dioxide‐Silicon Dioxide System
28. D. A.ReeveandN. F.Bright “Phase Relations in the System Calcium Oxide–Tantalum Pentoxide–silicon dioxide ” J. Am. Ceram. Soc. 52[8]405–9(1969).
29. R. S.RothandJ. L.Waring “Effect of Oxide Additions on the Polymorphism of Tantalum Pentoxide. III. Stabilization of the Low Temperature Structure Type ” J. Res. Natl. bur. Stand. Sec. A. 74[4]485–93(1970).10.6028/jres.074A.038 ↗
30. Silicoboride der Übergangsmetalle Vanadin, Niob, Tantal, Molybdän und Wolfram
31. 10.1051/jcp/199390037310.1051/jcp/1993900373 ↗
32. 10.1111/j.1551-2916.2007.01583.x10.1111/j.1551-2916.2007.01583.x ↗
33. 10.1016/j.msea.2008.09.02410.1016/j.msea.2008.09.024 ↗
34. Ammann J. J. · 1988 · 257
35. 10.1016/0921-5093(95)10100-410.1016/0921-5093(95)10100-4 ↗
36. Microstructural Changes in β‐Si3N4 Grains Upon Crystallizing the Grain Boundary Glass
37. 10.1016/j.msea.2007.01.16410.1016/j.msea.2007.01.164 ↗