journal article·2021-07

Corrosion behavior of calcium–magnesium–aluminosilicate (CMAS) on sintered Gd 2 SiO 5 for environmental barrier coatings

Seung‐Hyeon Kim, Nobuo Nagashima, Yoshitaka Matsushita, Byung‐Nam Kim, Byung‐Koog Jang

Publisher page

Abstract

Abstract The Gd 2 SiO 5 performed high‐temperature corrosion behavior on calcium–magnesium– aluminosilicate (CMAS) for environmental barrier coatings (EBCs). The synthesized Gd 2 O 3 ‐SiO 2 powder was prepared to fabricate a sintered Gd 2 SiO 5 by spark plasma sintering (SPS) at 1400°C for 20 min. CMAS was sprinkled on the sintered Gd 2 SiO 5 surface and exposed for 2, 12, and 48 h at 1400°C by isothermal heat treatment. The main corrosion factor is Ca, and Ca 2 Gd 8 (SiO 4 ) 6 O 2 phase is formed by reacting with Gd 2 SiO 5 . Extended morphology of Ca 2 Gd 8 (SiO 4 ) 6 O 2 particles observed in the reaction area become thicker as the heat treatment time increases as the CMAS is dissolved. According to the results of high‐temperature X‐ray diffraction (HT‐XRD) and differential scanning calorimetry (DSC), CMAS melted at 1243°C or a higher temperature formed the reaction area. The Ca 2 Gd 8 (SiO 4 ) 6 O 2 phase was recrystallized and grown due to the reaction of Gd 2 SiO 5 and Ca of the CMAS components.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · Microwave Dielectric Ceramics Synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Interdisciplinary Graduate School of Engineering Science Kyushu University Fukuoka Japan

Research Center for Structural Materials National Institute for Materials Science Tsukuba Ibaraki Japan

Research Network and Facility Services Division National Institute for Materials Science Tsukuba Ibaraki Japan

Research Center for Functional Materials National Institute for Materials Science Tsukuba Ibaraki Japan

Funding

Japan Society for the Promotion of Science

References (45)

Show source-provided references
1. 10.1016/j.jeurceramsoc.2004.12.01310.1016/j.jeurceramsoc.2004.12.013 ↗
2. Lee KN · 2014
3. 10.1016/S0257-8972(96)03074-510.1016/S0257-8972(96)03074-5 ↗
4. Hot corrosion behavior and wettability of calcium–magnesium–alumina–silicate (CMAS) on LaTi2Al9O19 ceramic
5. 10.1016/j.scriptamat.2019.12.01910.1016/j.scriptamat.2019.12.019 ↗
6. 10.1016/j.jeurceramsoc.2020.06.01610.1016/j.jeurceramsoc.2020.06.016 ↗
7. 10.1016/j.jeurceramsoc.2018.11.04810.1016/j.jeurceramsoc.2018.11.048 ↗
8. 10.1111/j.1151-2916.2003.tb03466.x10.1111/j.1151-2916.2003.tb03466.x ↗
9. 10.1016/j.jeurceramsoc.2019.06.05110.1016/j.jeurceramsoc.2019.06.051 ↗
10. 10.1111/jace.1669410.1111/jace.16694 ↗
11. 10.1111/j.1551-2916.2010.03916.x10.1111/j.1551-2916.2010.03916.x ↗
12. Environmental degradation of thermal‐barrier coatings by molten deposits
13. 10.1016/j.jallcom.2016.10.26310.1016/j.jallcom.2016.10.263 ↗
14. 10.1111/jace.1732810.1111/jace.17328 ↗
15. 10.1016/j.jeurceramsoc.2018.03.01010.1016/j.jeurceramsoc.2018.03.010 ↗
16. 10.1016/j.jeurceramsoc.2020.04.05810.1016/j.jeurceramsoc.2020.04.058 ↗
17. 10.1111/jace.1225110.1111/jace.12251 ↗
18. Calcium–magnesium aluminosilicate (CMAS) interactions with ytterbium silicate environmental barrier coating material at elevated temperatures
19. 10.1016/j.ceramint.2017.02.12310.1016/j.ceramint.2017.02.123 ↗
20. 10.1146/annurev-matsci-010917-10500010.1146/annurev-matsci-010917-105000 ↗
21. 10.1016/j.actamat.2017.12.00410.1016/j.actamat.2017.12.004 ↗
22. 10.1111/j.1551-2916.2007.02175.x10.1111/j.1551-2916.2007.02175.x ↗
23. 10.1111/jace.1398210.1111/jace.13982 ↗
24. 10.1016/j.surfcoat.2015.12.05310.1016/j.surfcoat.2015.12.053 ↗
25. 10.1111/jace.1697210.1111/jace.16972 ↗
26. 10.1016/j.ceramint.2016.10.14710.1016/j.ceramint.2016.10.147 ↗
27. CMAS degradation of environmental barrier coatings
28. 10.2109/jcersj2.1621110.2109/jcersj2.16211 ↗
29. 10.1016/j.surfcoat.2015.08.06910.1016/j.surfcoat.2015.08.069 ↗
30. 10.1016/j.ceramint.2017.04.04510.1016/j.ceramint.2017.04.045 ↗
31. 10.1515/psr‐2017‐010310.1515/psr‐2017‐0103 ↗
32. 10.1111/jace.1347810.1111/jace.13478 ↗
33. 10.1016/j.surfcoat.2016.09.08810.1016/j.surfcoat.2016.09.088 ↗
34. High‐temperature corrosion of spark plasma sintered Gd2SiO5 with volcanic ash for environmental barrier coatings
35. 10.1016/j.surfcoat.2013.07.02910.1016/j.surfcoat.2013.07.029 ↗
36. 10.1016/j.jeurceramsoc.2019.08.04010.1016/j.jeurceramsoc.2019.08.040 ↗
37. 10.1016/j.surfcoat.2012.03.05110.1016/j.surfcoat.2012.03.051 ↗
38. 10.1016/j.jeurceramsoc.2020.04.02110.1016/j.jeurceramsoc.2020.04.021 ↗
39. 10.1016/j.scriptamat.2016.07.02010.1016/j.scriptamat.2016.07.020 ↗
40. 10.1016/j.jeurceramsoc.2015.03.03210.1016/j.jeurceramsoc.2015.03.032 ↗
41. Earth Planet
42. Glass Technol
43. Poirier DR · 1994
44. 10.1111/j.1551-2916.2006.01209.x10.1111/j.1551-2916.2006.01209.x ↗
45. An estimation of the surface tension for silicate glass melts at 1400°C using statistical analysis