journal article·1965-06

Electrical Conductivity in the ZrO 2 ‐Rich Region of Several M 2 O 3 —ZrO 2 Systems

D. W. STRICKLER, W. G. CARLSON

Publisher page

Abstract

The electrical conductivity of M 2 O 3 ‐ZrO 2 compositions containing 6 to 24 mole % M 2 O 3 , where M represents La, Sm, Y, Yb, or Sc, was examined. Only Sm 2 O 3 , Y 2 O 3 , and Yb 2 O 3 formed cubic solid solutions with ZrO 2 over most of this substitutional range. Scandia forms a wide cubic solid solution region with ZrO 2 at temperatures above 130°C whereas the cubic solid solution region at room temperature is narrow (6 to 8 mole % Sc 2 O 3 ). Lanthana additions to ZrO 2 produced no fluorite‐type cubic solid solutions within the compositional range investigated. Generally, the electrical conductivity of these cubic solid solutions increased as the size of the substituted cation decreased and the electrical conductivity for each binary system attained a maximum at about 10 to 12 mole % M 2 O 3 .
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Advanced ceramic materials synthesis · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Some Structural Modifications of Fluorite‐Type Phases in Systems Based on Zirconia or Hafnium Oxide
2. Phase Relations in a Portion of the System Sc2O3‐ZrO2
3. 10.1007/BF0147568510.1007/BF01475685 ↗
4. Fluorite Phase in the Svstem ZrO2‐CaO: Its Defect Structure and Electrical Conductivity
5. 10.1111/j.1151-2916.1959.tb13599.x10.1111/j.1151-2916.1959.tb13599.x ↗
6. 10.1149/1.242553710.1149/1.2425537 ↗
7. 10.1111/j.1151-2916.1964.tb14368.x10.1111/j.1151-2916.1964.tb14368.x ↗
8. 10.1149/1.242614910.1149/1.2426149 ↗
9. Electrical Resistivity of Stabilized Zirconia at Elevatcd Temperatures
10. 10.1063/1.173435510.1063/1.1734355 ↗
11. 10.1149/1.242604210.1149/1.2426042 ↗
12. Phenomena of Order‐Disorder in Inorganic Chemistry
13. Electrical Conductivity in the System ZrO2‐La2O3 Between 1000° and 1700°C
14. Physics of Solids—Electrical Conductivity of a Sintered Mixture Consisting of 87% (mole) ZrO2 and 13% (mole) La2O3 Between 1200° and 1650°C
15. 10.1016/0022-3697(64)90173-810.1016/0022-3697(64)90173-8 ↗