Grain Growth of ZnO during Bi 2 O 3 Liquid‐Phase Sintering
Source abstract
Abstract
Grain growth of ZnO during the liquid‐phase sintering of binary ZnO–Bi 2 O 3 ceramics has been studied for Bi 2 O 3 contents from 3 to 12 wt% and sintering from 900° to 1400°C. The results are considered in combination with previously published studies of ZnO grain growth in the ZnO–Bi 2 O 3 system. For the Bi 2 O 3 contents of the present study, the rate of ZnO grain growth is found to decrease with increasing Bi 2 O 3 . Activation analysis, when combined with the results of similar analyses of the previous studies, reveals a change in the rate‐controlling mechanism for ZnO grain growth. Following a low‐Bi 2 O 3 ‐content region of nearly constant activation energy values of about 150 kJ/mol, further Bi 2 O 3 additions cause an increase of the activation energy to about 270 kJ/mol. consistent with accepted models of liquid‐phase sintering, it is concluded that the rate‐controlling mechanism of ZnO grain growth during liquid‐phase sintering in the presence of Bi 2 O 3 changes from one of a phase‐boundary reaction at low Bi 2 O 3 levels to one of diffusion through the liquid phase at about the 5 to 6 wt% Bi 2 O 3 level and above.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advancements in Solid Oxide Fuel Cells · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. 10.1143/JJAP.10.73610.1143/JJAP.10.736 ↗
2. 10.1111/j.1151-2916.1986.tb04774.x10.1111/j.1151-2916.1986.tb04774.x ↗
3. 10.1063/1.32826610.1063/1.328266 ↗
4. 10.1007/BF0113296510.1007/BF01132965 ↗
5. 10.1111/j.1151-2916.1989.tb07703.x10.1111/j.1151-2916.1989.tb07703.x ↗
6. 10.1111/j.1151-2916.1990.tb05099.x10.1111/j.1151-2916.1990.tb05099.x ↗
7. Zinc Oxide Varistors—A Review
8. Kingery W. D. · 1975 · 808
9. 10.1111/j.1151-2916.1990.tb05232.x10.1111/j.1151-2916.1990.tb05232.x ↗
10. 10.1146/annurev.ms.17.080187.00150310.1146/annurev.ms.17.080187.001503 ↗
11. Sintering in the Presence of a Liquid Phase
12. 10.1007/978-1-4899-3599-110.1007/978-1-4899-3599-1 ↗
13. 10.1111/j.1151-2916.1965.tb14654.x10.1111/j.1151-2916.1965.tb14654.x ↗
14. 10.1111/j.1151-2916.1961.tb15343.x10.1111/j.1151-2916.1961.tb15343.x ↗
15. 10.1111/j.1151-2916.1968.tb11896.x10.1111/j.1151-2916.1968.tb11896.x ↗
16. 10.1111/j.1151-2916.1969.tb11975.x10.1111/j.1151-2916.1969.tb11975.x ↗
17. 10.1111/j.1151-2916.1968.tb15679.x10.1111/j.1151-2916.1968.tb15679.x ↗
18. Readey D. W. · 1988 · 485
19. 10.2109/jcersj1950.76.880_40710.2109/jcersj1950.76.880_407 ↗
20. 10.1111/j.1151-2916.1970.tb12007.x10.1111/j.1151-2916.1970.tb12007.x ↗
21. Microstructure and Phases in Nonohmic ZnO–Bi2O3 Ceramics
22. 10.1063/1.32513510.1063/1.325135 ↗
23. 10.1111/j.1151-2916.1979.tb19064.x10.1111/j.1151-2916.1979.tb19064.x ↗
24. 10.1111/j.1151-2916.1988.tb05915.x10.1111/j.1151-2916.1988.tb05915.x ↗
25. 10.1007/BF0055238510.1007/BF00552385 ↗
26. Theory of Precipitate Change by Redesolution
27. Yan M. F. · 1977 · 276
28. 10.1016/0001-6160(56)90060-810.1016/0001-6160(56)90060-8 ↗