Effect of Polystyrene Addition on Freeze Casting of Ceramic/Camphene Slurry for Ultra‐High Porosity Ceramics with Aligned Pore Channels
Source abstract
Abstract
We investigated the effect of polystyrene (PS) addition on the freezing behavior of a very dilute alumina/camphene slurry with an initial solid loading of 5 vol% for the fabrication of ultra‐high porosity ceramics with aligned pore channels. To accomplish this, slurries with various PS contents (10, 20, and 30 vol% in relation to the alumina powders) were prepared by ball milling at 60°C and then cast into molds at a constant temperature of 20°C. After removing the frozen camphene, the samples were heat treated to burn out the organic phases and sinter the alumina walls. The addition of the PS binder remarkably enhanced the green strength of the sample, making it possible to handle it without difficulty. All of the sintered samples showed ultra‐high porosities of >88% without the collapse of the porous structure, wherein the pore channels were completely interconnected. Three distinctive zones having different pore structures were observed, viz. the outer shell with elongated pores, the inner zone with long aligned pore channels, and the center with equiaxed pores. The content of the PS polymer significantly affected the pore morphologies in the three distinctive zones. In addition, it was found that the addition of the PS polymer was highly beneficial to the alignment of the pore channels.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advancements in Solid Oxide Fuel Cells · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Gibson L. J. · 1999
2. 10.1016/j.ultras.2004.05.00110.1016/j.ultras.2004.05.001 ↗
3. 10.1111/j.1151-2916.1993.tb03645.x10.1111/j.1151-2916.1993.tb03645.x ↗
4. 10.1007/978-1-4615-5811-810.1007/978-1-4615-5811-8 ↗
5. K.SchwartzwalderandA. V.Somers “Method of Making Porous Ceramic Article ” US Patent No. 3 090 094 1963.
6. 10.1016/j.matlet.2006.01.03110.1016/j.matlet.2006.01.031 ↗
7. 10.1023/A:100666582996710.1023/A:1006665829967 ↗
8. 10.1111/j.1151-2916.2003.tb03534.x10.1111/j.1151-2916.2003.tb03534.x ↗
9. 10.1111/j.1551-2916.2005.00446.x10.1111/j.1551-2916.2005.00446.x ↗
10. Effect of Sucrose on Fabrication of Ceramic Foams from Aqueous Slurries10.1111/j.1551-2916.2004.00001.x ↗
11. 10.1111/j.1151-2916.2001.tb00997.x10.1111/j.1151-2916.2001.tb00997.x ↗
12. 10.1016/S0955-2219(97)00101-510.1016/S0955-2219(97)00101-5 ↗
13. 10.1111/j.1151-2916.2003.tb03311.x10.1111/j.1151-2916.2003.tb03311.x ↗
14. 10.1126/science.112093710.1126/science.1120937 ↗
15. 10.1111/j.1151-2916.2001.tb00638.x10.1111/j.1151-2916.2001.tb00638.x ↗
16. Fabrication of Porous Ceramics with Unidirectionally Aligned Continuous Pores10.1111/j.1151-2916.2001.tb00849.x ↗
17. 10.1111/j.1551-2916.2005.00176.x10.1111/j.1551-2916.2005.00176.x ↗
18. 10.1111/j.1551-2916.2005.00785.x10.1111/j.1551-2916.2005.00785.x ↗
19. 10.1111/j.1551-2916.2006.01092.x10.1111/j.1551-2916.2006.01092.x ↗
20. 10.1111/j.1551-2916.2006.01222.x10.1111/j.1551-2916.2006.01222.x ↗
21. New Freeze Casting Technique for Ceramics with Sublimable Vehicle10.1111/j.1151-2916.2004.tb06331.x ↗
22. 10.1016/S0376-7388(00)00587-110.1016/S0376-7388(00)00587-1 ↗
23. 10.1023/A:101867421221310.1023/A:1018674212213 ↗
24. 10.1016/0022-0248(91)90915-R10.1016/0022-0248(91)90915-R ↗
25. 10.1016/S0025-5408(00)00285-310.1016/S0025-5408(00)00285-3 ↗
26. 10.1007/978-1-4899-3051-410.1007/978-1-4899-3051-4 ↗
27. 10.1002/(SICI)1097-0126(200004)49:4<323::AID-PI369>3.0.CO;2-710.1002/(SICI)1097-0126(200004)49:4<323::AID-PI369>3.0.CO;2-7 ↗
28. 10.1023/A:100890012747510.1023/A:1008900127475 ↗