Corrosion of Ceramics in Aqueous Hydrofluoric Acid
Source abstract
Abstract
A variety of commercially available ceramic‐based oxides, carbides, nitrides, and borides were evaluated for chemical attack in an azeotropic aqueous hydrofluoric acid (HF) test protocol at 90°C. Weight change measurements and microstructure analysis showed that HF corrosion in polycrystalline ceramics generally occurred at grain boundaries by the dissolution of grain boundary phases although the bulk single crystal may inherently resist attack. Virtually all commercially prepared polycrystalline oxide ceramics (i.e., Al 2 O 3 , TiO 2 , ZrO 2 ) and nonoxide ceramics (i.e., Si 3 N 4 , AlN, BN) were extensively corroded while polycrystalline pure carbides (i.e., SiC, TiC, B 4 C, WC) resisted corrosion. Equilibrium thermodynamic calculations show that these materials are soluble in HF; however, the kinetics of dissolution are slow enough in some cases to permit useful engineering lifetimes.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Nuclear materials and radiation effects · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (8)
Show source-provided references
1. 10.1111/j.1151-2916.1998.tb02343.x10.1111/j.1151-2916.1998.tb02343.x ↗
2. Philips D. S. · 1984 · 357
3. 10.1111/j.1151-2916.1998.tb02747.x10.1111/j.1151-2916.1998.tb02747.x ↗
4. NBS Tables of Chemical Thermodynamic Properties, Selected Values for Inorganic and C1 and C2 Organic Substances in SI Units
5. The Mechanisms of Chemical Reaction Between Silicate Glass and Attacking Agents: Part 1, Electrophilic and Nucleophilic Mechanisms of Attack
6. The Mechanisms of Chemical Reaction Between Silicate Glass and Attacking Agents: Part 2, Chemical Equilibrium at Glass‐Solution Interfaces
7. 10.1111/j.1151-2916.1987.tb05708.x10.1111/j.1151-2916.1987.tb05708.x ↗
8. 10.1111/j.1151-2916.1982.tb10471.x10.1111/j.1151-2916.1982.tb10471.x ↗