journal article·1995-01

Formation and Microstructure of Carbon‐Containing Oxide Scales by Oxidation of Single Crystals of Zirconium Carbide

Shiro Shimada, Masaru Nishisako, Michio Inagaki, Kazuhide Yamamoto

Publisher page

Abstract

The isothermal oxidation of ZrC single crystals with (100) orientation was carried out at temperatures of 500°, 550°, and 600°C at an oxygen pressure of 2.6 kPa for times up to 240 h. A polished cross section of the oxidized crystal was observed by backscattered electron imaging in a scanning electron microscope. Quantitative chemical analysis for Zr, O, and C and their elemental profiles by the linescan method in the ZrC and oxide scale were performed by wavelength dispersive X‐ray microanalysis. A thin foil of a crystal oxidized at 600°C was examined by transmission electron microscopy. It was found that the oxide scale was divided into two regions, zones 1 and 2, which contained 14 to 23 and 7 to 10 at. % carbon, respectively. Zone 1 exhibited an almost compact, pore‐free matrix of c ‐ZrO 2 . In zone 2, some growth and aggregation of the c ‐ZrO 2 occurred, producing 5‐ to 20‐nm‐sized particles between which carbon should have been present. The thickness of zone 1 increased parabolically up to 240 h at 500°C and probably in an early period at 550° and 600°C, reaching a constant (about 2 (μm), in contrast to the thickness of zone 2, which increased linearly with time.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Nuclear Materials and Properties · Advanced ceramic materials synthesis · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Electric Refractory Materials—Transition Metal Carbides, Nitrides, and Diborides” (in Jpn.)
2. 10.1111/j.1151-2916.1990.tb06678.x10.1111/j.1151-2916.1990.tb06678.x ↗
3. 10.1149/1.242626310.1149/1.2426263 ↗
4. The Oxidation Kinetics of Zirconium Carbide
5. Oxidation of Powdered Samples of ZrC between 450° and 700°C and under Oxygen Pressure between 10–3 and 100 torr
6. A Comparative Study of the Oxidation Resistance of Zirconium Carbide and Zirconium Oxycarbide
7. 10.1007/BF0110721410.1007/BF01107214 ↗
8. 10.1111/j.1151-2916.1992.tb05487.x10.1111/j.1151-2916.1992.tb05487.x ↗
9. 10.1016/0167-2738(93)90122-J10.1016/0167-2738(93)90122-J ↗
10. 10.1111/j.1151-2916.1993.tb05332.x10.1111/j.1151-2916.1993.tb05332.x ↗
11. 10.1016/0022-0248(81)90297-910.1016/0022-0248(81)90297-9 ↗
12. Powder Diffraction File Card No. 27–997. Joint Committee on Powder Diffraction Standards Swarthmore PA .
13. Otsuka N. · 1990 · 84
14. 10.1016/0267-3762(86)90022-610.1016/0267-3762(86)90022-6 ↗
15. 1971