Spark Plasma‐Sintered WC–ZrO 2 –Co Nanocomposites with High Fracture Toughness and Strength
Source abstract
Abstract
In this paper, we demonstrate for the first time how partial/full replacement of Co (metallic phase) with ZrO 2 (ceramic phase) in WC–Co system, along with spark plasma sintering, can lead to the development of high‐performance WC‐based ceramic nanocomposites. Convergent beam electron diffraction analysis, in combination with transmission electron microscopy, reveal the dispersion of nanosized t ‐ZrO 2 particles, as well as the Co phase, in the dense WC–ZrO 2 –Co nanocomposites. In order to obtain reliable measures of strength and fracture toughness properties, four‐point bending configuration, and single‐edge V‐notch beam techniques, respectively, were used. Among the investigated nanocomposites, WC–6 wt% ZrO 2 inter/intragranular nanocomposite exhibited the optimum combination of mechanical properties such as high hardness (∼20 GPa), flexural strength (∼1.3 GPa), and fracture toughness (∼10 MPa·m 1/2 ). The flexural strength was superior by ∼18% to that measured with the reference WC–6 wt % Co cermet, while the fracture toughness was only modestly lower by ∼16%. Theoretical estimates, based on residual stress‐induced toughening, were found to be insignificant to explain the high toughness of the nanocomposites. The ability to maintain considerably high fracture toughness has been attributed partly to the transformation toughening by the t ‐ZrO 2 phase. Additional contributions from other toughening mechanisms originate from the change in fracture mode from intergranular (WC–6 wt% Co cermet) to transgranular in the presence of nanosized ZrO 2 particles, crack bridging, and crack deflection by the ZrO 2 particles. Based on finer scale microstructural analysis as well as mechanical property measurement, an effort has been made to establish the structure–property relationship in the investigated ceramic nanocomposite system.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Orthopaedic implants and arthroplasty
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (55)
Show source-provided references
1. Sarin V. K. · 1981 · 253
2. The Dawn of the Hardmetal Age
3. 10.1016/S0965-9773(98)00123-810.1016/S0965-9773(98)00123-8 ↗
4. 10.1016/S0924-0136(96)02748-310.1016/S0924-0136(96)02748-3 ↗
5. Inhibition of Grain Growth on Submicron Cemented Carbides
6. Lenel F. V. · 1980
7. Nanocrystalline Materials
8. 10.1016/S0921-5093(02)00605-610.1016/S0921-5093(02)00605-6 ↗
9. 10.1016/S1359-6462(01)00835-110.1016/S1359-6462(01)00835-1 ↗
10. 10.1016/j.msea.2004.09.04310.1016/j.msea.2004.09.043 ↗
11. 10.1016/j.ijrmhm.2005.11.00410.1016/j.ijrmhm.2005.11.004 ↗
12. 10.1016/j.ijrmhm.2006.09.00110.1016/j.ijrmhm.2006.09.001 ↗
13. 10.1016/j.ijrmhm.2006.03.00810.1016/j.ijrmhm.2006.03.008 ↗
14. Suzuki H. · 1986
15. S.SutthiruangwongaandG.Mori “Corrosion Properties of Co‐Based Cemented Carbides in Acidic Solutions ” Int. J. Refract. Met. Hard Mater. 21 135–45(2003).10.1016/S0263-4368(03)00027-1 ↗
16. Corrosion Resistance of Cemented Carbide
17. 10.1016/0263-4368(95)92676-B10.1016/0263-4368(95)92676-B ↗
18. 10.1016/j.ijrmhm.2004.08.00310.1016/j.ijrmhm.2004.08.003 ↗
19. 10.1016/j.ijrmhm.2005.04.00410.1016/j.ijrmhm.2005.04.004 ↗
20. 10.1016/S0921-5093(03)00151-510.1016/S0921-5093(03)00151-5 ↗
21. 10.1557/jmr.2007.018910.1557/jmr.2007.0189 ↗
22. 10.1111/j.1551-2916.2005.00129.x10.1111/j.1551-2916.2005.00129.x ↗
23. 10.1111/j.1151-2916.2000.tb01221.x10.1111/j.1151-2916.2000.tb01221.x ↗
24. 10.1038/258703a010.1038/258703a0 ↗
25. 10.1179/174328005X4111310.1179/174328005X41113 ↗
26. Pressureless Sintering of ZrO2–ZrB2 Composites
27. 10.1111/j.1551-2916.2006.01482.x10.1111/j.1551-2916.2006.01482.x ↗
28. 10.1007/BF0072807810.1007/BF00728078 ↗
29. 10.1007/BF0072470610.1007/BF00724706 ↗
30. 10.1111/j.1151-2916.1995.tb08891.x10.1111/j.1151-2916.1995.tb08891.x ↗
31. 10.1016/j.jeurceramsoc.2009.07.01310.1016/j.jeurceramsoc.2009.07.013 ↗
32. 10.1016/S0921-5093(97)00509-110.1016/S0921-5093(97)00509-1 ↗
33. 10.1016/j.ijrmhm.2005.11.01410.1016/j.ijrmhm.2005.11.014 ↗
34. The Influence of Binder Constitution on the Shape of WC Grains
35. 10.1179/09506607979013636310.1179/095066079790136363 ↗
36. ASM International. · 1989
37. Scussel H. J. · 1992
38. 10.1111/j.1151-2916.1990.tb05209.x10.1111/j.1151-2916.1990.tb05209.x ↗
39. Consolidation‐Microstructure‐Property Relationships in Bulk Nanoceramics and Ceramic Nanocomposites
40. A.Mukhopadhyay “Fabrication and Properties of Oxide Nanocomposites Containing Uniformly Dispersed Second Phases”; Ph.D. Thesis Oxford University Oxford U.K. 2009.
41. 10.1111/j.1551-2916.2007.01911.x10.1111/j.1551-2916.2007.01911.x ↗
42. Strengthening and Toughening Mechanisms of Ceramic Nanocomposites10.1111/j.1151-2916.1998.tb02503.x ↗
43. 10.1016/0001-6160(86)90052-010.1016/0001-6160(86)90052-0 ↗
44. 10.1007/BF0238572110.1007/BF02385721 ↗
45. Mechanical Properties of Hot‐Pressed TiB2–ZrO2 Composites
46. 10.1016/j.jeurceramsoc.2009.03.02310.1016/j.jeurceramsoc.2009.03.023 ↗
47. 10.1111/j.1151-2916.1993.tb05304.x10.1111/j.1151-2916.1993.tb05304.x ↗
48. Effect of Yttria Doping on the Microstructure and Mechanical Properties of Al2O3–FeAl2O4 Nanocomposites Developed Via Solid State Precipitation
49. 10.2109/jcersj.99.97410.2109/jcersj.99.974 ↗
50. 10.1111/j.1151-2916.1993.tb03814.x10.1111/j.1151-2916.1993.tb03814.x ↗
51. 10.1016/S0955-2219(98)00232-510.1016/S0955-2219(98)00232-5 ↗
52. 10.1111/j.1151-2916.2003.tb03306.x10.1111/j.1151-2916.2003.tb03306.x ↗
53. 10.1016/S0965-9773(98)00160-310.1016/S0965-9773(98)00160-3 ↗
54. 10.1016/0001-6160(83)90046-910.1016/0001-6160(83)90046-9 ↗
55. ZrO2–WC Nanocomposites with Superior Properties