Domain Wall Motion in A and B Site Donor‐Doped Pb ( Zr 0.52 Ti 0.48 ) O 3 Films
Source abstract
Abstract
Donor‐doped PbZr 0.52 Ti 0.48 O 3 ( PZT ) films were utilized to study the effect of dopants on the mobility of ferroelectric domain walls. For chemical solution deposited PZT films 2 μm in thickness, doped with 1%–4% Nb or La , the low field dielectric permittivity remained between 1100 and 1300. With increasing Nb concentration, both the reversible and irreversible Rayleigh constants increased from ɛ init and α ′ of 1150 and 39 cm/kV, respectively, for undoped PZT films to 1360 and 43 cm/kV for films doped with 2 mol% Nb . La doping increased the irreversible Rayleigh constant but did not strongly affect the reversible Rayleigh parameter. These observations are consistent with softening of the dielectric and electromechanical response with donor doping.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Dielectric properties of ceramics · Multiferroics and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Materials Research Institute The Pennsylvania State University University Park Pennsylvania 16802
Electronic Materials Research Laboratory Key Laboratory of the Ministry of Education Xi'an Jiaotong University Xi'an China 710049
References (54)
Show source-provided references
1. Jaffe B. · 1971
2. 10.1109/ISAF.2008.469382210.1109/ISAF.2008.4693822 ↗
3. 10.1111/j.1151-2916.1970.tb12105.x-i110.1111/j.1151-2916.1970.tb12105.x-i1 ↗
4. 10.1557/JMR.1997.003010.1557/JMR.1997.0030 ↗
5. L.Jin “Broadband Dielectric Response in Hard and Soft PZT: Understanding Softening and Hardening Mechanisms”; Ph.D. Thesis Swiss Federal Institute of Technology‐EPFL Lausanne Switzerland 2011.
6. 10.1007/s10832-007-9068-810.1007/s10832-007-9068-8 ↗
7. 10.1111/j.1551-2916.2009.03514.x10.1111/j.1551-2916.2009.03514.x ↗
8. 10.1063/1.173539710.1063/1.1735397 ↗
9. 10.1007/s10832-005-2403-z10.1007/s10832-005-2403-z ↗
10. 10.1016/j.physc.2008.05.07310.1016/j.physc.2008.05.073 ↗
11. 10.1111/j.1551-2916.2009.03528.x10.1111/j.1551-2916.2009.03528.x ↗
12. 10.1063/1.328495410.1063/1.3284954 ↗
13. 10.1016/0022-3697(86)90042-910.1016/0022-3697(86)90042-9 ↗
14. 10.1080/1040843070170734710.1080/10408430701707347 ↗
15. 10.1557/mrs2009.17710.1557/mrs2009.177 ↗
16. 10.1023/B:JECR.0000033998.72845.5110.1023/B:JECR.0000033998.72845.51 ↗
17. 10.1016/j.jeurceramsoc.2008.07.06210.1016/j.jeurceramsoc.2008.07.062 ↗
18. 10.1016/j.matchemphys.2004.06.03510.1016/j.matchemphys.2004.06.035 ↗
19. 10.1016/S0040-6090(02)01045-310.1016/S0040-6090(02)01045-3 ↗
20. 10.1016/j.mseb.2003.10.06510.1016/j.mseb.2003.10.065 ↗
21. 10.1063/1.149896610.1063/1.1498966 ↗
22. 10.1103/PhysRevLett.83.123110.1103/PhysRevLett.83.1231 ↗
23. 10.1063/1.163596810.1063/1.1635968 ↗
24. 10.1016/S1369-8001(02)00092-610.1016/S1369-8001(02)00092-6 ↗
25. 10.1111/j.1151-2916.1991.tb04130.x10.1111/j.1151-2916.1991.tb04130.x ↗
26. 10.1063/1.297516410.1063/1.2975164 ↗
27. 10.1016/j.tsf.2009.04.04510.1016/j.tsf.2009.04.045 ↗
28. 10.1007/BF0268420510.1007/BF02684205 ↗
29. 10.1023/A:102280650619310.1023/A:1022806506193 ↗
30. 10.1016/j.apsusc.2004.06.10310.1016/j.apsusc.2004.06.103 ↗
31. 10.1063/1.131381410.1063/1.1313814 ↗
32. 10.1063/1.36598110.1063/1.365981 ↗
33. 10.1007/s10832-007-9001-110.1007/s10832-007-9001-1 ↗
34. 10.1007/BF0159835510.1007/BF01598355 ↗
35. 10.1063/1.135916610.1063/1.1359166 ↗
36. 10.1063/1.155765610.1063/1.1557656 ↗
37. 10.1109/TUFFC.2010.161010.1109/TUFFC.2010.1610 ↗
38. P.Bintachitt “Local Origin of Macroscopic Properties and Patterning in PbZr1‐xTixO3Films”; Ph.D. Thesis The Pennsylvania State University University Park PA 2009.
39. 10.1063/1.162393710.1063/1.1623937 ↗
40. 10.1063/1.163653010.1063/1.1636530 ↗
41. 10.1111/j.1151-2916.1994.tb05398.x10.1111/j.1151-2916.1994.tb05398.x ↗
42. 10.1016/S0924-4247(98)00161-710.1016/S0924-4247(98)00161-7 ↗
43. 10.1063/1.355229810.1063/1.3552298 ↗
44. 10.1063/1.319431110.1063/1.3194311 ↗
45. 10.1088/0022-3727/41/22/22530210.1088/0022-3727/41/22/225302 ↗
46. Piezoelectric Properties of Sputtered PZT Films: Influence of Structure, Micro Structure, Film Thickness (Zr,Ti) Ratio and Nb Substitution
47. 10.1016/j.physb.2006.11.02610.1016/j.physb.2006.11.026 ↗
48. 10.1023/A:101795911140210.1023/A:1017959111402 ↗
49. 10.1063/1.299944110.1063/1.2999441 ↗
50. 10.1016/j.jeurceramsoc.2005.03.08610.1016/j.jeurceramsoc.2005.03.086 ↗
51. 10.1063/1.328494510.1063/1.3284945 ↗
52. 10.1103/PhysRevLett.108.15760410.1103/PhysRevLett.108.157604 ↗
53. 10.1063/1.37017610.1063/1.370176 ↗
54. 10.1109/TMAG.2003.81646710.1109/TMAG.2003.816467 ↗