Synthesis of Li 4 SiO 4 by a Modified Combustion Method

Daniel Cruz, Silvia Bulbulian

Publisher page

Abstract

We report for the first time the synthesis of Li 4 SiO 4 by the modified combustion method, a rapid chemical process that takes 5 min for completion. This method uses nonoxidizer compounds instead of nitrate mixtures, which are not always commercially available. The effects of the following parameters on the production of Li 4 SiO 4 were studied: (1) different lithium hydroxide:silicic acid:urea (LiOH:H 2 SiO 3 :CH 4 N 2 O) molar ratios; (2) the presence of air flow in the furnace chamber; and (3) the furnace heating temperature. It was found that LiOH:H 2 SiO 3 :CH 4 N 2 O molar ratios 6:1:3 heated at 1100°C in the presence of additional air in the muffle chamber formed the best precursors to produce Li 4 SiO 4 .
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Zeolite Catalysis and Synthesis · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. 10.1016/S0022-3115(02)01119-410.1016/S0022-3115(02)01119-4 ↗
2. 10.1016/0022-3115(92)90725-Z10.1016/0022-3115(92)90725-Z ↗
3. 10.1016/S0022-3115(98)00449-810.1016/S0022-3115(98)00449-8 ↗
4. 10.1016/S0272-8842(02)00190-610.1016/S0272-8842(02)00190-6 ↗
5. 10.1016/S0022-3115(01)00710-310.1016/S0022-3115(01)00710-3 ↗
6. 10.1016/j.jnucmat.2003.08.03610.1016/j.jnucmat.2003.08.036 ↗
7. 10.1023/A:101242680885510.1023/A:1012426808855 ↗
8. 10.1016/S0022-3115(02)01628-810.1016/S0022-3115(02)01628-8 ↗
9. 10.1016/0022-3115(91)90520-H10.1016/0022-3115(91)90520-H ↗
10. Nakamoto K. · 1986 · 71
11. Rao C. N. R. · 1963 · 287
12. Pouchert C. J. · 1985
13. 10.1016/S0022-3115(97)00313-910.1016/S0022-3115(97)00313-9 ↗
14. Klug H. P. · 1974 · 709