The role of moisture in affecting both intrinsic and extrinsic aspects of the fracture and fatigue‐crack growth resistance of a polycrystalline alumina (99.5% pure, 25 μm grain size) has been examined in both moist and dry environments at ambient temperature. The intrinsic (crack‐tip) toughness, deduced from measured crack‐opening profiles, is found to be less than for a single crystal and is 30% lower (∼0.6 MPa·m 1/2 ) in moist air versus in dry N 2 , implying that the grain‐boundary theoretical strength is higher in a dry environment. Despite this, in dry atmospheres, the R ‐curves (which derive from crack deflection and grain bridging) initially rose more steeply and nominal fatigue‐crack growth thresholds for short crack sizes (20–60 μm) were more than 1.3 MPa·m 1/2 higher. Owing to this quicker crack bridging development, strengths for natural flaws could be more than doubled in dry atmospheres, a difference that well exceeds the effect solely due to the intrinsic toughness change. After ∼2 mm of crack growth, however, the R ‐curve and steady‐state fatigue behavior appeared similar in both environments, although altering the atmosphere for such fatigue cracks in situ induced large, abrupt changes in transient growth rates. The environment influences the nature of the bridging zones, with uncracked‐ligament bridges playing a larger role in dry atmospheres, while frictional bridges are predominant in moist air. Evidently, to achieve optimal toughness in bridging ceramics, the window for the requisite grain‐boundary strength may be small; whereas weak boundaries are required to induce the necessary intergranular fracture, if too weak, shallower R ‐curves, less strengthening, and poorer fatigue resistance all follow.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Numerical methods in engineering · Fatigue and fracture mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (80)

Show source-provided references
1. Moisture Assisted Crack Growth in Ceramics10.1007/BF00188945 ↗
2. 10.1007/BF0055019610.1007/BF00550196 ↗
3. 10.1080/1478643730822098310.1080/14786437308220983 ↗
4. 10.1007/978-1-4615-7014-1_1410.1007/978-1-4615-7014-1_14 ↗
5. 10.1557/JMR.2000.002410.1557/JMR.2000.0024 ↗
6. 10.1016/S0142-9612(01)00206-X10.1016/S0142-9612(01)00206-X ↗
7. 10.1007/BF0054450210.1007/BF00544502 ↗
8. Crack‐Interface Grain Bridging as a Fracture Resistance Mechanism in Ceramics
9. 10.1111/j.1151-2916.1987.tb04983.x10.1111/j.1151-2916.1987.tb04983.x ↗
10. 10.1111/j.1151-2916.1982.tb10426.x10.1111/j.1151-2916.1982.tb10426.x ↗
11. 10.1016/0001-6160(86)90052-010.1016/0001-6160(86)90052-0 ↗
12. Mechanisms of Fatigue Crack Propagation in Metals, Ceramics and Composites
13. 10.1111/j.1151-2916.1967.tb15145.x10.1111/j.1151-2916.1967.tb15145.x ↗
14. 10.1111/j.1151-2916.1983.tb15715.x10.1111/j.1151-2916.1983.tb15715.x ↗
15. 10.1111/j.1151-2916.1990.tb07607.x10.1111/j.1151-2916.1990.tb07607.x ↗
16. 10.1016/0001-6160(89)90299-X10.1016/0001-6160(89)90299-X ↗
17. Indentation Toughness of Polycrystalline Alumina
18. 10.1557/mrs2000.6810.1557/mrs2000.68 ↗
19. 10.1111/j.1151-2916.1989.tb06171.x10.1111/j.1151-2916.1989.tb06171.x ↗
20. 10.1111/j.1151-2916.1996.tb08120.x10.1111/j.1151-2916.1996.tb08120.x ↗
21. 10.1016/0025-5416(88)90481-810.1016/0025-5416(88)90481-8 ↗
22. 10.1023/A:101865591705110.1023/A:1018655917051 ↗
23. Cyclic Fatigue from Frictional Degradation at Bridging Grains in Alumina10.1111/j.1151-2916.1991.tb04109.x ↗
24. Cyclic Fatigue in Monolithic Alumina
25. 10.1111/j.1551-2916.2004.00093.x10.1111/j.1551-2916.2004.00093.x ↗
26. “ASTM E561‐98 ” pp. 534–46 inAnnual Book of ASTM Standards Vol. 03.01: Metals‐ Mechanical Testing; Elevated and Low‐temperature Tests; Metallography. ASTM West Conshohocken PA USA 2002.
27. A Simple and Sensitive Method of Monitoring Crack and Load in Compact Fracture Mechanics Specimens Using Strain Gages10.1520/JTE11216J ↗
28. “ASTM E647‐00 ” pp. 595–635 inAnnual Book of ASTM Standards Vol. 03.01: Metals‐ Mechanical Testing; Elevated and Low‐temperature Tests; Metallography. ASTM West Conshohocken PA USA 2002.
29. 10.1016/0013-7944(87)90159-710.1016/0013-7944(87)90159-7 ↗
30. 10.1023/A:102262621433310.1023/A:1022626214333 ↗
31. 10.1111/j.1151-2916.2003.tb03593.x10.1111/j.1151-2916.2003.tb03593.x ↗
32. Fett T. · 1997
33. 10.1016/0956-7151(93)90145-I10.1016/0956-7151(93)90145-I ↗
34. 10.1016/S1359-6454(98)00408-X10.1016/S1359-6454(98)00408-X ↗
35. Iwasa M. · 1984 · 767
36. 10.1111/j.1151-2916.1976.tb09390.x10.1111/j.1151-2916.1976.tb09390.x ↗
37. 10.1111/j.1151-2916.1969.tb09199.x10.1111/j.1151-2916.1969.tb09199.x ↗
38. 10.1111/j.1151-2916.1961.tb13754.x10.1111/j.1151-2916.1961.tb13754.x ↗
39. 10.1111/j.1151-2916.1969.tb13350.x10.1111/j.1151-2916.1969.tb13350.x ↗
40. 10.1111/j.1151-2916.1965.tb14677.x10.1111/j.1151-2916.1965.tb14677.x ↗
41. 10.1007/BF0058548410.1007/BF00585484 ↗
42. 10.1111/j.1151-2916.1970.tb15962.x10.1111/j.1151-2916.1970.tb15962.x ↗
43. 10.1007/BF0075219110.1007/BF00752191 ↗
44. Crack Deflection at an Interface Between Dissimilar Elastic Materials10.1016/0020-7683(89)90021-8 ↗
45. Measurement of Crack Tip Toughness in Alumina as a Function of Grain Size10.1111/j.1151-2916.1997.tb02848.x ↗
46. 10.1111/j.1151-2916.1990.tb06454.x10.1111/j.1151-2916.1990.tb06454.x ↗
47. 10.1111/j.1151-2916.1996.tb08571.x10.1111/j.1151-2916.1996.tb08571.x ↗
48. 10.1016/S1359-6454(98)00317-610.1016/S1359-6454(98)00317-6 ↗
49. 10.1016/S0955-2219(00)00065-010.1016/S0955-2219(00)00065-0 ↗
50. 10.1111/j.1151-2916.2002.tb00491.x10.1111/j.1151-2916.2002.tb00491.x ↗
51. 10.1111/j.1151-2916.1988.tb05759.x10.1111/j.1151-2916.1988.tb05759.x ↗
52. 10.1007/978-94-011-2882-7_8110.1007/978-94-011-2882-7_81 ↗
53. Relations of Strength, Fracture Toughness and Grain Boundary Strength in Rare Earth‐Doped Si3N4–Ceramics
54. Crack Closure Forces in Ceramics
55. In situ Measurements of Frictional Bridging Stresses in Alumina Using Fluorescence Spectroscopy10.1111/j.1151-2916.1998.tb02312.x ↗
56. In situ Measurement of Bridging Stresses in Toughened Silicon Nitride Using Raman Microprobe Spectroscopy10.1111/j.1151-2916.1999.tb01903.x ↗
57. 10.1016/S0013-7944(00)00090-410.1016/S0013-7944(00)00090-4 ↗
58. Andersson P. · 1992 · 1241
59. Toughening of an Alumina–Mullite Composite by Unbroken Bridging Elements10.1111/j.1151-2916.2000.tb01282.x ↗
60. McClintock F. A. · 1997 · 81
61. 10.1016/S0921-5093(03)00534-310.1016/S0921-5093(03)00534-3 ↗
62. 10.1016/S0167-6636(02)00284-310.1016/S0167-6636(02)00284-3 ↗
63. Statistical Fracture Modeling
64. Fracture and Subcritical Crack‐Growth Behavior of Y–Si–Al–O–N Glasses and Si3N4 Ceramics10.1111/j.1151-2916.2000.tb01237.x ↗
65. 10.1111/j.1151-2916.1994.tb05387.x10.1111/j.1151-2916.1994.tb05387.x ↗
66. 10.1007/BF0054383410.1007/BF00543834 ↗
67. 10.1111/j.1151-2916.1995.tb08504.x10.1111/j.1151-2916.1995.tb08504.x ↗
68. Numerical Evaluation of Toughening by Crack‐Face Grain Interlocking in Self‐Reinforced Ceramics10.1111/j.1151-2916.2000.tb01280.x ↗
69. 10.4028/www.scientific.net/KEM.161-163.61510.4028/www.scientific.net/KEM.161-163.615 ↗
70. Strength‐Size Relations in Ceramic Materials
71. 10.1016/S0955-2219(99)00205-810.1016/S0955-2219(99)00205-8 ↗
72. 10.1016/S0167-577X(02)01370-810.1016/S0167-577X(02)01370-8 ↗
73. Relative Humidity and Modulus of Rupture
74. Pletka B. · 1978 · 745
75. 10.1016/j.actamat.2005.02.01810.1016/j.actamat.2005.02.018 ↗
76. 10.1111/j.1551-2916.2005.00421.x10.1111/j.1551-2916.2005.00421.x ↗
77. 10.1016/j.actamat.2003.08.03810.1016/j.actamat.2003.08.038 ↗
78. Crack‐Growth Resistance‐Curve Behavior in Silicon Carbide: Small Versus Long Cracks10.1111/j.1151-2916.1997.tb03115.x ↗
79. 10.1016/S0955-2219(99)00106-510.1016/S0955-2219(99)00106-5 ↗
80. 10.1080/0950083930824385810.1080/09500839308243858 ↗