Spark Plasma Sintering of Nano‐Sized TiN Prepared from TiO 2 by Controlled Hydrolysis of TiCl 4 and Ti(O‐i‐C 3 H 7 ) 4 Solution
Source abstract
Abstract
Nano‐sized TiO 2 powders were prepared by controlled hydrolysis of TiCl 4 and Ti(O‐i‐C 3 H 7 ) 4 solutions and nitrided in flowing NH 3 gas at 700°–1000°C to form TiN. Nano‐sized TiN was densified by spark plasma sintering at 1300°–1600°C to produce TiN ceramics with a relative density of 98% at 1600°C. The microstructure of the etched ceramic surface was observed by SEM, which revealed the formation of uniformly sized 1–2 μm grains in the TiCl 4 ‐derived product and 10–20 μm in the Ti(O‐i‐C 3 H 7 ) 4 ‐derived TiN. The electric resisitivity and Vickers micro‐hardness of the TiN ceramics was also measured.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. 10.1007/978-94-009-0071-410.1007/978-94-009-0071-4 ↗
2. 10.1116/1.57371410.1116/1.573714 ↗
3. 10.1149/1.204861510.1149/1.2048615 ↗
4. Fabrication and Characterization of Titanium Nitride by High Pressure Hot Press
5. 10.2109/jcersj.99.28610.2109/jcersj.99.286 ↗
6. 10.1016/S0921-5093(01)00936-410.1016/S0921-5093(01)00936-4 ↗
7. 10.1007/BF0056928210.1007/BF00569282 ↗
8. 10.1016/S0167-2738(97)84027-110.1016/S0167-2738(97)84027-1 ↗
9. 10.1016/S0921-5093(00)00676-610.1016/S0921-5093(00)00676-6 ↗
10. 10.1016/S0965-9773(97)00020-210.1016/S0965-9773(97)00020-2 ↗
11. 10.1111/j.1151-2916.2000.tb01369.x10.1111/j.1151-2916.2000.tb01369.x ↗
12. 10.1016/S0272-8842(99)00057-710.1016/S0272-8842(99)00057-7 ↗
13. 10.1039/b102794h10.1039/b102794h ↗
14. 10.1039/b107058b10.1039/b107058b ↗
15. JPCDS Cards No. 38 – 1420.
16. Toth L. E. · 1971 · 7