journal article·2011-06

The Reactivity of Ti 2 AlC and Ti 3 SiC 2 with SiC Fibers and Powders up to Temperatures of 1550°C

Charles B. Spencer, Jose M. Córdoba, Nicholas H. Obando, Miladin Radovic, Magnus Odén, Lars Hultman, Michel W. Barsoum

Publisher page

Abstract

The reactivities of commercially available Ti 2 AlC or Ti 3 SiC 2 powders with uncoated SiC fibers or SiC powders were evaluated in this paper. When Ti 2 AlC–SiC samples were hot pressed or hot isostatically pressed at temperatures up to 1500°C, fully dense composites were obtained. The latter were characterized by X‐ray diffraction and electron‐dispersive spectroscopy in a scanning and transmission electron microscope. Differential thermal analysis up to 1550°C was also carried out. In all cases, SiC reacted with the Ti 2 AlC powder resulting in the formation of Ti 3 (Al 1− x Si x )C 2 TiC and Al 1+ x Ti 1− x , where x ranges from 0 to 1. In the limit x =1, pure Al forms. Conversely, Ti 3 SiC 2 samples, reinforced with uncoated SiC fibers or powders, can be hot pressed in vacuum at temperatures as high as 1500°C to produce fully dense composites with no apparent reaction between the matrix and fibers. Based on these results, Ti 3 SiC 2 can, but Ti 2 AlC cannot, be reinforced with SiC. Such reinforcements will be needed if the MAX phases are to be used as structural materials at very high temperatures.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. The M N+1AX N Phases
2. 10.1016/0022-5088(64)90055-410.1016/0022-5088(64)90055-4 ↗
3. 10.1016/0079-6786(71)90016-110.1016/0079-6786(71)90016-1 ↗
4. 10.1111/j.1551-2916.2006.01303.x10.1111/j.1551-2916.2006.01303.x ↗
5. 10.1007/BF0264755910.1007/BF02647559 ↗
6. Die Kristallstruktur von Ti3GeC210.1007/BF00902438 ↗
7. 10.1557/JMR.2005.010510.1557/JMR.2005.0105 ↗
8. 10.1103/PhysRevB.70.16540110.1103/PhysRevB.70.165401 ↗
9. 10.1016/S0025-5408(00)00383-410.1016/S0025-5408(00)00383-4 ↗
10. Barsoum M. W. · 2001
11. 10.1016/B0-08-043152-6/01931-810.1016/B0-08-043152-6/01931-8 ↗
12. 10.1103/PhysRevB.71.13410110.1103/PhysRevB.71.134101 ↗
13. Barsoum M. W. · 2010
14. Incipient and Regular Kink Bands in Dense and 10 Vol.% Porous Ti2AlC
15. 10.1038/nmat81410.1038/nmat814 ↗
16. 10.1016/S1359-6454(01)00424-410.1016/S1359-6454(01)00424-4 ↗
17. 10.1016/S1359-6462(96)00418-610.1016/S1359-6462(96)00418-6 ↗
18. 10.1007/s11661-006-0243-310.1007/s11661-006-0243-3 ↗
19. 10.1016/S1359-6462(99)00427-310.1016/S1359-6462(99)00427-3 ↗
20. 10.1016/j.matlet.2007.09.00510.1016/j.matlet.2007.09.005 ↗
21. 10.1149/1.155603510.1149/1.1556035 ↗
22. 10.1023/A:101536311916410.1023/A:1015363119164 ↗
23. 10.1016/S0921-5093(03)00500-810.1016/S0921-5093(03)00500-8 ↗
24. 10.1016/j.ceramint.2003.12.04610.1016/j.ceramint.2003.12.046 ↗
25. 10.1007/s11085-007-9063-010.1007/s11085-007-9063-0 ↗
26. Oxidation of Ti n+1AlX n Where n=1–3 and X is C, N, Part II
27. Oxidation of Ti n+1AlX n Where n=1–3 and X is C, N, Part I
28. 10.1023/A:102309202769710.1023/A:1023092027697 ↗
29. 10.1016/S1359-6454(01)00243-910.1016/S1359-6454(01)00243-9 ↗
30. 10.1016/S0925-8388(03)00435-310.1016/S0925-8388(03)00435-3 ↗
31. 10.1016/j.actamat.2005.05.03710.1016/j.actamat.2005.05.037 ↗
32. 10.1016/j.jallcom.2009.08.07310.1016/j.jallcom.2009.08.073 ↗
33. 10.1016/0955-2219(91)90067-A10.1016/0955-2219(91)90067-A ↗
34. 10.1016/S0925-8388(02)00985-410.1016/S0925-8388(02)00985-4 ↗
35. 10.1016/j.scriptamat.2006.09.02910.1016/j.scriptamat.2006.09.029 ↗
36. 10.1016/j.compscitech.2007.06.00610.1016/j.compscitech.2007.06.006 ↗
37. Current Status in Layered Ternary Carbide Ti3SiC2, a Review
38. 10.1149/1.139257310.1149/1.1392573 ↗
39. Processing and Mechanical Properties of Ti3SiC2
40. Cottrell A. · 1995