Ultra‐Fast Fabrication of <110>‐Oriented β‐SiC Wafers by Halide CVD
Source abstract
Abstract
Φ80 mm‐diameter, highly <110>‐oriented β‐SiC wafers were ultra‐fast fabricated via halide chemical vapor deposition ( CVD ) using tetrachlorosilane (SiCl 4 ) and methane ( CH 4 ) as precursors. The effects of deposition temperature ( T dep ) and total pressure ( P tot ) on the orientations, microstructures, and deposition rate ( R dep ) were investigated. R dep dramatically increased with increasing T dep where maximum R dep was 930 μm/h at T dep = 1823 K and P tot = 4 kPa, leading to a maximum of 1.9 mm in thickness in 2 h deposition. The <110>‐oriented β‐SiC was obtained at T dep > 1773 K and P tot = 1–4 kPa. Growth mechanism of <110>‐oriented β‐SiC has also been discussed under consideration of crystallographic planes, surface energy, and surface morphology.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Silicon Carbide Semiconductor Technologies · Semiconductor materials and devices · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
State Key Laboratory of Advanced Technology for Materials Synthesis and Processing Wuhan University of Technology 122 Luoshi Road Wuhan 430070 China
Institute for Materials Research Tohoku University 2‐1‐1 Katahira, Aoba‐ku Sendai 980‐8577 Japan
R&D, Ibiden co., Ltd. 1‐1, Kitagata, Ibigawa‐cho, Ibi‐gun Gifu 501‐0695 Japan
Funding
National Natural Science Foundation of China · Natural Science Foundation of Hubei Province
References (35)
Show source-provided references
1. 10.1557/JMR.1993.261710.1557/JMR.1993.2617 ↗
2. 10.1016/j.jcrysgro.2004.06.00510.1016/j.jcrysgro.2004.06.005 ↗
3. 10.1103/PhysRevLett.77.201310.1103/PhysRevLett.77.2013 ↗
4. 10.1016/j.tsf.2009.10.08010.1016/j.tsf.2009.10.080 ↗
5. 10.1016/j.diamond.2009.09.01210.1016/j.diamond.2009.09.012 ↗
6. 10.1103/PhysRevLett.80.75810.1103/PhysRevLett.80.758 ↗
7. 10.1063/1.171927010.1063/1.1719270 ↗
8. 10.1111/j.1551-2916.2012.05354.x10.1111/j.1551-2916.2012.05354.x ↗
9. M.Nakao H.Iikawa K.Izumi T.Yokoyama andS.Kobayashi “Challenge to 200 mm 3C‐SiC Wafers Using SOI ”485 205–8(2005).10.4028/www.scientific.net/MSF.483-485.205 ↗
10. 10.1016/0039-6028(94)91529-610.1016/0039-6028(94)91529-6 ↗
11. 10.1021/jp209072n10.1021/jp209072n ↗
12. 10.1063/1.216987510.1063/1.2169875 ↗
13. 10.1149/1.210035910.1149/1.2100359 ↗
14. 10.1016/0040-6090(96)80023-X10.1016/0040-6090(96)80023-X ↗
15. 10.1063/1.213589610.1063/1.2135896 ↗
16. 10.1002/1521-3862(20020503)8:3<99::AID-CVDE99>3.0.CO;2-C10.1002/1521-3862(20020503)8:3<99::AID-CVDE99>3.0.CO;2-C ↗
17. 10.1016/0040-6090(94)06237-F10.1016/0040-6090(94)06237-F ↗
18. F.Loumagne F.Langlais andR.Naslain “Experimental Kinetic Study of the Chemical Vapour Deposition of SiC‐Based Ceramics from CH3SiCI3/H2Gas Precursor ”155 198–204(1995).10.1016/0022-0248(95)00180-8 ↗
19. 10.1016/0022-0248(95)00181-610.1016/0022-0248(95)00181-6 ↗
20. 10.1111/jace.1270610.1111/jace.12706 ↗
21. 10.1063/1.137098410.1063/1.1370984 ↗
22. Chemical Vapor Deposition of Graphene on a ‘Peeled‐Off’ Epitaxial Cu(111) Foil: A Simple Approach to Improved Properties
23. Evolutionary Selection, a Principle Governing Growth Orientation in Vapour‐Deposited Layers
24. 10.1149/1.139337410.1149/1.1393374 ↗
25. 10.1103/PhysRevB.87.23532110.1103/PhysRevB.87.235321 ↗
26. 10.1103/PhysRevB.42.904010.1103/PhysRevB.42.9040 ↗
27. 10.1103/PhysRevB.52.1515010.1103/PhysRevB.52.15150 ↗
28. 10.1007/BF0036215110.1007/BF00362151 ↗
29. 10.1016/0036-9748(86)90400-X10.1016/0036-9748(86)90400-X ↗
30. 10.1016/0022-0248(79)90162-310.1016/0022-0248(79)90162-3 ↗
31. 10.1016/0022-0248(88)90339-910.1016/0022-0248(88)90339-9 ↗
32. 10.1016/1359-6462(96)00091-710.1016/1359-6462(96)00091-7 ↗
33. 10.1116/1.57496910.1116/1.574969 ↗
34. 10.1016/0955-2219(92)90094-T10.1016/0955-2219(92)90094-T ↗
35. 10.1016/S0040-6090(97)00744-X10.1016/S0040-6090(97)00744-X ↗