journal article·2012-01

Dehydroxylation and Rehydroxylation Mechanisms in Fired Clay Ceramic: A TG ‐ MS and DRIFTS Investigation

Francis Clegg, Chris Breen, Margaret A. Carter, Ceren Ince, Shaun D. Savage, Moira A. Wilson

Publisher page

Abstract

Selected instrumental techniques [dilatometry, thermogravimetry – mass spectrometry ( TG ‐ MS ), and variable temperature – diffuse reflectance infrared Fourier transform spectroscopy ( VT ‐ DRIFTS )] have been used to investigate the role of moisture in the rehydroxylation reaction which causes expansion and mass gain in fired clay ceramics. The temperature range over which adsorbed water molecules and structural hydroxyl groups are desorbed from fired clay ceramic as it is reheated, and the nature of the structural hydroxyls that are formed as the ceramic is cooled and then held under controlled conditions have been explored. The mass chromatogram for m / z = 18, supported by VT ‐ DRIFTS , showed that physisorbed water molecules were removed from the ceramic at about 105°C, whereas strongly bound molecules of water and structural hydroxyls were held to ≤500°C. Dilatometry revealed a marked contraction of the ceramic between 200°C and 330°C which corresponded to loss of strongly bound molecules of water. The VT ‐ DRIFTS also showed that the interaction of water molecules with the ceramic body following reheating occurred in two stages and confirmed the kinetic law previously derived from mass gain and moisture expansion in fired clay ceramics.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Glass properties and applications · Recycling and utilization of industrial and municipal waste in materials production · Clay minerals and soil interactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Materials and Engineering Research Institute Sheffield Hallam University Sheffield S1 1WB UK

School of Mechanical Aerospace and Civil Engineering The University of Manchester Manchester M13 9PL UK

References (31)

Show source-provided references
1. 10.1111/j.1151-2916.1928.tb16178.x10.1111/j.1151-2916.1928.tb16178.x ↗
2. Masonry Cracking and Damage Caused by Moisture Expansion of Structural Clay Tile
3. Zsembery S. · 1985 · 1
4. 10.1038/192737a010.1038/192737a0 ↗
5. 10.1103/PhysRevLett.90.12550310.1103/PhysRevLett.90.125503 ↗
6. 10.1111/j.1551-2916.2008.02541.x10.1111/j.1551-2916.2008.02541.x ↗
7. 10.1088/0022-3727/41/5/05540210.1088/0022-3727/41/5/055402 ↗
8. 10.1007/BF0191349010.1007/BF01913490 ↗
9. 10.1111/j.1475-4754.1974.tb01099.x10.1111/j.1475-4754.1974.tb01099.x ↗
10. Investigations on Moisture Expansion of Porous Ceramic Bodies
11. Size Changes of Porous Ceramics Caused by Water and Soluble Salts
12. Moisture Expansion
13. 10.1038/196127a010.1038/196127a0 ↗
14. 10.1016/j.petrol.2007.05.00110.1016/j.petrol.2007.05.001 ↗
15. 10.1098/rspa.2009.011710.1098/rspa.2009.0117 ↗
16. 10.1080/0026897041233129385710.1080/00268970412331293857 ↗
17. 10.1346/CCMN.1994.042060610.1346/CCMN.1994.0420606 ↗
18. 10.1021/j100358a03210.1021/j100358a032 ↗
19. 10.1021/jp980169n10.1021/jp980169n ↗
20. 10.1039/f1975710177710.1039/f19757101777 ↗
21. 10.1021/la950571i10.1021/la950571i ↗
22. Davidov V. Y. · 2000 · 63
23. 10.1016/0167-577X(95)00039-910.1016/0167-577X(95)00039-9 ↗
24. 10.1346/CCMN.2001.049050810.1346/CCMN.2001.0490508 ↗
25. Proportion of Central Atoms in Octahedra of Smectites Calculated from Infrared Spectra
26. 10.1016/S1350-4495(01)00117-710.1016/S1350-4495(01)00117-7 ↗
27. 10.1016/0371-1951(64)80165-X10.1016/0371-1951(64)80165-X ↗
28. 10.1002/anie.19900553110.1002/anie.199005531 ↗
29. 10.1016/0169-1317(94)90022-110.1016/0169-1317(94)90022-1 ↗
30. 10.1016/j.vibspec.2006.04.02210.1016/j.vibspec.2006.04.022 ↗
31. Studies of the Dehydroxylated‐Rehydroxylated Montmorillonite: Structure of the Layers and Intercalation of Water Molecules