journal article·2018-10

Mechanical properties and microstructure evolution of 3D C f /SiBCN composites at elevated temperatures

Qi Ding, Dewei Ni, Zhen Wang, Hongda Wang, Haijun Zhou, Yanmei Kan, Shaoming Dong

Publisher page

Abstract

Abstract 3D C f /SiBCN composites were fabricated by an efficient polymer impregnation and pyrolysis (PIP) method using liquid poly(methylvinyl)borosilazanes as precursor. Mechanical properties and microstructure evolution of the prepared 3D C f /SiBCN composites at elevated temperatures in the range of 1500‐1700°C were investigated. As temperature increased from room temperature (371 ± 31 MPa, 31 ± 2 GPa) to 1500°C (316 ± 29 MPa, 27 ± 3 GPa), strength and elastic modulus of the composite decreased slightly, which degraded seriously as temperature further increased to 1600°C (92 ± 15 MPa, 12 ± 2 GPa) and 1700°C (84 ± 12 MPa, 11 ± 2GPa). To clarify the conversion of failure mechanisms, interfacial shear strength (IFSS) and microstructure evolution of the 3D C f /SiBCN composites at different temperatures were investigated in detail. It reveals that the declines of the strength and changes of the IFSS of the composites are strongly related to the defects and SiC nano‐crystals formed in the composites at elevated temperatures.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

State Key Laboratory of High Performance Ceramics and Superfine Microstructure Shanghai Institute of Ceramics Chinese Academy of Sciences Shanghai China

Structural Ceramics and Composites Engineering Research Center Shanghai Institute of Ceramics Chinese Academy of Sciences Shanghai China

University of Chinese Academy of Sciences Beijing China

ShanghaiTech University Shanghai China

Funding

National Natural Science Foundation of China · Chinese Academy of Sciences

References (20)

Show source-provided references
1. 10.1038/382796a010.1038/382796a0 ↗
2. 10.1111/j.1151-2916.2000.tb01678.x10.1111/j.1151-2916.2000.tb01678.x ↗
3. 10.1016/j.actamat.2005.06.01110.1016/j.actamat.2005.06.011 ↗
4. 10.1016/j.jeurceramsoc.2004.08.00410.1016/j.jeurceramsoc.2004.08.004 ↗
5. 10.1016/j.msea.2010.11.03210.1016/j.msea.2010.11.032 ↗
6. 10.1016/j.ceramint.2017.08.02810.1016/j.ceramint.2017.08.028 ↗
7. 10.1016/j.jeurceramsoc.2016.11.00910.1016/j.jeurceramsoc.2016.11.009 ↗
8. 10.1016/j.actamat.2007.12.00110.1016/j.actamat.2007.12.001 ↗
9. 10.1016/j.actamat.2009.05.03310.1016/j.actamat.2009.05.033 ↗
10. 10.1016/j.carbon.2013.12.00510.1016/j.carbon.2013.12.005 ↗
11. 10.1002/1527-2648(200106)3:6<371::AID-ADEM371>3.0.CO;2-Y10.1002/1527-2648(200106)3:6<371::AID-ADEM371>3.0.CO;2-Y ↗
12. 10.1016/j.apsusc.2015.10.01810.1016/j.apsusc.2015.10.018 ↗
13. 10.1016/j.compositesa.2013.01.01410.1016/j.compositesa.2013.01.014 ↗
14. 10.1016/j.jeurceramsoc.2014.05.03910.1016/j.jeurceramsoc.2014.05.039 ↗
15. 10.1016/j.ceramint.2012.02.04510.1016/j.ceramint.2012.02.045 ↗
16. 10.1111/j.1151-2916.2002.tb00357.x10.1111/j.1151-2916.2002.tb00357.x ↗
17. 10.1007/s10853-012-6683-910.1007/s10853-012-6683-9 ↗
18. 10.1111/jace.1380710.1111/jace.13807 ↗
19. 10.1111/j.1151-2916.2001.tb00984.x10.1111/j.1151-2916.2001.tb00984.x ↗
20. 10.1023/A:100877583083010.1023/A:1008775830830 ↗