Tailoring the microstructure of high porosity Si 3 N 4 foams by direct foaming with mixed surfactants
Source abstract
Abstract
Abstract The mixed surfactants were successfully applied to fabricate the highly porous Si 3 N 4 ceramic foams by the direct foaming method. The oppositely charged surfactants mixed in slurries could combined into catanionic surfactant by the electrostatic attraction and facilitate the formation of ultra‐stable foams. The microstructure of the Si 3 N 4 ceramic foams, including pore structure, mean pore size, pore size distribution and porosity were tailored by varying the mixing ratio of surfactant, mixed surfactants concentration and solid content of the initial slurries. Si 3 N 4 ceramic foams with porosity of 92%‐97%, mean pore size of 140‐240 µm and compressive strength of 0.85‐5.38 MPa were obtained by adjusting mixed surfactants between 0.1 and 0.4 wt% and solid content between 22 and 30 vol%. The compressive strength of Si 3 N 4 ceramic foams in current work was much higher than most reported results.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Mesoporous Materials and Catalysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
State Key Laboratory of High Performance Ceramics and Superfine Microstructure Shanghai Institute of Ceramics, Chinese Academy of Sciences Shanghai China
University of Chinese Academy of Sciences Beijing China
Funding
National Natural Science Foundation of China
References (31)
Show source-provided references
1. 10.1016/S0955-2219(98)00063-610.1016/S0955-2219(98)00063-6 ↗
2. 10.1111/j.1551-2916.2006.01044.x10.1111/j.1551-2916.2006.01044.x ↗
3. 10.1021/la048913k10.1021/la048913k ↗
4. 10.1016/j.matdes.2015.10.02010.1016/j.matdes.2015.10.020 ↗
5. 10.1111/j.1551-2916.2011.05017.x10.1111/j.1551-2916.2011.05017.x ↗
6. 10.1016/j.jeurceramsoc.2012.12.02110.1016/j.jeurceramsoc.2012.12.021 ↗
7. 10.1016/j.jeurceramsoc.2016.06.03010.1016/j.jeurceramsoc.2016.06.030 ↗
8. 10.1016/j.jeurceramsoc.2012.11.01010.1016/j.jeurceramsoc.2012.11.010 ↗
9. 10.1016/j.jeurceramsoc.2015.01.01010.1016/j.jeurceramsoc.2015.01.010 ↗
10. 10.1111/jace.1432010.1111/jace.14320 ↗
11. 10.1016/j.colsurfa.2010.12.01910.1016/j.colsurfa.2010.12.019 ↗
12. 10.1016/j.molliq.2017.03.05910.1016/j.molliq.2017.03.059 ↗
13. 10.1021/acs.jpcb.5b0623110.1021/acs.jpcb.5b06231 ↗
14. 10.1039/c1sm06477k10.1039/c1sm06477k ↗
15. 10.1016/j.ceramint.2015.03.23710.1016/j.ceramint.2015.03.237 ↗
16. 10.1111/j.1151-2916.1999.tb02258.x10.1111/j.1151-2916.1999.tb02258.x ↗
17. 10.1007/BF0071120310.1007/BF00711203 ↗
18. 10.1016/j.cjche.2014.10.01510.1016/j.cjche.2014.10.015 ↗
19. Influence of hydrophobically modified silicon dioxide particles on stability of EOR flooding foam
20. Investigation of macromolecule/surfactant interaction by interfacial dilational rheology method10.3866/PKU.WHXB20090135 ↗
21. 10.1016/j.jeurceramsoc.2006.01.02310.1016/j.jeurceramsoc.2006.01.023 ↗
22. 10.1016/j.cis.2003.08.00310.1016/j.cis.2003.08.003 ↗
23. 10.1016/j.matchemphys.2008.07.09910.1016/j.matchemphys.2008.07.099 ↗
24. 10.1098/rspa.1932.016910.1098/rspa.1932.0169 ↗
25. 10.1021/la970058010.1021/la9700580 ↗
26. 10.1021/la062484410.1021/la0624844 ↗
27. 10.1016/j.ceramint.2018.10.11810.1016/j.ceramint.2018.10.118 ↗
28. 10.1002/adma.20100072910.1002/adma.201000729 ↗
29. 10.1111/j.1744-7402.2012.02847.x10.1111/j.1744-7402.2012.02847.x ↗
30. Porous Si3N4 fabrication via volume‐controlled foaming and their sound absorption properties
31. 10.1111/ijac.1249710.1111/ijac.12497 ↗