White Si–O–C Ceramic: Structure and Thermodynamic Stability
Source abstract
Abstract
While pyrolysis of a polysiloxane precursor in argon typically produces a black amorphous Si–O–C ceramic containing “free” carbon ( sp 2 carbon), pyrolyzing the same precursor in hydrogen leads to a white amorphous ceramic with a negligible amount of sp 2 carbon and a considerable hydrogen content. 29 Si magic‐angle‐spinning nuclear magnetic resonance ( MAS NMR ) spectroscopy confirms the existence of very similar bonding environments of Si atoms in the Si–O–C network for both samples. In addition, 1 H NMR spectroscopic measurements on both samples reveal that the hydrogen atoms are bonded mainly to carbon. For the thermodynamic analysis, the enthalpies of formation with respect to the most stable components ( SiO 2 , SiC , C ) of the black‐and‐white Si – O – C samples obtained after the pyrolysis at 1100°C are determined using high‐temperature oxidative drop‐solution calorimetry in a molten oxide solvent. The white ceramic is 6 kJ/g‐atom more stable in enthalpy than the black one. Although the role of hydrogen in the thermodynamic stability of the white sample remains ambiguous, the thermodynamic findings and structural analysis suggest that the existence of sp 2 ‐bonded carbon in the amorphous network of polymer derived Si–O–C ceramics does not provide additional thermodynamic stability to the ceramic.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Glass properties and applications · Nuclear materials and radiation effects
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Peter A. Rock Thermochemistry Laboratory and NEAT ORU University of California Davis California 95616
Graduate School of Engineering Osaka Prefecture University 1‐1 Gakuen‐Cho, Naka‐Ku, Sakai Osaka 599‐8531 Japan
Department of Chemical Engineering and Materials Science University of California Davis California 95616
Funding
National Science Foundation
References (30)
Show source-provided references
1. 10.1016/0955-2219(95)00186-710.1016/0955-2219(95)00186-7 ↗
2. 10.1111/j.1551-2916.2010.03876.x10.1111/j.1551-2916.2010.03876.x ↗
3. 10.1557/JMR.1991.272310.1557/JMR.1991.2723 ↗
4. 10.1016/S0955-2219(00)00068-610.1016/S0955-2219(00)00068-6 ↗
5. 10.1111/j.1151-2916.2001.tb01000.x10.1111/j.1151-2916.2001.tb01000.x ↗
6. 10.1111/j.1151-2916.2001.tb00789.x10.1111/j.1151-2916.2001.tb00789.x ↗
7. 10.1016/j.jnoncrysol.2005.06.00810.1016/j.jnoncrysol.2005.06.008 ↗
8. 10.1023/A:100872381399110.1023/A:1008723813991 ↗
9. 10.1016/j.scriptamat.2013.07.00910.1016/j.scriptamat.2013.07.009 ↗
10. 10.1111/j.1151-2916.1995.tb08811.x10.1111/j.1151-2916.1995.tb08811.x ↗
11. 10.1063/1.348293810.1063/1.3482938 ↗
12. 10.1246/bcsj.2011035710.1246/bcsj.20110357 ↗
13. 10.1002/chem.1996002120710.1002/chem.19960021207 ↗
14. 10.1007/BF0030752610.1007/BF00307526 ↗
15. 10.1007/s00269005003510.1007/s002690050035 ↗
16. 10.1016/S0925-8388(01)00965-310.1016/S0925-8388(01)00965-3 ↗
17. 10.1111/j.1551-2916.2007.01874.x10.1111/j.1551-2916.2007.01874.x ↗
18. 10.1111/j.1551-2916.2008.02543.x10.1111/j.1551-2916.2008.02543.x ↗
19. 10.1111/j.1551-2916.2008.02626.x10.1111/j.1551-2916.2008.02626.x ↗
20. 10.1111/j.1551-2916.2008.02427.x10.1111/j.1551-2916.2008.02427.x ↗
21. 10.1016/j.actamat.2012.05.01010.1016/j.actamat.2012.05.010 ↗
22. 10.1111/jace.1265810.1111/jace.12658 ↗
23. 10.1557/JMR.1999.026410.1557/JMR.1999.0264 ↗
24. 10.1557/JMR.1999.062610.1557/JMR.1999.0626 ↗
25. 10.1557/jmr.2006.003310.1557/jmr.2006.0033 ↗
26. 10.1111/j.1551-2916.2006.00920.x10.1111/j.1551-2916.2006.00920.x ↗
27. 10.1021/cm102143210.1021/cm1021432 ↗
28. 10.1039/c2ta00727d10.1039/c2ta00727d ↗
29. Bale C. W. · 2002 · 189
30. R. A.RobieandB. S.Hemingway “Thermodynamic Properties of Minerals and Related Substances at 298.15 K and 1 Bar (105Pascals) Pressure and at Higher Temperatures”; in U. S. Geological Survey Bulletin 2131 Washington 1995.