Low‐Temperature Sintering and Microwave Dielectric Properties of V 2 O 5 ‐Added Zn 2 SiO 4 Ceramics
Source abstract
Abstract
V 2 O 5 was added to ceramics of nominal composition Zn 1.8 SiO 3.8 (ZS) in order to decrease their sintering temperature for application to low‐temperature cofired ceramic devices. For the specimens sintered at 875°C, a dense microstructure was developed when the V 2 O 5 content exceeded 9.0 mol% due to the presence of the liquid phase containing SiO 2 and V 2 O 5 . The microwave dielectric properties of the ZS ceramics were influenced by the V 2 O 5 content. Good microwave dielectric properties of Q × f =17 500 GHz, ɛ r =7.3, and τ f =−28 ppm/°C were obtained from the specimen containing 12.0 mol% V 2 O 5 sintered at 875°C for 2 h.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Microwave Dielectric Ceramics Synthesis · Ferroelectric and Piezoelectric Materials · Acoustic Wave Resonator Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. 10.1111/j.1151-2916.1991.tb04320.x10.1111/j.1151-2916.1991.tb04320.x ↗
2. 10.1016/j.jeurceramsoc.2005.09.00810.1016/j.jeurceramsoc.2005.09.008 ↗
3. 10.4191/KCERS.2003.40.4.35010.4191/KCERS.2003.40.4.350 ↗
4. 10.4028/www.scientific.net/KEM.269.19510.4028/www.scientific.net/KEM.269.195 ↗
5. 10.1016/S0955-2219(03)00167-510.1016/S0955-2219(03)00167-5 ↗
6. 10.4028/www.scientific.net/KEM.269.19910.4028/www.scientific.net/KEM.269.199 ↗
7. 10.1111/j.1551-2916.2006.01435.x10.1111/j.1551-2916.2006.01435.x ↗
8. 10.1111/j.1551-2916.2007.01891.x10.1111/j.1551-2916.2007.01891.x ↗
9. Phase Equilibria Diagrams CD‐ROM Database Version 3.0.1 The American Ceramic Society Fig. 02401.
10. 10.1109/TMTT.1960.112474910.1109/TMTT.1960.1124749 ↗
11. 10.1109/TMTT.1970.112727110.1109/TMTT.1970.1127271 ↗
12. S.‐I.Yoo Korea–UK Seminar on Microwave Dielectric Materials Seoul Koyuk Munhwa‐Hoekwan Korea February 7–8 2003.