journal article·2017-06

Microstructure and mechanical properties of TaC ceramics with 1–7.5 mol% Si as sintering aid

Guihong Geng, Limeng Liu, Yujin Wang, Wanxiu Hai, Wenzhou Sun, Yuhong Chen, Laner Wu

Publisher page

Abstract

Abstract Metallic Si as sintering aid was effective in densifying tantalum carbide ceramic (TaC) by spark plasma sintering ( SPS ) at 1700°C. Full density was reached at 5.0 mol% Si addition (equivalent to 1.088% Si in weight) and above. Enhanced densification of TaC ceramic with Si was associated with decrease in oxygen content from ~0.24 wt% in TaC powder to ~0.03 wt% in consolidated specimen. Rest of the oxygen species was collected at multigrain conjunctions to form SiO 2 ‐based liquid at high temperatures. Upon cooling, Ta, Si, O, and C dissolving in the liquid precipitated minor phases of TaSi x and SiC of low concentrations. Microstructure of TaC ceramics was refined by the Si addition, with average grain size decreasing from 11±8 μm at 1.0 mol% Si to 3±2 μm at 7.5 mol% Si addition. Ta solute in SiC and Si solute in TaC were evidenced. TaC ceramic containing 7.5 mol% Si had a relatively good flexural strength and fracture toughness of 646±51 MPa and 5.0 MPa·m 1/2 , respectively.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering Beifang University of Nationalities Yinchuan China

School of Materials Science and Engineering Harbin Institute of Technology Harbin China

Funding

National Natural Science Foundation of China · Beifang University of Nationalities

References (35)

Show source-provided references
1. 10.1016/j.jeurceramsoc.2014.11.01810.1016/j.jeurceramsoc.2014.11.018 ↗
2. 10.1111/j.1551-2916.2007.01583.x10.1111/j.1551-2916.2007.01583.x ↗
3. 10.1016/j.jeurceramsoc.2012.02.03510.1016/j.jeurceramsoc.2012.02.035 ↗
4. 10.1016/j.scriptamat.2008.05.02610.1016/j.scriptamat.2008.05.026 ↗
5. 10.1111/j.1551-2916.2009.03201.x10.1111/j.1551-2916.2009.03201.x ↗
6. 10.1016/j.msea.2008.09.02410.1016/j.msea.2008.09.024 ↗
7. 10.1111/jace.1363510.1111/jace.13635 ↗
8. 10.1016/j.scriptamat.2013.06.02410.1016/j.scriptamat.2013.06.024 ↗
9. 10.1016/j.actamat.2014.11.00510.1016/j.actamat.2014.11.005 ↗
10. 10.1111/j.1551-2916.2006.01416.x10.1111/j.1551-2916.2006.01416.x ↗
11. 10.1179/pom.1966.9.17.00210.1179/pom.1966.9.17.002 ↗
12. 10.1016/j.msea.2011.09.07910.1016/j.msea.2011.09.079 ↗
13. 10.1016/j.jeurceramsoc.2012.04.04210.1016/j.jeurceramsoc.2012.04.042 ↗
14. 10.1016/j.jeurceramsoc.2010.01.03210.1016/j.jeurceramsoc.2010.01.032 ↗
15. 10.1111/j.1551-2916.2008.02780.x10.1111/j.1551-2916.2008.02780.x ↗
16. 10.1016/j.jeurceramsoc.2011.07.00310.1016/j.jeurceramsoc.2011.07.003 ↗
17. 10.1016/j.compositesb.2014.11.04310.1016/j.compositesb.2014.11.043 ↗
18. 10.1016/j.ceramint.2014.09.07010.1016/j.ceramint.2014.09.070 ↗
19. 10.1111/j.1551-2916.2009.03437.x10.1111/j.1551-2916.2009.03437.x ↗
20. 10.1016/j.ceramint.2015.05.12410.1016/j.ceramint.2015.05.124 ↗
21. Pressure‐densification in tantalum carbide
22. 10.1007/BF0076179610.1007/BF00761796 ↗
23. 10.1016/j.ijrmhm.2015.06.01510.1016/j.ijrmhm.2015.06.015 ↗
24. 10.1016/j.matchemphys.2014.10.05210.1016/j.matchemphys.2014.10.052 ↗
25. 10.1111/j.1551-2916.2010.04210.x10.1111/j.1551-2916.2010.04210.x ↗
26. 10.1016/j.mser.2008.09.00310.1016/j.mser.2008.09.003 ↗
27. 10.1016/j.scriptamat.2014.03.01110.1016/j.scriptamat.2014.03.011 ↗
28. Standard Test Methods for Determining Average Grain Size. ASTM 112‐13.
29. 10.1111/j.1151-2916.1969.tb11968.x10.1111/j.1151-2916.1969.tb11968.x ↗
30. 10.1149/1.243023110.1149/1.2430231 ↗
31. 10.1063/1.33373810.1063/1.333738 ↗
32. Rahaman MN · 2003
33. 10.1557/jmr.2009.023210.1557/jmr.2009.0232 ↗
34. 10.1016/j.jeurceramsoc.2013.01.01710.1016/j.jeurceramsoc.2013.01.017 ↗
35. 10.1021/j100905a02810.1021/j100905a028 ↗