Simultaneous control of particle size and morphology of α‐Ca SO 4 ·1/2H 2 O with organic additives
Source abstract
Abstract
Abstract Here we reported a method to simultaneously control the particle size and morphology of α‐Ca SO 4 ·1/2H 2 O (α‐ HH ) prepared from flue gas desulfurization gypsum by adjusting the succinic acid concentration and glycerol content under mild conditions. Succinic acid controlled the crystal morphology by adsorption onto α‐ HH surfaces, and glycerol controlled the crystal particle size, in which an increase in the maximal relative supersaturation ( S max ) and nucleation rate of α‐ HH was hypothesized to cause the change in α‐ HH particle size. Then, based on the method, α‐ HH with different particle sizes but with almost the same morphology was prepared, and the influence of the crystal particle size on the mechanical strength of the α‐ HH pastes was explored. With decreasing α‐ HH particle size from about 26 to 5 μm, the dry compressive strength of the pastes made from the α‐ HH decreased remarkably from 68.02 to 34.85 MPa, which was ascribed to an increase in the internal porosity of the pastes.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Calcium Carbonate Crystallization and Inhibition · Crystallization and Solubility Studies · Industrial Gas Emission Control
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Resource Environment and Safety Engineering Hunan University of Science and Technology Xiangtan China
School of Mineral Processing and Bioengineering Central South University Changsha China
College of Chemical and Environmental Engineering Shandong University of Science and Technology Qingdao China
Funding
Central South University
References (53)
Show source-provided references
1. 10.1107/S160057671500714110.1107/S1600576715007141 ↗
2. 10.1111/j.1551-2916.2009.03330.x10.1111/j.1551-2916.2009.03330.x ↗
3. 10.1111/j.1551-2916.2008.02729.x10.1111/j.1551-2916.2008.02729.x ↗
4. 10.1002/jctb.501018100510.1002/jctb.5010181005 ↗
5. 10.1016/j.fuel.2009.01.00410.1016/j.fuel.2009.01.004 ↗
6. The treatment of gypsum as a product of the flue gas desulphurization process
7. 10.1111/j.1151-2916.1991.tb04351.x10.1111/j.1151-2916.1991.tb04351.x ↗
8. 10.1021/ie201040y10.1021/ie201040y ↗
9. 10.1111/j.1551-2916.2011.04470.x10.1111/j.1551-2916.2011.04470.x ↗
10. Nonlattice cation‐SO4 2– ion pairs in calcium sulfate hemihydrate nucleation
11. 10.1021/acs.iecr.6b0206410.1021/acs.iecr.6b02064 ↗
12. 10.4028/www.scientific.net/KEM.477.11810.4028/www.scientific.net/KEM.477.118 ↗
13. 10.1016/j.powtec.2008.05.00710.1016/j.powtec.2008.05.007 ↗
14. 10.1002/jbm.82029010510.1002/jbm.820290105 ↗
15. Influence of organic acid structure on crystal morphology of α‐hemihydrate desulfurization gypsum and its crystal modification mechanism
16. 10.1111/j.1551-2916.2008.02358.x10.1111/j.1551-2916.2008.02358.x ↗
17. 10.4028/www.scientific.net/KEM.240-242.36910.4028/www.scientific.net/KEM.240-242.369 ↗
18. 10.1016/j.biomaterials.2004.05.01010.1016/j.biomaterials.2004.05.010 ↗
19. 10.1021/acs.est.6b0115210.1021/acs.est.6b01152 ↗
20. 10.1021/acs.est.7b0290110.1021/acs.est.7b02901 ↗
21. 10.1016/j.powtec.2010.02.01510.1016/j.powtec.2010.02.015 ↗
22. 10.1021/la502451f10.1021/la502451f ↗
23. 10.1127/0935-1221/2001/0013/098510.1127/0935-1221/2001/0013/0985 ↗
24. 10.1006/jssc.1995.126010.1006/jssc.1995.1260 ↗
25. 10.1021/acs.iecr.5b0058510.1021/acs.iecr.5b00585 ↗
26. 10.1021/la302459z10.1021/la302459z ↗
27. Morris MD · 1976
28. 10.1016/j.ces.2017.02.01310.1016/j.ces.2017.02.013 ↗
29. XPS characterization of chalcopyrite, tetrahedrite, and tennantite surface products after different conditioning. 1. Aqueous solution at pH 10
30. 10.1016/j.jallcom.2018.07.06810.1016/j.jallcom.2018.07.068 ↗
31. 10.1016/j.mineng.2012.07.01610.1016/j.mineng.2012.07.016 ↗
32. 10.1016/j.vacuum.2015.12.00610.1016/j.vacuum.2015.12.006 ↗
33. 10.1002/sia.516510.1002/sia.5165 ↗
34. 10.1016/S0003-2670(97)00111-610.1016/S0003-2670(97)00111-6 ↗
35. 10.1039/C5CE01923K10.1039/C5CE01923K ↗
36. 10.1111/j.1744-7402.2012.02800.x10.1111/j.1744-7402.2012.02800.x ↗
37. 10.1039/C5RA07712E10.1039/C5RA07712E ↗
38. 10.1116/1.57268010.1116/1.572680 ↗
39. 10.1016/0378-5963(83)90018-110.1016/0378-5963(83)90018-1 ↗
40. 10.1016/0924-0136(95)02023-310.1016/0924-0136(95)02023-3 ↗
41. 10.1016/0169-4332(86)90107-810.1016/0169-4332(86)90107-8 ↗
42. 10.1016/S0008-8846(98)00037-410.1016/S0008-8846(98)00037-4 ↗
43. 10.1016/0008-8846(85)90044-410.1016/0008-8846(85)90044-4 ↗
44. 10.1007/s00706-003-0590-310.1007/s00706-003-0590-3 ↗
45. 10.1007/BF0166609110.1007/BF01666091 ↗
46. 10.1524/zkri.1995.210.3.19910.1524/zkri.1995.210.3.199 ↗
47. 10.1016/j.jcrysgro.2003.12.04710.1016/j.jcrysgro.2003.12.047 ↗
48. 10.1021/cr60006a00210.1021/cr60006a002 ↗
49. Shi EW · 2004
50. 10.1021/ie400796810.1021/ie4007968 ↗
51. 10.1016/j.cep.2005.12.00610.1016/j.cep.2005.12.006 ↗
52. Correlation of diffusion coefficients in dilute solutions10.1002/aic.690010222 ↗
53. 10.1016/S0022-0248(98)01156-710.1016/S0022-0248(98)01156-7 ↗