journal article·2012-01

Intact and Predamaged Boron Carbide Strength under Moderate Confinement Pressures

Sidney Chocron, Charles E. Anderson, Kathryn A. Dannemann, Arthur E. Nicholls, Nikki L. King

Publisher page

Abstract

This article summarizes the characterization work performed on intact and predamaged boron carbide tested in compression under confinement in a pressure vessel or using a thick steel confining sleeve. The focus is on the effect of pressure (up to 2 GPa hydrostatic pressure) on the strength. The techniques used for characterization are described. The failure curves obtained are presented and written as Drucker‐Prager and Mohr‐Coulomb failure criteria. Optical and stereomicroscopy were used to evaluate and document damage. Finally, the results are discussed and compared to the literature. It is shown that data obtained with very different techniques (confined compression, plate impact, and divergent plate impact) overlap, increasing the confidence in the results.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-Velocity Impact and Material Behavior · Boron and Carbon Nanomaterials Research · Energetic Materials and Combustion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Engineering Dynamics Department Southwest Research Institute San Antonio Texas 78238

References (36)

Show source-provided references
1. Bridgman P. W. · 1952
2. 10.2172/417315110.2172/4173151 ↗
3. 10.1007/BF0055061410.1007/BF00550614 ↗
4. Johnson G. R. · 1990
5. Lankford J. · 1991
6. 10.1023/A:101757612302610.1023/A:1017576123026 ↗
7. 10.1111/j.1744-7402.2004.tb00171.x10.1111/j.1744-7402.2004.tb00171.x ↗
8. 10.1007/BF0232871210.1007/BF02328712 ↗
9. 10.1111/j.1151-2916.1996.tb07913.x10.1111/j.1151-2916.1996.tb07913.x ↗
10. Ahrens T. J. · 1996
11. 10.1016/S0022-5096(97)00006-910.1016/S0022-5096(97)00006-9 ↗
12. 10.1023/A:100767242270010.1023/A:1007672422700 ↗
13. 10.1111/j.1551-2916.2005.00688.x10.1111/j.1551-2916.2005.00688.x ↗
14. 10.1111/j.1551-2916.2007.01515.x10.1111/j.1551-2916.2007.01515.x ↗
15. 10.1111/j.1551-2916.2008.02712.x10.1111/j.1551-2916.2008.02712.x ↗
16. Walker J. D. · 1995 · 179
17. 10.1007/BF0232754610.1007/BF02327546 ↗
18. 10.1111/j.1551-2916.2010.03863.x10.1111/j.1551-2916.2010.03863.x ↗
19. 10.1111/j.1744-7402.2010.02540.x10.1111/j.1744-7402.2010.02540.x ↗
20. 10.1063/1.37064310.1063/1.370643 ↗
21. 10.1063/1.236297910.1063/1.2362979 ↗
22. Compressive Failure Threshold of Brittle Materials10.1002/9781118408100.ch12 ↗
23. 10.1016/j.ijimpeng.2010.10.02710.1016/j.ijimpeng.2010.10.027 ↗
24. Dannemann K. A. · 2004
25. Chocron S. · 2010
26. Desai C. S. · 1984
27. 10.1090/qam/4829110.1090/qam/48291 ↗
28. 10.1017/CBO978051160004310.1017/CBO9780511600043 ↗
29. 10.1016/j.msea.2007.06.05310.1016/j.msea.2007.06.053 ↗
30. Timoshenko S. · 1951
31. Investigations on Granular Ceramics and Ceramic Powder
32. 10.1016/j.ijimpeng.2003.10.02110.1016/j.ijimpeng.2003.10.021 ↗
33. 10.1063/1.168690210.1063/1.1686902 ↗
34. 10.1016/0734-743X(87)90029-710.1016/0734-743X(87)90029-7 ↗
35. 10.1016/j.ijimpeng.2011.03.00710.1016/j.ijimpeng.2011.03.007 ↗
36. 10.1007/BF0087800210.1007/BF00878002 ↗