journal article·2018-09

Foam glass obtained through high‐pressure sintering

Martin B. Østergaard, Rasmus R. Petersen, Jakob König, Michal Bockowski, Yuanzheng Yue

Publisher page

Abstract

Abstract Foam glasses are usually prepared through a chemical approach, that is, by mixing glass powder with foaming agents, and heating the mixture to a temperature above the softening point (10 6.6 Pa s) of the glass. The foaming agents release gas, enabling expansion of the sintered glass. Here, we use a physical foaming approach to prepare foam glass. First, closed pores filled with inert gases (He, Ar, or N 2 ) are physically introduced into a glass body by sintering cathode ray tube ( CRT ) panel glass powder at high gas pressure (5‐25 MP a) at 640°C and, then cooled to room temperature. The sintered bodies are subjected to a second heat treatment above the glass transition temperature at atmospheric pressure. This heat treatment causes expansion of the pores due to high internal gas pressure. We found that the foaming ability strongly depends on the gas pressure applied during sintering, and on the kinetic diameters of the gases. The pressure for attaining maximum expansion, that is, lowest density and highest porosity, is found to be around 20 MP a.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Pigment Synthesis and Properties · Glass properties and applications · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Chemistry and Bioscience Aalborg University Aalborg Denmark

Advanced Materials Department Jožef Stefan Institute Ljubljana Slovenia

Institute of High‐Pressure Physics Polish Academy of Sciences Warsaw Poland

References (34)

Show source-provided references
1. 10.1002/3527606696.ch2g10.1002/3527606696.ch2g ↗
2. Gibson LJ · 1999
3. LongB.Glass product and method of manufacturing sponge‐like glass. US Patent 1 945 052 1934. p.1‐2.
4. KernL.Process of manufacturing porous silica ware. US Patent 1 898 839 1933. p.1‐2.
5. Foaming of CRT panel glass powder using Na2CO3
6. 10.1016/j.jeurceramsoc.2013.12.02010.1016/j.jeurceramsoc.2013.12.020 ↗
7. 10.1016/j.ceramint.2014.10.12710.1016/j.ceramint.2014.10.127 ↗
8. 10.1016/j.ceramint.2014.05.05310.1016/j.ceramint.2014.05.053 ↗
9. 10.1016/j.jnoncrysol.2015.05.03010.1016/j.jnoncrysol.2015.05.030 ↗
10. 10.1016/j.ceramint.2015.04.05110.1016/j.ceramint.2015.04.051 ↗
11. 10.1179/1743676114Y.000000015110.1179/1743676114Y.0000000151 ↗
12. 10.1016/j.jnoncrysol.2017.12.04110.1016/j.jnoncrysol.2017.12.041 ↗
13. 10.1088/1748-6041/3/3/03400510.1088/1748-6041/3/3/034005 ↗
14. 10.1016/j.jeurceramsoc.2017.01.01210.1016/j.jeurceramsoc.2017.01.012 ↗
15. 10.3390/ma307386710.3390/ma3073867 ↗
16. 10.1016/j.actamat.2012.04.01610.1016/j.actamat.2012.04.016 ↗
17. KearnsMW.Formation of porous bodies. US Patent 4 659 546 1987. p.49‐51.
18. 10.1016/j.actamat.2004.01.03910.1016/j.actamat.2004.01.039 ↗
19. 10.1016/j.actamat.2010.04.03410.1016/j.actamat.2010.04.034 ↗
20. 10.1016/S1359-6462(00)00614-X10.1016/S1359-6462(00)00614-X ↗
21. 10.1007/978-3-642-04830-2_1010.1007/978-3-642-04830-2_10 ↗
22. 10.1016/j.jnoncrysol.2016.10.04110.1016/j.jnoncrysol.2016.10.041 ↗
23. 10.1201/b13722-210.1201/b13722-2 ↗
24. 10.1039/b802426j10.1039/b802426j ↗
25. Shelby JE · 1996
26. 10.1073/pnas.110236110810.1073/pnas.1102361108 ↗
27. 10.1038/ncomms134310.1038/ncomms1343 ↗
28. 10.1111/j.1151-2916.1953.tb12843.x10.1111/j.1151-2916.1953.tb12843.x ↗
29. 10.1103/PhysRevLett.109.24550410.1103/PhysRevLett.109.245504 ↗
30. 10.1103/PhysRevB.93.22430310.1103/PhysRevB.93.224303 ↗
31. 10.1016/j.jnoncrysol.2017.03.03510.1016/j.jnoncrysol.2017.03.035 ↗
32. Evaluation of foaming behavior of glass melts by high‐temperature microscopy10.1111/ijag.12185 ↗
33. 10.1016/j.ceramint.2008.10.02210.1016/j.ceramint.2008.10.022 ↗
34. 10.1016/j.jnoncrysol.2016.05.02110.1016/j.jnoncrysol.2016.05.021 ↗