Structural and electric properties of Ce‐doped Na 0.5 Bi 4.5 Ti 4 O 15 piezoceramics with high Curie temperatures
Source abstract
Abstract
Abstract Na 0.5 Bi 4.5‐ x Ce x Ti 4 O 15 ( x = 0, 0.02, 0.04, 0.06, 0.08, 0.10) lead‐free piezoelectric ceramics with high Curie temperatures are fabricated using the conventional solid‐phase method. The effects of the Ce content on the phase structures, morphologies, and electrical properties of the Na 0.5 Bi 4.5‐ x Ce x Ti 4 O 15 ceramics are systematically investigated. The appropriate content of Ce increases b/a and c/a and induces the distortion of the crystal structure. The increased b/a leads to a transverse asymmetry of the Na 0.5 Bi 4.5‐ x Ce x Ti 4 O 15 ceramics, which facilitates the dipole flipping, thus enhancing the piezoelectric properties ( d 33 = 20 pC/N). Although the improved c/a increases the degree of tetragonality of the Na 0.5 Bi 4.5‐ x Ce x Ti 4 O 15 ceramic, which decreases the Curie temperature ( T C ), the T C values of all samples are higher than 600°C, considerably higher than the practical application temperature. The Ce doping significantly reduces the dielectric loss of the sample and increases its dielectric performance. The improvements in electric properties by the cerium doping can expand its use in high‐temperature environments for oilfield logging, aerospace, and military applications.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Acoustic Wave Resonator Technologies · Multiferroics and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Key Laboratory of Ferro and Piezoelectric Materials and Devices of Hubei Province Hubei Collaborative Innovation Center for Advanced Organic Chemical Materials Key Laboratory of Green Preparation and Application for Functional Materials Ministry of Education, and School of Physics and Electronic Science Hubei University Wuhan PR China
School of Materials Science and Engineering Hubei University Wuhan China
Funding
Natural Science Foundation of Hubei Province
References (29)
Show source-provided references
1. 10.1016/j.jeurceramsoc.2006.04.07310.1016/j.jeurceramsoc.2006.04.073 ↗
2. 10.1111/jace.1541910.1111/jace.15419 ↗
3. 10.1111/j.1551-2916.2009.03261.x10.1111/j.1551-2916.2009.03261.x ↗
4. 10.1016/j.ceramint.2015.06.06710.1016/j.ceramint.2015.06.067 ↗
5. 10.1038/nmat378210.1038/nmat3782 ↗
6. 10.1088/0022-3727/41/4/04540110.1088/0022-3727/41/4/045401 ↗
7. Synthesis and properties of lead free ferroelectric Na0.5Bi0.5TiO3 ceramic at different sintering temperature
8. 10.1016/j.ceramint.2016.09.16810.1016/j.ceramint.2016.09.168 ↗
9. 10.1088/0022-3727/42/3/03541110.1088/0022-3727/42/3/035411 ↗
10. Mixed bismuth oxides with layer lattices
11. 10.1111/jace.1603310.1111/jace.16033 ↗
12. 10.1007/s11595-016-1478-510.1007/s11595-016-1478-5 ↗
13. 10.1016/j.matchemphys.2014.11.07410.1016/j.matchemphys.2014.11.074 ↗
14. 10.1016/j.ceramint.2018.07.03710.1016/j.ceramint.2018.07.037 ↗
15. 10.1016/j.ceramint.2017.07.12810.1016/j.ceramint.2017.07.128 ↗
16. 10.1111/jace.1411510.1111/jace.14115 ↗
17. 10.1016/j.jallcom.2018.06.12710.1016/j.jallcom.2018.06.127 ↗
18. 10.3938/jkps.71.41310.3938/jkps.71.413 ↗
19. 10.1023/A:100993651515210.1023/A:1009936515152 ↗
20. 10.1016/j.matlet.2016.05.14810.1016/j.matlet.2016.05.148 ↗
21. 10.1088/2053-1591/ab3ae610.1088/2053-1591/ab3ae6 ↗
22. 10.1016/j.jmat.2019.12.00110.1016/j.jmat.2019.12.001 ↗
23. 10.1016/j.jallcom.2010.06.20010.1016/j.jallcom.2010.06.200 ↗
24. 10.1039/C4DT01712A10.1039/C4DT01712A ↗
25. 10.1088/1674-1056/26/4/04770110.1088/1674-1056/26/4/047701 ↗
26. 10.1016/j.ceramint.2012.08.01310.1016/j.ceramint.2012.08.013 ↗
27. 10.1002/adma.20040186010.1002/adma.200401860 ↗
28. 10.1021/acsnano.5b0337110.1021/acsnano.5b03371 ↗
29. 10.1111/jace.1625010.1111/jace.16250 ↗