Novel phenomenon of quasi‐volcanic corrosion on the alumina refractory‐slag‐air interface
Source abstract
Abstract
Abstract A novel phenomenon of quasi‐volcanic corrosion at refractory – slag – air interface under simulated normal smelting conditions was discovered when alumina refractory came in contact with CaO‐Al 2 O 3 ‐SiO 2 slags and soaked at 1600°C. Based on thermodynamic and microstructure analysis, the mechanism of quasi‐volcanic corrosion was revealed and the effect of CaO/SiO 2 mass ratio (C/S ratio) on corrosion was discussed. The results indicate that a two‐stage intensified convection led to the severe upwelling corrosion of the refractory at the triple‐phase interface. Furthermore, the critical intensity of the corrosive convection at the first stage on the formation of “slag volcano” was determined. This can serve as guidance for prolonging the service life of alumina refractory.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Magnesium Oxide Properties and Applications · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
The State Key Laboratory of Refractories and Metallurgy Wuhan University of Science and Technology Wuhan China
Funding
National Natural Science Foundation of China
References (36)
Show source-provided references
1. 10.1016/j.corsci.2020.10851710.1016/j.corsci.2020.108517 ↗
2. 10.1111/jace.1684110.1111/jace.16841 ↗
3. 10.1016/j.corsci.2019.10818210.1016/j.corsci.2019.108182 ↗
4. 10.1016/j.ceramint.2018.05.08510.1016/j.ceramint.2018.05.085 ↗
5. 10.1098/rsta.1998.020610.1098/rsta.1998.0206 ↗
6. 10.2355/isijinternational.32.1910.2355/isijinternational.32.19 ↗
7. Harmuth H · 2014 · 14
8. 10.1016/j.ceramint.2017.10.09510.1016/j.ceramint.2017.10.095 ↗
9. 10.1007/s11663-020-01788-x10.1007/s11663-020-01788-x ↗
10. 10.1111/jace.1533710.1111/jace.15337 ↗
11. 10.1038/187186a010.1038/187186a0 ↗
12. 10.1016/j.ijheatmasstransfer.2015.06.01510.1016/j.ijheatmasstransfer.2015.06.015 ↗
13. 10.1016/j.jcrysgro.2012.02.03110.1016/j.jcrysgro.2012.02.031 ↗
14. 10.1002/srin.20110029410.1002/srin.201100294 ↗
15. 10.1063/1.496654210.1063/1.4966542 ↗
16. Struktur des randes von wassertropfen bei benetzung von glas und ihre bedeutung
17. 10.1034/j.1600-0692.2002.00542.x10.1034/j.1600-0692.2002.00542.x ↗
18. 10.1016/j.corsci.2018.08.02210.1016/j.corsci.2018.08.022 ↗
19. 10.1016/j.jeurceramsoc.2005.12.02510.1016/j.jeurceramsoc.2005.12.025 ↗
20. The corrosion of refractory castables
21. 10.1007/BF0113870910.1007/BF01138709 ↗
22. 10.2320/jinstmet1952.47.5_39710.2320/jinstmet1952.47.5_397 ↗
23. 10.1111/jace.1620510.1111/jace.16205 ↗
24. A novel approach to lightweight alumina‐carbon refractories for flow control of molten steel
25. 10.1007/s11663-018-1300-110.1007/s11663-018-1300-1 ↗
26. 10.1179/1751584X13Y.000000003910.1179/1751584X13Y.0000000039 ↗
27. 10.1016/j.corsci.2017.01.01810.1016/j.corsci.2017.01.018 ↗
28. 10.1179/09506608779015029610.1179/095066087790150296 ↗
29. 10.1007/s11663-010-9385-110.1007/s11663-010-9385-1 ↗
30. 10.3390/min1003025710.3390/min10030257 ↗
31. 10.2355/isijinternational.47.93510.2355/isijinternational.47.935 ↗
32. 10.1016/j.pepi.2009.10.00110.1016/j.pepi.2009.10.001 ↗
33. 10.1038/ngeo111110.1038/ngeo1111 ↗
34. 10.1002/2014GC00564110.1002/2014GC005641 ↗
35. 10.1002/2016GL06948310.1002/2016GL069483 ↗
36. 10.1016/j.tecto.2017.04.01510.1016/j.tecto.2017.04.015 ↗