Precipitation Coating of Monazite on Woven Ceramic Fibers: III—Coating without Strength Degradation Using a Phytic Acid Precursor
Source abstract
Abstract
Multiple coatings of La‐monazite (LaPO 4 ) were applied to Nextel ™ 610 and 720 oxide fibers using a heterogeneous nucleation and growth coating process with phytic acid solution precursors. The as‐processed coatings were found to be largely amorphous. Coated fibers were heat treated at 1200°C for 1–2 h, whereupon the coatings crystallized to porous LaPO 4 with thin (50–100 nm) layers of AlPO 4 at the fiber–coating interface. Heat‐treated fibers exhibited full strength retention, in marked contrast to fibers coated by precipitation using citric acid precursors as in a previous work. The microstructural evolution of the amorphous coatings was studied as a function of temperature. AlPO 4 forms at the fiber–coating interface between 700° and 800°C, before high‐temperature outgassing of the coating as measured by TGA. NMR spectroscopy was used to study as‐precipitated powders and as‐processed coatings to gain insights into the structural nature of the materials. A possible explanation for the retention of fiber strength through the coating process is proposed and discussed in light of the experimental evidence.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Layered Double Hydroxides Synthesis and Applications · MXene and MAX Phase Materials · Extraction and Separation Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. 10.1016/0266-3538(91)90010-M10.1016/0266-3538(91)90010-M ↗
2. The Role of the Fiber‐Matrix Interface in Ceramic Composites
3. Interface Design for Oxidation‐Resistant Ceramic Composites10.1111/j.1151-2916.2002.tb00505.x ↗
4. 10.1016/0921-5093(90)90026-Y10.1016/0921-5093(90)90026-Y ↗
5. 10.1111/j.1151-2916.1995.tb08851.x10.1111/j.1151-2916.1995.tb08851.x ↗
6. 10.1016/S0955-2219(99)00112-010.1016/S0955-2219(99)00112-0 ↗
7. 10.1016/S0955-2219(99)00256-310.1016/S0955-2219(99)00256-3 ↗
8. 10.1111/j.1151-2916.2003.tb00018.x10.1111/j.1151-2916.2003.tb00018.x ↗
9. R. S.Hay“Method for Coating Continuous Tows ” U. S. Patent No. 5 164 229 Nov. 17 1992.
10. Continuous Coating of Oxide Fiber Tows Using Liquid Precursors
11. Initial Assessment of the Weavability of Monazite‐Coated Oxide Fibers10.1111/jace.2004.87.9.1775 ↗
12. Precipitation Coating of Monazite on Woven Ceramic Fibers
13. 10.1111/j.1551-2916.2008.02333.x10.1111/j.1551-2916.2008.02333.x ↗
14. 10.1111/j.1551-2916.2008.02431.x10.1111/j.1551-2916.2008.02431.x ↗
15. 10.1016/S0955-2219(99)00257-510.1016/S0955-2219(99)00257-5 ↗
16. Monazite Coatings on Fibers
17. Monazite Coatings on Fibers
18. P. E. D.MorganandD. B.Marshall “Fibrous Composites including Monazites and Xenotimes ” U.S. Patent No. 5 665 463 Sep. 9 1997.
19. 10.1016/j.ccr.2007.09.00810.1016/j.ccr.2007.09.008 ↗
20. K. L.Nash L. R.Morss M. P.Jensen E. H.Appleman M. A.Schmidt S.Friedrich M.Redko andJ. J.Hines“Water‐Soluble Organophosphorus Reagents for Mineralization of Heavy Metals ”U.S. Dept. of Energy Report ANL/CHM/CP‐98479(1999).
21. 10.1021/bk-1996-0651.ch01710.1021/bk-1996-0651.ch017 ↗
22. 10.1016/j.jinorgbio.2004.12.01110.1016/j.jinorgbio.2004.12.011 ↗
23. 10.2134/jeq2006.000810.2134/jeq2006.0008 ↗
24. 10.1021/jp063380510.1021/jp0633805 ↗
25. 10.1016/0162-0134(86)80105-210.1016/0162-0134(86)80105-2 ↗
26. 10.1016/0162-0134(88)85013-X10.1016/0162-0134(88)85013-X ↗
27. 10.1016/0162-0134(91)80016-B10.1016/0162-0134(91)80016-B ↗
28. 10.1016/0162-0134(92)80004-F10.1016/0162-0134(92)80004-F ↗
29. Equilibrium Studies of Interactions of Rare Earth Ions with Phytic Acid
30. 10.1016/S0955-2219(99)00256-310.1016/S0955-2219(99)00256-3 ↗
31. D. B.Marshall private communication.
32. 10.1111/j.1151-2916.1996.tb09001.x10.1111/j.1151-2916.1996.tb09001.x ↗
33. 10.1557/PROC-480-310.1557/PROC-480-3 ↗
34. Validity of Using Average Diameter for Determination of Tensile Strength and Weibull Modulus of Ceramic Filaments10.1111/j.1151-2916.1997.tb03188.x ↗
35. Effect of Thermal Exposures on the Strength of Nextel™ 550 and 720 Filaments10.1111/j.1151-2916.1999.tb02159.x ↗
36. 10.1016/S0009-2614(90)87174-P10.1016/S0009-2614(90)87174-P ↗
37. Proton Environments in Hydrous Aluminate Glasses
38. 10.1021/cm000717l10.1021/cm000717l ↗
39. Lanthanum Phosphate Calcium Aluminum Glass
40. Synthesis of Nanosized Spherical Rhabdophane Particles
41. 10.1016/j.jssc.2003.11.00310.1016/j.jssc.2003.11.003 ↗
42. 10.1016/j.jssc.2003.11.00310.1016/j.jssc.2003.11.003 ↗
43. Thermal, Mechanical, and Chemical Properties of Sintered Xenotime‐Type RPO4 (R=Y, Er, Yb, or Lu)10.1111/j.1151-2916.1998.tb02613.x ↗
44. 10.2465/minerj.19.12310.2465/minerj.19.123 ↗
45. 10.1016/S0020-1693(00)81141-X10.1016/S0020-1693(00)81141-X ↗
46. 10.1021/jf00037a00410.1021/jf00037a004 ↗