journal article·2003-04

A study of kinetically limited dendritic growth at high undercooling using phase-field techniques

A.M. Mullis

Acta Materialia· Volume 51· Issue 7
Publisher page

Abstract

Abstract A phase-field model has been used to study the evolution of growth velocity, V , and tip radius, R , as a function of undercooling during the dendritic solidification of pure metals at high undercooling. We find that at sufficiently high undercooling the tip radius passes through a local minimum, beyond which the tip radius increases with undercooling. This local minimum in R is related to a change in the rate limiting process from diffusive transport to interface kinetics. Growth velocity continues to increase with undercooling above the transition undercooling, so that an undercooling regime exists where both V and R increase with undercooling. Clearly under these condition the R 2 V ≈constant scaling law normally applied to dendritic growth can no longer hold. On the basis of a limited number of data points in the region where both V and R increase with undercooling alternative scaling laws are suggested.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Solidification and crystal growth phenomena · Aluminum Alloy Microstructure Properties · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Corrigan · Phys Rev E · 1999 · 60 · 721710.1103/PhysRevE.60.7217 ↗
2. Bisang · Phys Rev E · 1996 · 54 · 530910.1103/PhysRevE.54.5309 ↗
3. Ivantsov · Doklady Akademii Nauk SSSR · 1947 · 58 · 567
4. Mullins · J Appl Phys · 1964 · 33 · 44410.1063/1.1713333 ↗
5. Lipton · Acta Metall · 1987 · 35 · 95710.1016/0001-6160(87)90174-X ↗
6. Willnecker · Phys Rev Lett · 1989 · 62 · 270710.1103/PhysRevLett.62.2707 ↗
7. Huang · Acta Metall · 1981 · 29 · 70110.1016/0001-6160(81)90115-2 ↗
8. Kessler · Adv Phys · 1988 · 37 · 25510.1080/00018738800101379 ↗
9. Pomeau · 1992 · 365
10. Brener · Phys Rev E · 1995 · 51 · 35110.1103/PhysRevE.51.351 ↗
11. Mushol · Phys Rev A · 1992 · 46 · 103810.1103/PhysRevA.46.1038 ↗
12. Brener · Adv Phys · 1991 · 40 · 5310.1080/00018739100101472 ↗
13. Kobayashi · Physica D · 1993 · 63 · 41010.1016/0167-2789(93)90120-P ↗
14. Wheeler · Physica D · 1993 · 66 · 24310.1016/0167-2789(93)90242-S ↗
15. Mullis · Acta Mater · 2001 · 49 · 220510.1016/S1359-6454(01)00133-1 ↗
16. Karma · Phys Rev Lett · 1996 · 77 · 405010.1103/PhysRevLett.77.4050 ↗
17. Karma · J Cryst Growth · 1997 · 174 · 5410.1016/S0022-0248(96)01060-3 ↗
18. Karma · Phys Rev E · 2000 · 61 · 399610.1103/PhysRevE.61.3996 ↗
19. Wang · Physica D · 1993 · 69 · 18910.1016/0167-2789(93)90189-8 ↗
20. Kessler · Adv Phys · 1988 · 37 · 25510.1080/00018738800101379 ↗
21. Kessler · Adv Phys · 1988 · 37 · 25510.1080/00018738800101379 ↗
22. Pomeau · 1992 · 3365
23. Turnbull · Acta Metall · 1982 · 30 · 213510.1016/0001-6160(82)90134-1 ↗
24. Battersby · J Mater Sci · 1999 · 34 · 204910.1023/A:1004547423857 ↗
25. Battersby · J Mater Sci · 2000 · 35 · 136510.1023/A:1004782107849 ↗
26. Mullis · J Appl Phys · 1997 · 82 · 378310.1063/1.365740 ↗
27. Mullis · Int J Non-equilibrium Processing · 2000 · 11 · 283
28. Trivedi · Metall Trans A · 1991 · 22 · 23510.1007/BF03350965 ↗