journal article·2003-04

Reaction sintering of TiN-TiB2 ceramics

K. Wang, V.D. Krstic

Acta Materialia· Volume 51· Issue 6
Publisher page

Abstract

Reaction sintering of TiN with B4C addition was carried out at temperatures ranging from 1980–2020 °C. The process involves a reaction between TiN and B4C at temperatures of 1400–1500 °C resulting in the formation of fine highly active TiB2 particles uniformly distributed in a matrix of TiN. The role of extremely fine particles of TiB2 in providing the additional driving force for sintering is discussed. The highest sintered density achieved was over 96%TD at ~2000 °C for samples containing 4wt% B4C. At the highest density, the TiN grain size was <15 μm as opposed to 50–60 μm size for samples with very small or no addition of B4C.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Boron and Carbon Nanomaterials Research · MXene and MAX Phase Materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (6)

Show source-provided references
1. Effect of aluminum addition on TiN hot-pressed sintering10.1007/BF00271008 ↗
2. TiN-TiB2 composites prepared by reactive hot pressing and effects of Ni addition10.1111/j.1151-2916.1995.tb08061.x ↗
3. Densification and characteristics of TiN ceramics10.1007/BF00258170 ↗
4. Toth LE. Refractory materials, Vol. 7: Transition metal carbides and nitrides. San Diego: Academic Press, 1971.
5. High strength-high toughness B4C-TiB2 xomposites10.1023/A:1006766910536 ↗
6. Mechanical properties of pressureless sintered boron carbide containing TiB2 phase10.1007/BF00240800 ↗