Use of Cube‐Corner Nano‐Indentation Crack Length Measurements to Estimate Residual Stresses Over Small Spatial Dimensions
Source abstract
Abstract
Cube‐corner indenters, by virtue of their acuity, possess a lowered threshold load for cracking. Shorter crack lengths allow the sampling of residual stresses in small spatial dimensions. We conducted cube‐corner indentation on tempered and annealed glasses. Indentation crack geometry was found to be “quarter‐penny.” A stress‐intensity factor for this geometry, and crack length decrements on tempered materials were used in a stress‐intensity superposition to provide reasonable estimates of residual stress. Stresses ∼100 MPa over a length scale of 10 μm, and 30 MPa over 20 μm were measured accurately, indicating that cube‐corner indentation is a promising tool for materials characterization.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Advanced Surface Polishing Techniques · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. 10.1111/j.1151-2916.1968.tb11840.x10.1111/j.1151-2916.1968.tb11840.x ↗
2. 10.1111/j.1151-2916.1978.tb16126.x10.1111/j.1151-2916.1978.tb16126.x ↗
3. Residual Stresses in Coating Technology
4. 10.1016/S0043-1648(99)00155-610.1016/S0043-1648(99)00155-6 ↗
5. 10.1111/j.1151-2916.2001.tb01119.x10.1111/j.1151-2916.2001.tb01119.x ↗
6. Residual Stresses in Alumina/Zirconia Composites
7. 10.1111/j.1151-2916.1985.tb15289.x10.1111/j.1151-2916.1985.tb15289.x ↗
8. 10.1063/1.169991310.1063/1.1699913 ↗
9. 10.1111/j.1151-2916.1990.tb05276.x10.1111/j.1151-2916.1990.tb05276.x ↗
10. McKenzie H. W. · 1999
11. 10.1111/j.1151-2916.1993.tb03922.x10.1111/j.1151-2916.1993.tb03922.x ↗
12. Raman Study of Silica Glass Under Tensile Stress
13. 10.1111/j.1151-2916.1977.tb16106.x10.1111/j.1151-2916.1977.tb16106.x ↗
14. 10.1007/BF0098077210.1007/BF00980772 ↗
15. 10.1111/j.1151-2916.1987.tb05006.x10.1111/j.1151-2916.1987.tb05006.x ↗
16. 10.1111/j.1151-2916.1990.tb05145.x10.1111/j.1151-2916.1990.tb05145.x ↗
17. 10.1016/S1359-6454(99)00248-710.1016/S1359-6454(99)00248-7 ↗
18. 10.1557/JMR.2001.028610.1557/JMR.2001.0286 ↗
19. 10.1016/S1359-6454(98)00226-210.1016/S1359-6454(98)00226-2 ↗
20. Influence of Stress on the Measurement of Mechanical Properties Using Nanoindentation
21. Influence of Stress on the Measurement of Mechanical Properties Using Nanoindentation
22. T. E.BuchheitandR.Tandon. Measuring Residual Stresses in Glasses and Ceramics using Instrumented Indentation to be submitted toJ. Mater. Res. Dec. 2006.
23. 10.1007/978-94-011-1765-4_2910.1007/978-94-011-1765-4_29 ↗
24. 10.1016/S0921-5093(98)00724-210.1016/S0921-5093(98)00724-2 ↗
25. 10.1111/j.1551-2916.2004.01494.x10.1111/j.1551-2916.2004.01494.x ↗
26. 10.1111/j.1151-2916.2003.tb03380.x10.1111/j.1151-2916.2003.tb03380.x ↗
27. 10.1111/j.1151-2916.1990.tb06738.x10.1111/j.1151-2916.1990.tb06738.x ↗
28. 10.1007/978-0-387-28920-5_710.1007/978-0-387-28920-5_7 ↗
29. Stress Intensity Factors for Penny and Half‐Penny Shaped Cracks Subjected to a Stress Gradient10.1007/BF00035075 ↗
30. R.Tandon Unpublished work 2006.
31. 10.1016/0013-7944(81)90116-810.1016/0013-7944(81)90116-8 ↗
32. A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness
33. 10.1016/0013-7944(95)00171-910.1016/0013-7944(95)00171-9 ↗
34. Radial Fracture During Indentation by Acute Probes
35. Radial Fracture During Indentation By Acute Probes