Abstract

The (111) oriented plate‐like BaTiO 3 ( BT ) particles with a tetragonal perovskite structure and a stoichiometric composition were successfully synthesized by a two‐step molten‐salt synthesis method ( MSS ). The as‐synthesized BT particles preserved the plate‐like shape of precursor Ba 6 Ti 17 O 40 ( B 6 T 17) particles with (001) major crystalline face, and, however, had a preferred pseudo‐cubic (111) orientation. BT particle with a high aspect ratio (10–20 μm in diameter and <1.5 μm in thickness) was achieved as the soaking temperature and time were optimized to be 1170°C and 5 h, respectively. Oriented particulate layer X ‐ray diffraction analysis revealed that the crystallographic (001) plane of B 6 T 17 has a topotactic relation with the (111) plane of BT particles.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Multiferroics and related materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute of Electro Ceramics and Devices School of Materials Science and Engineering Hefei University of Technology Hefei 230009 China

References (19)

Show source-provided references
1. 10.1038/nature0302810.1038/nature03028 ↗
2. 10.1063/1.164353710.1063/1.1643537 ↗
3. 10.1016/j.jeurceramsoc.2005.03.13010.1016/j.jeurceramsoc.2005.03.130 ↗
4. 10.1111/j.1151-2916.1997.tb02961.x10.1111/j.1151-2916.1997.tb02961.x ↗
5. 10.1021/ja01632a10710.1021/ja01632a107 ↗
6. 10.1111/j.1551-2916.2005.00057.x10.1111/j.1551-2916.2005.00057.x ↗
7. 10.1063/1.155448810.1063/1.1554488 ↗
8. 10.1016/j.jeurceramsoc.2007.02.09910.1016/j.jeurceramsoc.2007.02.099 ↗
9. 10.1016/j.matlet.2010.02.03710.1016/j.matlet.2010.02.037 ↗
10. 10.1007/s10832-006-6243-210.1007/s10832-006-6243-2 ↗
11. Preparation of Tabular BaTiO3 Powder by Two‐Step Molten Salt Method
12. 10.1111/j.1551-2916.2007.01525.x10.1111/j.1551-2916.2007.01525.x ↗
13. Topotaxy Between BaTiO3 and Ba6Ti17O4010.1111/j.1151-2916.1987.tb05723.x ↗
14. 10.1016/j.solidstatesciences.2007.08.00110.1016/j.solidstatesciences.2007.08.001 ↗
15. 10.1111/j.1151-2916.1998.tb02484.x10.1111/j.1151-2916.1998.tb02484.x ↗
16. 10.1016/j.ceramint.2007.09.02110.1016/j.ceramint.2007.09.021 ↗
17. 10.1111/j.1744-7402.2005.02007.x10.1111/j.1744-7402.2005.02007.x ↗
18. 10.1021/cm802776g10.1021/cm802776g ↗
19. 10.1021/cm903315u10.1021/cm903315u ↗