journal article·1994-03

Erosion Wear Properties of Tetragonal ZrO 2 (Y 2 O 3 )‐Toughened Al 2 O 3 Composites

Hidehiro Kamiya, Masato Sakakibara, Yukio Sakurai, Genji Jimbo, Shigetaka Wada

Publisher page

Abstract

Erosion wear properties of tetragonal zirconia ( t ‐ZrO 2 with 3 mol% Y 2 O 3 )/Al 2 O 3 composites with different volume fractions of t ‐ZrO 2 in the rang of O to 100 vol% (including Al 2 O 3 or t ‐ZrO 2 ceramics), were measured by a collision test between Al 2 O 3 or SiC particles accelerated in an air stream (240 m/s) and a stationary composite or ceramics target. In the case of Al 2 O 3 erodent particles, the wear rate of composites decreased to one‐tenth of the wear rate of Al 2 O 3 or t ‐ZrO 2 ceramics. The optimum volume fraction of the addi‐tive phase for increased wear resistance was in the range of 7 to 22 vol% of t‐ZrO 2 . However, the wear resistance of all composites in collision with SiC particles deteriorated. The maximum wear rate appeared at about 40 vol% of t‐ZrO 2 , and reached two times that of the Al 2 O 3 or t‐ZrO 2 ceramics. The mean fracture load of the SiC erodent particle in a diametral compression test under quasi‐static loading was 2.3 times the value of the Al 2 O 3 particle, which broke after collision with the target. Therefore, the mean impact force produced by Al 2 O 3 particles striking the target was much lower than that from SiC particles. Because the impact force acting from the Al 2 O 3 particles did not reach the threshold force required for lateral crack propagation in the composites, the principal damage mechanism, the wear resistance of composites increased. However, the impact force from SiC particles was greater than the threshold force, and lateral or other damaging cracking was promoted at the wear surface of the composite materials. This discussion is in agreement with the analysis by the lateral crack model and the results for the median crack length of each ceramic measured by Vickers indentation tests with different loads. The slope of the logarithm of median crack length as a function of the logarithm of Vickers indent load was larger than the value of 2/3 obtained theoretically.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Orthopaedic implants and arthroplasty

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. 10.1111/j.1151-2916.1976.tb09386.x10.1111/j.1151-2916.1976.tb09386.x ↗
2. Effect of Induced Microcracking on the Fracture Toughness of Ceramics
3. 10.1111/j.1151-2916.1985.tb15251.x10.1111/j.1151-2916.1985.tb15251.x ↗
4. 10.2109/jcersj.98.45610.2109/jcersj.98.456 ↗
5. 10.1111/j.1151-2916.1991.tb06882.x10.1111/j.1151-2916.1991.tb06882.x ↗
6. 10.1111/j.1151-2916.1991.tb07290.x10.1111/j.1151-2916.1991.tb07290.x ↗
7. 10.2109/jcersj.98.1310.2109/jcersj.98.13 ↗
8. Solid Particle Erosion of Brittle Materials (Part 4); The Erosion Wear of Thirteen Kinds of Commercial Al2O3 Ceramics
9. 10.2109/jcersj.96.11110.2109/jcersj.96.111 ↗
10. Wada S. · 1989 · 481
11. J. L.Routbort D. A.Helberg andK. C.Goretta “Erosion of Whisker Reinforced Ceramics ”J. Hard Mater. in press.
12. 10.1111/j.1151-2916.1979.tb18807.x10.1111/j.1151-2916.1979.tb18807.x ↗
13. 10.2109/jcersj.96.59910.2109/jcersj.96.599 ↗
14. 10.2109/jcersj.97.13110.2109/jcersj.97.131 ↗
15. 10.1111/j.1151-2916.1979.tb18807.x10.1111/j.1151-2916.1979.tb18807.x ↗
16. 10.1111/j.1151-2916.1990.tb05216.x10.1111/j.1151-2916.1990.tb05216.x ↗
17. 10.1111/j.1151-2916.1988.tb06412.x10.1111/j.1151-2916.1988.tb06412.x ↗
18. Solid Particle Erosion of Brittle Materials (Part 1): The Relation between Erosion Wear Properties of Gas Pressure Sintering Si3N4
19. 10.1016/0043-1648(88)90180-910.1016/0043-1648(88)90180-9 ↗
20. Solid Particle Erosion of Brittle Materials (Part 4); The Effecf of Impingement Angle
21. 10.1016/0001-6160(76)90042-010.1016/0001-6160(76)90042-0 ↗
22. Evans A. G. · 1980 · 7
23. 10.1111/j.1151-2916.1976.tb10991.x10.1111/j.1151-2916.1976.tb10991.x ↗
24. 10.1111/j.1151-2916.1980.tb10768.x10.1111/j.1151-2916.1980.tb10768.x ↗
25. 10.1111/j.1151-2916.1982.tb10782.x10.1111/j.1151-2916.1982.tb10782.x ↗
26. 10.1098/rspa.1978.010610.1098/rspa.1978.0106 ↗
27. 10.1111/j.1151-2916.1984.tb19167.x10.1111/j.1151-2916.1984.tb19167.x ↗
28. 10.1111/j.1151-2916.1986.tb04769.x10.1111/j.1151-2916.1986.tb04769.x ↗
29. 10.1111/j.1151-2916.1982.tb10342.x10.1111/j.1151-2916.1982.tb10342.x ↗
30. 10.1557/PROC-78-20710.1557/PROC-78-207 ↗
31. Impact Damage and Strength Degradation in a Silicon Car‐bide Reinforced Silicon Nitride Composite