Fatigue mechanism in Ni3Fe single crystals with L12 superlattice structure
Source abstract
Abstract
Abstract Ni 3 Fe single crystals with the L1 2 structure were cyclically deformed with various loading axes at different plastic strain amplitudes. The crystals demonstrated initial strong cyclic hardening followed by rapid cyclic softening at any orientation tested. There existed a typical plateau region in the cyclic stress–strain curves of the crystals oriented for single slip, while the saturation shear stress ( τ s ) monotonically increased with increasing plastic shear strain amplitude ( γ pl ) for double-slip oriented crystals. Persistent slip bands (PSBs) with cell-like dislocation structure developed in fatigued Ni 3 Fe single crystals. The relationship between the volume fraction of PSBs and γ pl suggests that Winter’s two-phase model can be applied to explain the cyclic stress–strain response in Ni 3 Fe single crystals. Activation of the secondary slip is closely related to the cyclic hardening/softening behaviour and the formation of PSB in Ni 3 Fe single crystals.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · High Temperature Alloys and Creep · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Suresh · 1998
2. Neumann P. In: Chan RW, Haasen P, editors. Physical metallurgy, 3rd ed.; 1983. p. 1554.
3. Winter · Phil. Mag. · 1973 · 30 · 71910.1080/14786437408207230 ↗
4. Mughrabi · Mater. Sci. Eng. · 1978 · 33 · 20710.1016/0025-5416(78)90174-X ↗
5. Ackermann · Acta metall. · 1984 · 32 · 71510.1016/0001-6160(84)90145-7 ↗
6. Li · Defect and Diffusion Forum, Mater. Sci. Forum · 2001 · 188-190 · 15310.4028/www.scientific.net/DDF.188-190.153 ↗
7. Lukáš · Mater. Sci. Eng. · 1994 · A189 · 110.1016/0921-5093(94)90395-6 ↗
8. High temperature ordered intermetallic alloys
9. Stoloff · ISIJ Int. · 1997 · 37 · 119710.2355/isijinternational.37.1197 ↗
10. Yamaguchi · Prog. Mater. Sci. · 1990 · 34 · 110.1016/0079-6425(90)90002-Q ↗
11. Hsiung · Acta metall. mater. · 1991 · 38 · 119110.1016/0956-7151(90)90192-J ↗
12. Hsiung · Acta metall. mater. · 1992 · 40 · 299310.1016/0956-7151(92)90463-O ↗
13. Hsiung · Acta metall. mater. · 1994 · 42 · 145710.1016/0956-7151(94)90164-3 ↗
14. Dahl · Z. Metallk · 1936 · 28 · 133
15. Chikazumi · J. Phys. Soc. Jpn. · 1957 · 12 · 125910.1143/JPSJ.12.1259 ↗
16. Takahashi · Phys. Stat. Sol. (a) · 1977 · 42 · 20110.1002/pssa.2210420121 ↗
17. Takahashi · Phys. Stat. Sol. (a) · 1977 · 42 · 52910.1002/pssa.2210420215 ↗
18. Kronmüller · Int. J. Nondestructive Testing · 1972 · 3 · 315
19. Yasuda · Acta mater. · 2000 · 48 · 340110.1016/S1359-6454(00)00143-9 ↗
20. Yasuda · J. Appl. Phys. · 2000 · 88 · 590910.1063/1.1313781 ↗
21. Yasuda HY, Furuta D, Sasaki A, Izaki A, Umakoshi Y. J. Appl. Phys., submitted for publication.
22. Morris · Acta metall. · 1976 · 24 · 2110.1016/0001-6160(76)90142-5 ↗
23. Yoo · Acta metall. · 1988 · 36 · 293510.1016/0001-6160(88)90176-9 ↗
24. Horton · Phil. Mag. · 1991 · A63 · 31910.1080/01418619108204852 ↗